Different types of iron powder


Electrolytic iron powder, Carbonyl iron powder and regular iron powder

Even if they are equally pure, they have different capacity to reduce nitroalkene to ketone. Why is that, I can't figure out even after an hour Googling.

The carbonyl iron powder has, without a doubt, better reducing capacity per Mol eq than electrolytically manufactured or regular very pure iron powder (Fischer, +99.9% purity). Why is that? I don't understand what difference their actions are in chemistry.

And is it same with zinc reductions, is the shape / type of particles of the metal relevant to the reducing capacity of the zinc?
View user's profile View All Posts By User
valeg96
Hazard to Others
***




Posts: 254
Registered: 6-4-2014
Location: Italy
Member Is Offline

Mood: Moodless

[*] posted on 20-12-2020 at 15:14


Probably the specific surface. Nickel and iron made by decomposition of their carbonyl compounds are very, very pure and fine, with a huge area where the reaction can take place.




View user's profile Visit user's homepage View All Posts By User
RustyShackleford
Hazard to Others
***




Posts: 195
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline


[*] posted on 20-12-2020 at 15:44


surface area, assuming everything else is equal. Its the same with zinc and any metals that work by similar mechanism
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

[*] posted on 20-12-2020 at 18:32


Carbonyl iron powder used to make iron powder toroidal inductors and transformers. also to make experimental alloys in the laboratory hence need for inert atmosphere handling. for reduction just ballmill steel swarf from machining shop.