Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Ferrosulphate
lipiman
Harmless
*




Posts: 4
Registered: 10-11-2005
Member Is Offline

Mood: No Mood

sad.gif posted on 10-11-2005 at 03:26
Ferrosulphate


Hi, good day everybody. Right now I have some problem with my ferrosulphate. The color of my ferrosulphate has already changed to brown. Ferrosulphate should be green color. Does anyone have any idea for me to make the color change to green?
Thanks.
View user's profile View All Posts By User
Darkblade48
Hazard to Others
***




Posts: 411
Registered: 27-3-2005
Location: Canada
Member Is Offline

Mood: No Mood

[*] posted on 10-11-2005 at 03:33


Well, from google, the MSDS says:


Quote:

Stable under ordinary conditions of use and storage. Looses water in dry air and oxidizes upon exposure to moisture, forming a brown coating of extremely corrosive basic ferric sulfate.


Were you storing it in a non-closed container of some sort (thus allowing it to become oxidizied)?
View user's profile View All Posts By User