Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Anti Static Pyro Compositions
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 26-2-2017 at 10:35
Anti Static Pyro Compositions


Hello All,

I have been doing extensive research on pyrotechnic compositions and their sensitivity to static electricity... and have not been satisfied with any potential solutions.

Obviously mixtures with metal particles are more static sensitive, such as 70/30 flash. And the smaller the metal particles the more sensitive to static (I presume this is because a smaller particle will melt and vaporizes with a smaller energy input such as static). In regards to flash, I have also heard it is static sensitive because the oxide layer is non conductive, and the inside Al is... essentially forming a capacitor.

So... lets take 70/30 (2-5 micron flake Al as an example... if I don't want to use a larger Al size because performance will drop... what are my options?

1) Mixing in a non conductive clay, although I hear this reduces performance. Has anyone tried this?

2) Perhaps coating the Al powder with a thin (micron to nanometer) coat of wax or animal fat, sterin? Again, has anyone tried this?

3) I can't find any information on this in regards to pyrotechnics but I know copper nano particles (5-7nm) are used in making anti static plastics. If this were mixed in with the flash powder wouldn't it create a Gaussian cage?? surly at 5-7nm all of the particles would be evenly coated and surrounded. Perhaps mill the Al with copper nano particles?

That is all of my ideas..

Bert your response is mandatory because you have experience in all of these things, or you can always point me in the right direction...:D

I don't care if the solution is expensive... lets partake in some thought experiments, or actual experiments!!:D
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2552
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 26-2-2017 at 14:44


I wonder if adding some graphite powder would help dissipate static charges. It might be worth a try.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 26-2-2017 at 15:01


I am pretty sure coating with wax or polymer works, i wonder what requirements you need from your mixtures since wax coating usually reduces the burn rate.
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 26-2-2017 at 17:17


Are there any polymers that work particularly well for Al that you know of?
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 27-2-2017 at 03:03


From what I remember form my 20 year ago chemical engineering lessons:

The oxide layer is part of the problem but also the bad conductivity of other ingredients (amorphous Carbon, Sulfur, wax coating)...

If you understand wel what is static electricity and a capacitor...you clearly get the feeling that the core of the problem is the charge separation from insulating materials (by friction, swirling, flowing) and eventually the mutual charge induction of metallic material.

It is known that into hydrophobic non conductive solvents flowing into metallic pipes or into plastic ones (that are not grounded to the soil)...that you can have hurge electrostatic potential and discharge...like thunder bolts...

The static electricity will also be reduced if metallic particles get in touch with each others (thus forming kind a continuous phase entraping non conductive nuggets --> Gaussian cage); or following the reverse idea a lot of insulating material to keep the metallic particles to be able to spark between each others...thus increasing the spark gap.

Wax or polymer may thus not be the smartest to use...and the waxy coating treatment of Al powder (reducing its sensitivity to moist air) asmuch as the Al2O3 or Al(OH)O layer are insulating the metallic core of the particles.

In fact the best option would be to render the powder conductive so that all charges can exit or fade...but increasing interparticulate conductivity also means a storage concern...because of the inherent reactivity of Al powder...or a severe reduction of initiability (typical example is moisture)

The use of Cu powder will not play any role... because it will play the same role as the Al...

A Gaussian cage needs continuous contact media...sothat the charges can repel each other to the extremal external surface...the inside is thus chargeless...so you need continuous wires, grids or planes or volumes eventually with voïds...

Also the surface of the metal plays a role..."the power of nails" (I have found no translation of this into English...but the Lightning rod is based on that principle...and generates a ionised wind); so when there is a sharp edge usually this means charges gathers there and the electrostatic potential is localy increased...air passing by (or other materials can be ionised) and thus the material discharges by gaseous convection...This can be seen into the dark by some glowing of the pin point (St-Elmo's fire)...so if the metallic conductor is smooth, polished, with moderate curves (ideally perfectly sperical), it will hold its charge longer and be less prone to easily dicharge and sparks.

