Refinery
Hazard to Others
 
Posts: 371
Registered: 17-2-2014
Member Is Offline
Mood: Still
|
|
Silver electrolysis purification
Do I need silver nitrate as electrolyte or can I use copper nitrate as well since it is much cheaper? I would use SS anode and junk silver items as
cathode and electrolyse them this way. Would this work?
|
|
|
gdflp
Super Moderator
     
Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline
Mood: Staring at code
|
|
No you cannot. The entire purpose of that method is to reduce the concentration of contaminating metals(such as copper) in the silver by selectively
dissolving and reprecipitating pure silver metal. If you used copper nitrate as an electrolyte, you would initially precipitate pure copper, then
most likely a mixture of copper and silver, but most certainly not the pure silver you're after. You might be able to use a dilute solution of nitric
acid, so long as the concentration is low enough that it won't attack either metal, but I am unsure if this will work. In the end, you will end up
with a silver nitrate solution as your electrolyte regardless of what you use initially, so you might as well just use it to begin with.
|
|
|
Metacelsus
International Hazard
   
Posts: 2554
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Wouldn't you want to use a junk silver anode and a pure silver cathode? The silver will dissolve from the anode and deposit on the cathode. Impurities
will become sludge, or stay in solution. You'll need to keep the voltage controlled to ensure purity. For a reference (with copper): http://chemwiki.ucdavis.edu/Core/Inorganic_Chemistry/Descrip...
[Edited on 5-5-2016 by Metacelsus]
|
|
|
Refinery
Hazard to Others
 
Posts: 371
Registered: 17-2-2014
Member Is Offline
Mood: Still
|
|
Nitric acid is currently banned in EU area so I was thinking alternative routes. If must, I will make some HNO3 and go with it then.
|
|
|
aga
Forum Drunkard
   
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
You can still buy Silver Nitrate and it'll end up cleaner/purer than making it yourself.
I think a member here called 'hegi' was selling some. Top quality too.
|
|
|