Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Polyaniline as inert anode?
MeshPL
Hazard to Others
***




Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2015 at 20:05
Polyaniline as inert anode?


So a simple question:
Is there any way I can make polyaniline electrode suitable for use as the anode in chlorate production?

You know, it's an easy to make conductive polymer.
View user's profile View All Posts By User
jock88
National Hazard
****




Posts: 505
Registered: 13-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 26-4-2015 at 13:30



How do you make polyaniline
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 26-4-2015 at 14:45


Answer #1: I wouldn't be optimistic about the results. A conductive organic polymer coupled with a warm, strong,

oxidizer would present a rocky marriage during the best of days. Even if it survives direct attack, once bias is applied to

the electrode the polymer will no doubt become oxidized. But hey, it would be interesting to try it and see what happens...


Answer #2:

Attachment: Electrochemical properties of PANI as Single Electrode of.pdf (2.9MB)
This file has been downloaded 706 times
View user's profile View All Posts By User
MeshPL
Hazard to Others
***




Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline

Mood: No Mood

[*] posted on 4-5-2015 at 11:09


Yeah, I doubt they will work.
View user's profile View All Posts By User