Iron oxide
im going to make red iron oxide by first putting steel wool in water with a little bit salt in. after more a less a day i'll heat the iron
hydroxide in the oven and then i obtain red iron oxide. will this work? is it simplier to use hydrochloric acid, and then put it in lye and then let
it oxidize in air or add hydrogen peroxide and heat it in the oven? and if ihave it in water, how do i see it's done? iron hydroxide is grey too.
very thankful for answers
[Edited on 23-10-2005 by The_Simpsons]
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Er, easier and cheaper to take scrap iron, add water, sulfuric acid (or hydrochloric) and a bubbler. The ferrous sulfate/chloride formed is oxidized
by air to ferric, releasing drab orange ferric hydroxide; the iron metal then reduces the ferric ions in solution to ferrous (thus the salt is a
catalyst). Calcine the orange rust to a reddish brown ferric oxide (rouge) product.
You could do worse than oxidize an iron anode in a salt solution. Mind that the product is very adsorbent and you have to calcine it near red heat
before washing will remove the remaining salt.
Tim
|
|
The_Simpsons
Harmless
Posts: 15
Registered: 17-7-2005
Location: Falun, Sweden
Member Is Offline
Mood: No Mood
|
|
thanks, english isn't my first language, what is scrap iron?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Scrap iron is iron that has been used and would now be waste or sent for recycling. Old nails, rusted fence wire... anything that is made from iron
but is rubbish.
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Scrap iron is every American car that gets less than 30 miles per gallon at today's fuel prices.
|
|