CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
Good sources of cerium
I've recently began studying the lanthanides more closely and I learned that Ce (IV) is a very strong oxidizer with very interesting properties which
can replace KMnO4 (which is completely banned in Romania; it is treated the same as red P or iodine are treated in the US) in many situations. What
would be a good source of this metal/its compounds? CeO2 is sold dirt-cheap as a cleaning powder, but I'm afraid that might be calcined so much that
it doesn't react with anything. Another possible source are the ferrocerium rods, which contain iron, cerium and smaller amounts of other lanthanides,
but, as far as I'm aware, extracting cerium from them would require first dissolving them in dilute nitric acid (or sulfuric acid if you have access
to M(NO3)2 where M has an insoluble sulfate; I don't), then oxidizing Ce(NO3)3 to Ce(NO3)4 with hydrogen peroxide and then extracting this salt with
light naphtha (or any other non-polar solvent; I chose light naphtha because it is very cheap here), but this method wastes valuable nitric acid.
TL;DR: What cheap source of cerium do you recommend? Is cleaning CeO2 good? Is there an OTC method of extracting cerium from ferrocerium rods? (dilute
H2SO4 is the cheapest acid here, light naphtha is the cheapest non-polar solvent)
|
|
|
j_sum1
Administrator
      
Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline
Mood: Just got through yet another "take this job and shove it" moment.
|
|
Onyxmet.
|
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
I know the site, but the price for cerium salts is huge (at that price I'm better off doing the extraction from ferrocerium)! Also, I've heard the
CeO2 they have (which is more reasonably priced) is unreactive.
[Edited on 27-5-2018 by CobaltChloride]
|
|
|
diddi
National Hazard
  
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
what about lapidary grade cerium oxide?
Beginning construction of periodic table display
|
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
That is what I was referring to when I was talking about "cleaning CeO2". My question is: is the material reactive towards aqueous acids or is it so
calcined that it becomes unreactive?
|
|
|
Dr.Bob
International Hazard
   
Posts: 2918
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
Ceric Ammonium Nitrate is used in many labs, that would be my first thing to try to find a sample of if I wanted a pure cerium compound. It is often
used for visualizing TLC plates and other oxidations.
|
|
|
DavidJR
National Hazard
  
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Quote: Originally posted by Dr.Bob  | | Ceric Ammonium Nitrate is used in many labs, that would be my first thing to try to find a sample of if I wanted a pure cerium compound. It is often
used for visualizing TLC plates and other oxidations. |
I would quite like to buy some but I haven't found anywhere that will sell it to me.
|
|
|
Bert
Super Administrator
       
Posts: 2822
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Ceric Ammonium Nitrate on Amazon
Or from Chemsavers?
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
|
ninhydric1
Hazard to Others
 
Posts: 345
Registered: 21-4-2017
Location: Western US
Member Is Offline
Mood: Bleached
|
|
Maybe you could try electrolysis with a ferrocerium rod in, say, sulfuric acid. Wikipedia states that cerium readily dissolves in dilute sulfuric
acid, so I don't think that nitric acid is needed. Iron can be readily dissolved by HCl, so that shouldn't be a problem.
The philosophy of one century is the common sense of the next.
|
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
I chose nitric acid because only Ce(NO3)4 has the property of being soluble in nonpolar solvents. Ce(SO4)2 isn't soluble in nonpolar solvents. If
anyone has a better method of separation, I'm all ears.
|
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
Again, these are a lot more expensive than just extracting from ferrocerium rods or buying ceric ammonium nitrate from onyxmet.
|
|
|
indigofuzzy
Hazard to Others
 
Posts: 145
Registered: 1-10-2006
Location: DarkCity, Bay of Rainbows, Moon
Member Is Offline
Mood: Distilled
|
|
Ferrocerium rods will dissolve readily in HCl.
If you get the stoichiometry right, only the cerium and other stray lanthanoids will dissolve, and the iron will be displaced out of solution as a
black powder.
|
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Plz recommend brands of cleaning powder that contain decent amount of CeO2. Ive never heard of this fact.
|
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Ferrocerium actually contains a significant bit of La (something like 50% Ce, 25% La, balance Fe/Mg if I recall, though that's a very uncontrolled
recipe so it can vary quite a bit).
'Cleaning cerium' doesn't refer to any cleaning product, but rather a polishing slurry used for stones and other hard lapidary substances. From my
experience, it isn't terribly reactive, but you can force it by reacting with magnesium or another reducing agent, dissolving the resultant mixture of
magnesium and cerium compounds in an acid of your choice, and separating the magnesium.
What's more fascinating still is that certain brands of pool phosphate remover are, apparently, pure lanthanum chloride in aqueous solution. I've
boiled these down and got a clean white precipitate with little trouble (though I haven't verified its contents just yet).
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
What kind of pool phosphate remover has LaCl3? Why would you use such an expensive (because of the cost of the separation from other lanthanides)
chemical for a pool?!
@fusso search for "cerium oxide" on ebay or aliexpress and you'll get a lot of offers for CeO2.
|
|
|
Dancing Rain
Harmless
Posts: 5
Registered: 26-11-2017
Member Is Offline
Mood: Electrorefined
|
|
| Quote: | | What kind of pool phosphate remover has LaCl3? |
It's called PhosPrevent, and is readily available from pool supply stores in Portland OR. Your mileage may vary elsewhere.
I'm going to try to extract lanthanum metal from it as soon as my budget permits.
|
|
|
wg48
National Hazard
  
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Nice find DR.
I am surprised too that lanthanum chloride is used for something as mundane as precipitating (presumably) the phosphate out of pool water.
I found an msds for a similar product called PhosFree. It states it contains 26.52% LaCl3
I also found PhosFree on sale at fruugo.co.uk about £50 for 3 litres + about £50 delivery. About £10 for 80g of LaCl3.
LaCl3 is also sold on Ebay UK. The best price I could find was about £30 for 100g
Attachment: phosfree-extra-strength-msds.pdf (138kB) This file has been downloaded 462 times
|
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
I can't quite recall the product name that I came across, but I do remember it was available at Walmart (~$8 for 16 fl. oz.) and claimed 60% lanthanum
chloride in solution. Precipitation with sodium hydroxide yielded a gelatinous, white precipitate that dried to give a crumbly, brittle powder
(La(OH)3, if I'm right). The white color indicates that it doesn't contain Nd, Ce, Pr, or other rare earth contaminants in any appreciable amount.
What is your plan for extraction, Dancing Rain? I seem to recall MrHomeScientist attempting neodymium from its oxide a while back, with... limited
success. I was thinking electrolysis in propylene carbonate, but that would first require dehydration of the hydrated chloride (unfortunately
difficult due to formation of useless oxychlorides).
[Edited on 6/12/2018 by elementcollector1]
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
|
violet sin
International Hazard
   
Posts: 1501
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
The HTH brand of pool supply chemicals has theirs listed as 35-65% lanthanum salt and 65-35% water. Clorox brand is 6-10%, so.... There seems to be
some variation in composition. Yet another brand had no named substance as it wasn't considered toxic enough... That doesn't sound good. I've been
tempted to buy before, but due diligence may be required as it's not the cheapest stuff.
|
|
|