Absolutely not an easy subject...also very depending onto atmospheric conditions (heat/moisture).

[Edited on 27-2-2017 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-2-2017 at 13:12


Philou,

Thank you for your reply... I understand what you are saying but have a few questions.

If the best thing is for the metallic particles to touch each other than why do compositions become more static sensitive when nano particles are induced... as they completely coat a 120 micron oxidizer particle?

How would nano copper or silver not help with this, especially if they were 5-7nm, they would coat everything, and silver, being a noble metal will not oxidize easily?

So for this flash powder, would it be better to use spherical Al 500nm instead of the 2-5 micron flake?... but then it will become more impact sensitive... ahhh!

[Edited on 27-2-2017 by MineMan]

[Edited on 27-2-2017 by MineMan]
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 28-2-2017 at 02:16


Quote: Originally posted by MineMan  
Philou,

Thank you for your reply... I understand what you are saying but have a few questions.

If the best thing is for the metallic particles to touch each other than why do compositions become more static sensitive when nano particles are induced... as they completely coat a 120 micron oxidizer particle?

How would nano copper or silver not help with this, especially if they were 5-7nm, they would coat everything, and silver, being a noble metal will not oxidize easily?

So for this flash powder, would it be better to use spherical Al 500nm instead of the 2-5 micron flake?... but then it will become more impact sensitive... ahhh!

Usullay they don't coat efficiently...have you made a simultation or a calculation to say this? Can you show me the calculation to see if it is correct?

Apparently...it is hard to understand or visualize (again linked to the "pin point power"): if you have two different particle size of the same material brought at the same electric potential...the radius reduction of the particle reduces the overal electric charge of the particle propotionnally...and at the same distance (bigger than R) the electric field is also lower
So if R = 2*r
$$q R = V × 4 π ε 0 R {\displaystyle q_{R}=V\times 4\pi \varepsilon _{0}R} {\displaystyle q_{R}=V\times 4\pi \varepsilon _{0}R}$$

$${\displaystyle q_{r}=V\times 4\pi \varepsilon _{0}r={\frac {V\times 4\pi \varepsilon _{0}R}{2}}={\frac {q_{R}}{2}}}$$

$${\displaystyle E_{R}={\frac {V\times R}{d^{2}}}}$$

$${\displaystyle E_{r}={\frac {V\times r}{d^{2}}}={\frac {V\times R/2}{d^{2}}}={\frac {1}{2}}{\frac {V\times R}{d^{2}}}={\frac {E_{R}}{2}}}$$

so at the distance d (what is further than R itself twice as big as r)...the electric field of the particle r is reduced by a factor 2 vs particle R.

But if you go in close contact with the external layer for the tinier particle r you can go much closer than into the R case since R is unpenetrable solid and charges are onto the outer shell/surface.
So
$${\displaystyle E_{R}={\frac {V\times R}{R^{2}}}}$$
$${\displaystyle E_{r}={\frac {V\times r}{r^{2}}}={\frac {V\times R/2}{(R/2)^{2}}}={\frac {V\times R/2}{R^{2}/4}}=2{\frac {V\times R}{R^{2}}}=2E_{R}}$$

And in fine, we observe that the electric field in close viccinity to the surface of the tinier particle will be twice bigger than the one in close viccinity of the larger one.
By extension...if the radius is n times smaller...the electric field at the surface will be n times bigger.
It comes from the fact that the sum of the charges q set on a spherical surface submitted to an electric potential V is increasing linearly with the increasing radius while the electric field decreases at the same time as a function of 1/d².

