Author: Subject: Solvent for metals
veerenyadav
Harmless
*




Posts: 30
Registered: 1-3-2014
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2017 at 02:54
Solvent for metals


Which solvent can be most effective for metals ?

I tried to leach solid dust of metals with Fe, Mn, Si, Al, etc . But I could not leach out these effectively.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6241
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 27-5-2017 at 03:47


Acids "dissolve" metals in the sense that they react with them and oxidise them to ionic species.
Strong alkaline solutions also work similarly for amphoteric metals (eg, Al, Zn).

But for dissolving in the sense that I think you mean, you need a liquid metal. Both mercury and hot lead are used in some applications.

It would help if you explained what it is you were trying to do.
View user's profile View All Posts By User
gdflp
Super Moderator
Thread Moved
27-5-2017 at 04:29
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-5-2017 at 02:43


Are you trying to extract the metals for analysis?
View user's profile View All Posts By User
Elemental Phosphorus
Hazard to Others
***




Posts: 184
Registered: 11-11-2016
Location: Is everything
Member Is Offline

Mood: No Mood

[*] posted on 28-5-2017 at 05:44


Depending on the metal, some chemicals form a complex with metals like cyanide and gold, which could be used to leach them. As jsum said, other metals can amalgamate some things. If you would tell us what metal you are trying to leach, it would be a lot easier to give help.
View user's profile View All Posts By User
veerenyadav
Harmless
*




Posts: 30
Registered: 1-3-2014
Member Is Offline

Mood: No Mood

[*] posted on 3-6-2017 at 05:06


I have impure metal powder and want to leach pure metal but leaching is too slow using combentional acids. So searching alternatives ? Suggest any ?
View user's profile View All Posts By User
Elemental Phosphorus
Hazard to Others
***




Posts: 184
Registered: 11-11-2016
Location: Is everything
Member Is Offline

Mood: No Mood

[*] posted on 4-6-2017 at 09:59


It depends what metals the powder contains. What metal is it that you want to leach? If it is gold I would recommend cyanide or thiosulfate, but if it is a more easily dissolved metal, try dissolving in concentrated nitric acid if you have not already.
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 4-6-2017 at 15:43


This dissolving metal majes me tgink of recoverable metal desolved such as sodium in mercury or lead. Aluminium desolved in gallium
View user's profile View All Posts By User

  Go To Top