Strontium?
So uh...how could I make strontium (oxide, carbonate, etc.)? We have some celestite in the house (okay, so it's a beautiful blue mineral, well
no one will miss a corner ), but what the heck reduces an insoluble sulfate?
From what I can tell, decomposition temperature is uselessly high...
Tim
|
|
JohnWW
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
Celestite is SrSO4, found in tabular crystals, and is the principal ore of strontium. It is similar to anhydrite, CaSO4, and barite, BaSO4, which is
the principal ore of barium.
I would think that a method of refining it would be by electrolysis of the molten sulfate, but it is stated as decomposing at 1,580ºC. This
temperature, which would result in SrO, is expensive to attain and maintain, and steel-type alloys cannot be used for a vessel. Reaction with HF is
another possibility, but rather dangerous and messy.
|
|
notagod
Harmless
Posts: 21
Registered: 23-10-2002
Location: Sunny Scandinavia
Member Is Offline
Mood: No Mood
|
|
12AX
If you want the carbonate, search for a post I made in the calcium sulphide post.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Ah, interesting! I may also have to try the carbon or aluminum reduction too ![:D](./images/smilies/biggrin.gif)
Tim
|
|
Mr. Wizard
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
Red road safety flares are supposed to be over 70% Strontium Nitrate. This could be easily done by putting a few in a bucket of boiling water to get a
soluble nitrate. If you were to burn the flare first you would end up with the strontium slag as the oxide, sulfate, and carbonate.(just a guess) A
dry crushed mixture of the white slag with aluminum might yield the metal through a thermite reduction.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Quote: | Originally posted by Mr. WizardA dry crushed mixture of the white slag with aluminum might yield the metal through a thermite reduction.
|
The sulfate perhaps, but is Al + (alkaline earth oxide) > Al2O3 + (metal) favorable? Since, those are all pretty high melting point = stable
oxides, after all.
Tim
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
It might cause some reaction, but it wouldn’t work for the oxides, even with aluminum oxide’s high lattice energy.
Doing the calculation for SrO, I got deltaH = +101KJ/mol, deltaS = -3.88J/mol*K, meaning that you’d have a hard time getting any kind of reaction
with this particular oxide. Even if you did, the metal you’d get out would mostly be aluminum.
[Edited on 2-4-2005 by neutrino]
|
|
Mr. Wizard
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
It's not practical that's for sure. I did find this though:
The metal can be prepared by electrolysis of the fused chloride mixed with potassium chloride, or is made by reducing strontium oxide with aluminum in
a vacuum at a temperature at which strontium distills off. The BP is about 1370C at 760 mm Hg.
Not exactly a self sustaining thermite reaction :-( Anyway the part about the red flares is still a viable source of the nitrate.
|
|