If you consider a pin point as a very small diameter half sphere (what is the case if you look at it under strong magnification)...the electric field obtained at that point has a value that tends to the infinity...and this very high field will contribute to air ionisation, and electric arc triggering.
Effet_pointe.jpg - 40kB
Last thing to consider for R vs r (=1/2*R)...if at the surface of r you have an electric field twice bigger...for the same weight of metal (at the same density) you have also the same volume...
So
VR = 4/3*π*R3
and
Vr = 4/3*π*r3
thus
Vr = 4/3*π*(R/2)3 = 1/23*4/3*π*R3 = 1/8*VR
You thus have potentially 8 times more electric field per equivalent weight without counting the already double value...
In the case of a reduction of factor n (R=n*r) you thus have for each particule r an electric field n*ER bigger but also n3 times more particles than into the R case...and this makes a serious increase of n3*n*ER = n4*ER
So reducing the radius by a factor 2 increases the risk of static by 16...I let you imagine what happens when passing from micro to nano sized metallic powder....

Silver and copper are near "noble metals" they don't oxidise easily from air or oxygen...but they are oxidised by trace poluants from air (ammonia, CO2, H2SO4, H2S)...silver has the bad habit to turn dark grey/black upon time...but this will normally not lead to connectivity troubles only a % reduction (how much I don't know).

In theory from all what is explained here above...mixes with larger spherical particles will be less prone to static...and flakes will increase static because of their sharp edges at the end of the plannar surface acting like a pin point all arround the flake.



[Edited on 28-2-2017 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1383
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 28-2-2017 at 12:55


Speculating here, but for large sparks, it is also a requirement that the charge can move quickly towards the point of discharge.
That is why you can get long bright sparks from the metal sphere from a van der graaf accelerator, but not from the bottom plastic roller even though the amount of charge stored in each should be roughly the same.

Translating that to your question, at higher concentrations of metal powder, bigger networks of interconnected particles can form that can transport a larger amount of the charge stored in the powder quickly to the location where it is dissipated in the form of a spark.

Maybe adding a poorly conducting powder (graphite?) will help, by dissipating the energy gradually along the way as ohmic heating rather than as a localised, high-energy spark?




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 1-3-2017 at 05:06


Quote: Originally posted by phlogiston  
Speculating here, but for large sparks, it is also a requirement that the charge can move quickly towards the point of discharge.
That is why you can get long bright sparks from the metal sphere from a van der graaf accelerator, but not from the bottom plastic roller even though the amount of charge stored in each should be roughly the same.

Translating that to your question, at higher concentrations of metal powder, bigger networks of interconnected particles can form that can transport a larger amount of the charge stored in the powder quickly to the location where it is dissipated in the form of a spark.

Maybe adding a poorly conducting powder (graphite?) will help, by dissipating the energy gradually along the way as ohmic heating rather than as a localised, high-energy spark?

Graphite comes into line of my proposal to increase the conductivity of the media...

This can be done for example:
-by moisturizing (but is detrimental to sensitivity and initiation)...
-by increasing the amount of metallic powder (but then detrimental to OB)...

Graphite spray is known to be used to render certains surfaces a-static...it is used for example when making O2/Acetylen baloons because of the inherent risk of detonation induced by static on such a sensitive and powerful gas mix.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2017 at 08:56


Yes, my experiments are showing that graphite may be valuable.... I just wish there was an easy non expensive way to test static sensitivity... The only way I know of is using a BBQ Piezo spark..
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 2-3-2017 at 15:30


Quote: Originally posted by MineMan  
Yes, my experiments are showing that graphite may be valuable.... I just wish there was an easy non expensive way to test static sensitivity... The only way I know of is using a BBQ Piezo spark..

You need a device that can variate the electric field/charge and the distance --> a "sparker gapper" if I may name it so...
The gap/distance when the spark is triggered defines the charge of the metallic ball and the energy provided by the spark.

To make one maybe get inspiration from a Van der Graaf device or a static charge holding bottle.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
gregxy
Hazard to Others
***




Posts: 421
Registered: 26-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 7-3-2017 at 14:25


Commercial smokeless powder reduces static sensitivity by coating the grains with graphite. This increases their conductivity (you can measure it with an simple ohm meter through lightly compressed powder in the 1000 ohm range)

The electrical power is P=I^2*R reducing R reduces the heating in the powder so the electrical power ends up being dissipated "somewhere else" in the circuit, probably in the air above the powder.
View user's profile View All Posts By User

  Go To Top