Magnesium-zinc intermetallics
(If this belongs better in Energetic Matl's, well, you know what to do )
Has anyone experimented with Mg-Zn for reductions or pyrotechnic compositions?
http://webpages.charter.net/dawill/Images/Mg-Zn.gif
I just mixed small batches of 25% Mg-75% Zn and 15% Mg-85% Zn (by weight, corresponding to Mg<SUB>12</SUB>Zn<SUB>13</SUB> and
MgZn<SUB>2</SUB> respectively). Both are brittle and easy to grind; the 12:13 catches fire readily above the melting point (burning with
the blue to green to white flame you would expect from such a mixture), while the other did not burn. Both crushed well (though minor galling was
noticed grinding the 1:2 mix) and both burned well once powdered. The 1:2 burned with a more distinct bluish-green color when mixed with some
chlorate + charcoal composition.
I will yet try the remaining two intermetallics (2:3 and 2:11).
Oh, and the ultimate purpose of this is to find brittle intermetallics for reactive metals (such as Mg, Al and Zn) to simplify grinding.
Tim
|
|
my nootloss
Harmless
Posts: 39
Registered: 23-5-2005
Member Is Offline
Mood: No Mood
|
|
Have you tried sulfur and zinc?
|
|
uber luminal
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 25-8-2004
Member Is Offline
Mood: No Mood
|
|
interesting idea. I would think the phase diagram would come in handy here. *wishes for ASM BPD vol 1-3*.
However, *scratches head* this is my first, 'I just woke up from 4 hours of crappy sleep' impression: if the 2 metals reacted in air...
wouldnt the reaction then be Mg, Zn and O2?
When Mg is reactive with other metals in an inert chamber, it does not give off different colors like this. I would try it today to find out for you,
but all the melters are under a heavey queue right now. and even if I had more time reserved today, I have 14 melts I need to make before I can screw
around.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Ohh, this is just brittle metals for crushing-- not entropy released on forming intermetallics. I noticed no heat of formation when alloying.