jimwig
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
aluminium welding
at certain events such as gun shows and county fairs there has been in the past folks who demonstrate a kind of alloy which will solder/weld aluminum.
does anyone have knowledge of the alloy's composition?
oh i should add this is done with heat of a propane torch
jim
E.b.C.:Title
[Edited on 9-7-2005 by chemoleo]
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Not weld, braze (or solder). The former is a ZA alloy (zinc aluminum) with melting point 716°F (eutectic) up to about 900°F. The latter is a
tin-zinc solder.
The brazing rods can be used without flux, in which case the (solid) rod is rubbed against the work, mechanically removing the aluminum oxide surface.
Solders usually come with some sort of chloride + fluoride flux that's probably very bad to eat.
Tim
|
|
jimwig
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
is this within the range of preparation of the average noob type with access to moderately high temp via muffle furnace say like 2000 degrees?
that is can the zinc and aluminum be alloyed in a simple proces and extruded (whatever) to form usable solder brazing material.
i remember the demonstrator defiantly stressed the important of oxide removal via staninless wire brush. this is i understand the largest impetiment
to successful aluminum brazing/soldering.
|
|
uber luminal
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 25-8-2004
Member Is Offline
Mood: No Mood
|
|
Those people that sell that solder are not very smart if they say you must use a brush to remove oxides from the Aluminum.
Coming from someone who makes a lot of custom alloys, its almost cheaper to buy the crappy solder than to try and make it. You must get the mostly
pure raw materials (which costs money to buy and ship esp in low quantities). Then you must spend time prepping and massing out the materials. put
them into some sort of furnace that will not allow oxidation. (gas with flux, muffle with vacuum or sealed can etc). bring it up to the alloy temp,
which is pretty low(below 600C), allow it to sit, and then somehow quench it, without contaminating it again. Then to extrude the stuff... no... thats
a lot of work. I would swage it if it doesnt end up brittle.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Erm...
No offense but you really don't have much really practical experience with metal, do you? Brazing isn't exactly analytical chemistry.
Aluminum scrap (besides cast alloy) and zinc scrap (any) can be mixed to get some sort of a ZA alloy, around 5-10% Al I'd figure for a brazing
rod. Heat it to a dark red glow (at night might be helpful) and cast a long thin ingot in a (possibly preheated) ingot mold. You can also pour into
a sand mold with holes poked in it of the desired size.
For the Zn-Sn alloy, you might get away with some OTS lead-free solder. I'd have to guess you'd want one of the sort that contains copper
and/or silver to harden the tin, as opposed to antimony, although depending on how much Sb it has, it may still be acceptable when alloyed with zinc.
Tim
|
|
uber luminal
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 25-8-2004
Member Is Offline
Mood: No Mood
|
|
off topic
Quote: | Erm...
No offense but you really don't have much really practical experience with metal, do you? Brazing isn't exactly analytical chemistry.
| ohh harsh. I am curious what leads you to believe that I 'really don't have much really'
practical experience with metal' ? (in your expert opinion of course. )
I also would like to know why it is suggested to scratch the surface of the Al... to remove the Al oxide...
scratching the surface with something that is harder than the Al is useful to create mechanical sites for the liquid metal. (and to clean it).
Scratching the surface with brazing rod... which is likely softer than the base alloy, helps the braze or solder adhere to the surface. However,
neither of these two methods, would be methods for removing surface oxides for any period of time that would be of use.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Quote: | Originally posted by uber luminal
ohh harsh. I am curious what leads you to believe that I 'really don't have much really' practical experience with metal' ? (in
your expert opinion of course. )
|
Well in particular... no one in the business cares about 99.99% pure materials (except for sulfur in ferrous alloys, but that's a special case).
I get passable results (yeah, for overbuilt castings ) using literally any
aluminum available.
Tolerances get comfortably baggy and loose when you're not doing things to litigious specifications...
Quote: | I also would like to know why it is suggested to scratch the surface of the Al... to remove the Al oxide...
scratching the surface with something that is harder than the Al is useful to create mechanical sites for the liquid metal. (and to clean it).
Scratching the surface with brazing rod... which is likely softer than the base alloy, helps the braze or solder adhere to the surface. However,
neither of these two methods, would be methods for removing surface oxides for any period of time that would be of use. |
Well, then, I guess you'll just have to see it to believe it.
I've done it with 2.5% Cu, 97% Zn (oh I'm sorry, Cu0.025 Zn0.97, as bulky as THAT is...), when it gets to the right temperature, the oxide
losens from the metal and, more importantly, the rod forms an eutectic which melts on contact. This lubricates and makes the oxide that much more
mobile, allowing it to be simply pushed aside. Without pretinning or fluxes, full penetration cannot be had, although with careful temperature
control and technique, smooth fillets can be made.
Tim
P.S. Yes indeedy, this (and the preceeding) post of mine have been unusually harsh... just trying things the MSDB way... er, oops...
|
|
Lambda
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 566
Registered: 15-4-2005
Location: Netherlands
Member Is Offline
Mood: Euforic Online
|
|
Aluminium solder
Aluminium solder # 1
Aluminium....30 parts
Zink................20 parts
Tin..................15 parts
Copper.............5 parts
Bismuth..........10 parts
Silver...............10 parts
Aluminium solder # 2
Aluminium......88 parts
Silicium...........12 parts
Remark about unit usage:
Parts = Weight units.
Refference:
UPLOAD / LAMBDA / Mengen en Roeren (Dutch) / Mengen en Roeren volume 1.
Page: 225.
Location:
MadHatter's FTP (Mengen en Roeren volume 1 & 2).
Book downloaded from Gamekeeper's website:
http://gamekeeper.deds.nl/
Remark: No specific flux for Aluminium was found in "Mengen en Roeren" volume 1 & 2. These fluxes are cheap, and easily obtainable.
Fluorides may be the stumbling block in making it yourself.
[Edited on 10-7-2005 by Lambda]
|
|
jimwig
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
girls girls didn't mean to start a pissing contest. although that is an interesting graphic.
no, i may be wrong but surface oxidation can be removed with a wire brush or at least enough of it to allow some type of soldering/brazing (try not to
nitpick my choice of words here).
'course an approipriate flux also helps.
i have been doing that for a while. you do not have to be a metalagist (sp?) to understand this rather basic operation.
oxidation layers for the most part are surfical. and since aluminum oxidizes almost immediately then removing the top most surface should reduce if
not remove the "rust".
i suppose this affinity for aluminu for oxygen has to with bond angles, valence coordinates and all kinds of stuff that i really don't care
about.
you see i don't have refine my own petroleum to use it my infernal combustion engine.
thanks for the help ----
[Edited on 11-7-2005 by jimwig]
|
|