After watching the oleum from Sodium bisulfate thermal process work done by Hennig Brandt with his nifty quartz tube retort, and this work with
phosphoric acid in borosilicate glass- I had a couple of thoughts
If you were needing a bit more than these smallish quantities but did not care to invest in larger vessels? (Apparently the pyrex is a CONSUMABLE,
replacements could get expensive, plus the increased joy of having a LARGE one fail at operating temperature...)
The 85% phosphoric acid (H3PO4) used to make HPO3 is not consumed, but takes up the water from the strong sulfuric acid and is mostly re converted to
H3PO4. If a vessel suffiently robust and non reactive were used, could it not merely be disconnected from the condenser and oleum collection vessel,
the heating continued and increased to the point of driving off the water again and regenerating the HPO3?
One could then do a cyclic process, adding more 98% H2SO4, distilling SO3, disconnect collection equipment, re constitute to HPO3, add more H2SO4, re
connect to condensor/collector, distill the next increment of SO3 and so on, ad infinitum? Never needing to remove the H3PO4 from the aparatus until
you had made yourself howevee much oleum you required?
Would quartz glass or Vycor be sufficiently resistant to heat, acid mixtures and SO3 for cycling in this fashion?
|
|
|
Magpie
lab constructor
   
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Yes, the recycling of H3PO4 is possible, and was mentioned by garage chemist.
I have never used vycor but have used quartz at high temperature to make oleum.
There is an Amish glassblower in Pennsylvania who has fabricated quartz retorts for me at a very reasonable price. Just send him a sketch of what you
want.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
|
byko3y
National Hazard
  
Posts: 721
Registered: 16-3-2015
Member Is Offline
Mood: dooM
|
|
Carbon, graphite and gold are the only common material capable of withstanding hot phosphoric/metaphosphoric acid. Platinum and silver won't work for
that btw.
Quartz can hold the hot phosphoric acid up to 250 C without noticable destruction, while borosilicate is usable only below 200 C.
To make metaphosphoric acid you need either vacuum and 300 C, or 350-400 C at atmospheric pressure. But at these temperatures carbon, graphite, gold,
and platinum all will be attacked by sulfur trioxide.
There's a similar problem with controlled nuclear fusion.
|
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Quote: Originally posted by byko3y  | Carbon, graphite and gold are the only common material capable of withstanding hot phosphoric/metaphosphoric acid. Platinum and silver won't work for
that btw.
Quartz can hold the hot phosphoric acid up to 250 C without noticable destruction, while borosilicate is usable only below 200 C.
To make metaphosphoric acid you need either vacuum and 300 C, or 350-400 C at atmospheric pressure. But at these temperatures carbon, graphite, gold,
and platinum all will be attacked by sulfur trioxide. | Please explain how the acids attack the materials.
What are the equations for the rxns?
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2932
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
Silicon carbide is apparently used for some of these kinds of extremely corrosive solutions.
https://www.gab-neumann.com/Corrosion-resistance-of-sintered...
Less than one micrometer per year in 85% H3PO4 or 98% H2SO4 at 100 C is a good outlook. Boron carbide also has similar properties; this book reports
that H2SO4 + H3PO4 + CrO3 attacks it, but maybe in the absence of chromates it would be more resistant:
https://books.google.com/books?id=px_yCAAAQBAJ&pg=PA80&a...
|
|
|
MrDoctor
Hazard to Others
 
Posts: 250
Registered: 5-7-2022
Member Is Online
|
|
one thing im not clear on; at what actual temperature does the metaphosphoric acid dehydrate the sulfuric acid? and to what degree?
My understanding is that if not fully consumed, the hydrated phosphoric acids should still be a solid yes? in which case, is there a scenario wherin
you can mix your acids, heat to a degree that wont eat borosilicate, or quartz if that is more resistant and wont suffer any corrosion, to produce
merely 100% water-free sulfuric acid, without distilling it, and then just accept that wholesale, decanting/filtering, with some phosphoric acid
contamination as well as the salts of, at this point most likely copper or iron.
Also, i had this really stupid idea, im not sure if it would work, i just thought, if metaphosphoric acid is a rather glass-like substance, what if
one were to melt it in a crucible and coat it in the acid? at high temperatures where the acid is solid enough to hold its shape, could equally hot
sulfuric acid be dripped into the crucible, causing a instant reaction releasing SO3 without having sulfuric acid exist in the liquid phase, meaning
that the materials for the assembly might not need to resist liquid sulfuric acid.
such a reaction might be pushed forward additionally by performing this all under vacuum, which i believe wasnt previously an option since the temps
are too high to safely apply hard vacuum in borosilicate, and quartz is attacked too easily to be worthwhile either.
batch yields would be terribly low, also im not sure how you address the hydrated phosphoric acid either, but this does allow for moderate temperature
and hard vacuum with, theoretically no damage to any glassware or exceptionally high temperatures either for that matter.
|
|
|