e waste precious metal refining
Dear sir . Fine metal refining by aquaregia process the photo attachment color received give a suggestion for pricipitating gold
|
|
TmNhRhMgBrSe
Hazard to Others
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
Sodium metabisulphite.
Go youtube, search sreetips, watch his vids. He has a bunch of gold refining vids.
|
|
gdnaiudu
Harmless
Posts: 2
Registered: 2-8-2019
Member Is Offline
|
|
DEar all, after filtration of brow precipitate washing with hot water as shown attachment out put ur suggestion could help me come to an
conclusion of refining it