Author: Subject: Potash from Charcoal Ashes
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2019 at 11:11
Potash from Charcoal Ashes


I know potash can be recovered from wood ash, but can it be made from charcoal ash? Charcoal comes from wood, after all.

I have a ton of ashes from years of grilling that I was about to throw away, but thought it might be cool to try extracting potash from it. Obviously not a great way to get reagents, but could be a fun experiment.
View user's profile Visit user's homepage View All Posts By User
Pumukli
National Hazard
****




Posts: 724
Registered: 2-3-2014
Location: EU
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2019 at 11:44


Yes. :)
If you have lots of it as you wrote, it may worth trying.
View user's profile View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 30-8-2019 at 16:38


Give it a try, but be aware that yields vary greatly with the kind of wood.

Oak works great, cedar quite badly.

Some charcoal briquets are made from culm (waste coal powder and pieces), and I don't know how the potash content of that is.




View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3942
Registered: 8-2-2015
Member Is Offline


[*] posted on 30-8-2019 at 17:34


A couple of years ago I did similar ... the ashes saved from many bbq left to soak in a large bucket of water.
Some time later my wife informed me that she had helped to tidy up the area,
and cleaned out that messy bucket :(

So that's one mistake to not make :P




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 31-8-2019 at 00:47


Justus Liebig wrote: You can get more pottash from the plants beside the road than if you burn down an forrest for it.
Wormwood. 35-45% Pottash
Thistle. 30-35%
Sunflower 15-25%
View 15-20%.
I think oakwood ash has only 5% and needle trees below 3%.
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 31-8-2019 at 01:12


Indeed, potash comes from burnt green plant matter!

View user's profile View All Posts By User
Carbon8
Harmless
*




Posts: 34
Registered: 1-1-2018
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2019 at 11:10


Here's a partially-gated link that compares potash recovery from charcoal ash and tobacco ash:

https://pubs.acs.org/doi/10.1021/ed024p231

Here's a partially-gated link that discusses the first link:

https://pubs.acs.org/doi/10.1021/ed038pA612.3

It is also possible to titrate the potassium carbonate in ash without isolating it. Here's a gated link:

https://scholar.google.com/scholar?hl=en&as_sdt=0%2C5&am...

It might be interesting to do a video comparing the recovery of potash and soda ash from various charcoal ashes, wood ashes and seaweed ashes.
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 3-9-2019 at 06:23


Well I gave it a shot this weekend. I filled a gallon jug with 1 kg of ash and added distilled water until it was roughly halfway full. After vigorous shaking and allowing to stand for a couple days, the solution is very basic (>10). Promising!

Thanks for the links Carbon8. That would make a cool video. The first link found charcoal ash to contain 19% potash; I'll have to see how mine compares.
View user's profile Visit user's homepage View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 4-9-2019 at 03:53


i recall leaves were something like 3x as concentrated in potassium as regular wood, so sign yourself up for collecting leaves as weekend gig
thistle is great if you can come by it, wormwood, if you ask me is not really doable because it doesnt grow a whole lot of places, i have an idea that plants who feature some pink/purple components may contain reasonable amounts of potassium but this is pure assumption.

i recall unburnt wood soaked in water was used back in time to produce NaOH, so let it stand for a bit and you would end up with the corresponding carbonate




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User

  Go To Top