Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: stainless steel and hydrochloric acid purification
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 9-7-2015 at 18:37
stainless steel and hydrochloric acid purification


My problem is the separation of metal ions from each other including chromium and iron chloride from a solution that was gotten from the reaction of stainless steel wool and 9 molar hydrochloric acid. I am sure that the green nature of the solution is from chromium chloride and this is a unwanted impurity for my needs.

After the mixture is filtered and crystallized what is the best way to separate the products?




We are chemists , we bring light to the darkness. Knowledge to ignorant, excitement to the depressed and unknowing. we bring crops to broken fields and water to the desert. Where there is fear we bring curiosity.

View user's profile View All Posts By User
Molecular Manipulations
Hazard to Others
***




Posts: 447
Registered: 17-12-2014
Location: The Garden of Eden
Member Is Offline

Mood: High on forbidden fruit

[*] posted on 9-7-2015 at 20:20


First I'd oxidize them to (III) with hydrogen peroxide, next boil off the water, then heat the two chloride hydrates until they liberate hydrogen chloride gas and then their water. Now you have a mixture of oxides of iron (III) and chromium (III), treat this with hydrochloric acid, the iron oxide will dissolve but the chromium oxide will not.



-The manipulator
We are all here on earth to help others; what on earth the others are here for I don't know. -W. H. Auden
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 10-7-2015 at 19:29


After oxidizing the salts with hydrogen peroxide is it possible to extract the iron (III) chloride with acetone and leave the chromium (III) chloride behind?



We are chemists , we bring light to the darkness. Knowledge to ignorant, excitement to the depressed and unknowing. we bring crops to broken fields and water to the desert. Where there is fear we bring curiosity.

View user's profile View All Posts By User
Oscilllator
National Hazard
****




Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline

Mood: No Mood

[*] posted on 10-7-2015 at 20:02


Quote: Originally posted by SimpleChemist-238  
After oxidizing the salts with hydrogen peroxide is it possible to extract the iron (III) chloride with acetone and leave the chromium (III) chloride behind?

Not while they are in solution, since of course acetone is miscible with water. Also, Iron(III) chloride cannot be dehydrated to anhydrous iron chloride by heating, so you can't go that route. You *might* be able to boil off enough water to get the iron and chromium to crystallise out though, and try an extraction with that.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4744
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 10-7-2015 at 21:18


You could also oxidize the Cr to chromate with hypochlorite and separate it that way, through fractional crystallization. And that way you also get some useful chromate out of it.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 10-7-2015 at 21:46


What is the point of this exercise? You primarily have a solution of iron, nickel, and chromium salts. Which are you looking to recover and which are you not interested in?

Assuming the Chromium is in the +3 oxidation state, addition of ammonia will prpecipitate iron oxides and most of the chromium as the hydroxide. The solution will contain mainly nickel and a small amount of chromium.

Treating the residue with sodium hydroxide solution will dissolve the chromium hydroxide and leave behind the iron. Or if you treat the initial solution with NaOH, you will produce a solution of chromium and a sludge of hydrous iron oxides and nickel hydroxide.

If you want iron salts from this mess, why on earth did you not start with regular steel wool. If you wanted nickel, perhaps coins would have been a better starting place.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 11-7-2015 at 02:47


Quote: Originally posted by SimpleChemist-238  
After oxidizing the salts with hydrogen peroxide is it possible to extract the iron (III) chloride with acetone and leave the chromium (III) chloride behind?


It is possible to extract the iron from solution with ether.
You need an excess of HCl to get the extraction to work.
View user's profile View All Posts By User
SimpleChemist-238
Hazard to Others
***




Posts: 147
Registered: 28-9-2014
Member Is Offline

Mood: Chlorine Trifloride Flame Thrower

[*] posted on 11-7-2015 at 12:06


My extraction with acetone would happen after the solution crystallized. The iron would dissolve in the acetone and leave behind the chromium and nickel. I don't believe there is much nickel in the solution because the steel I used is very low grade.



We are chemists , we bring light to the darkness. Knowledge to ignorant, excitement to the depressed and unknowing. we bring crops to broken fields and water to the desert. Where there is fear we bring curiosity.