any one know iron phosphate melting point ?
any one know
|
|
icelake
Harmless
Posts: 48
Registered: 9-10-2017
Member Is Offline
Mood: No Mood
|
|
Take this with a grain of salt.
https://www.carlroth.com/downloads/sdb/en/9/SDB_9358_MT_EN.p...
m.p: > 450 °C
Decomposition temp: 500 °C
ps: It says Iron(III) phosphate hydrate, but Mw = 150.8 says otherwise.
|
|
rockyit98
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline
Mood: no mood is a good mood
|
|
even if decompose ,which i don't think it dos ,the anhydrous salt is use to make type of glass (Iron(II) phosphate
Iron(III) phosphate )called phosphate glass (https://en.wikipedia.org/wiki/Phosphate_glass)
|
|
rockyit98
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline
Mood: no mood is a good mood
|
|
found it https://scholarsmine.mst.edu/cgi/viewcontent.cgi?article=295...
|
|