Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Purity test for grocery Ca(NO3)2
kazaa81
Hazard to Others
***




Posts: 368
Registered: 30-4-2004
Member Is Offline

Mood: ok

shocked.gif posted on 8-5-2006 at 15:03
Purity test for grocery Ca(NO3)2


I came around 5kg bags of Ca(NO3)2 in pottery, but I'm not sure of it's purity. It's a white powder, but the stange thing is that on the bag aren't wrote N contents and/or purity.
Just a big "Calcium Nitrate".
It seems strange that it's 95+% pure or something like that, of course for pottery things 45% is enough...otherwise too much N will come to grass etc.

Can anyone suggest me a test about purity? Even because I couldn't imagine how to purify, if I don't know what is and in what conc.
View user's profile View All Posts By User
skippy
Harmless
*




Posts: 35
Registered: 10-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 8-5-2006 at 16:11


If it says 95% pure, it probably is at least that pure. Does it all dissolve? Anything that doesn't dissolve definately isn't calcium nitrate and that would be one easy thing to isolate

It was made by reacting nitric acid with calcium carbonate, and whatever soluble impurities are present are probably those that were in the neutralized limestone (calcium carbonate). Maybe some magnesium? How pure do you actually need it to be? 95% is probably fine for many uses.
View user's profile View All Posts By User
kazaa81
Hazard to Others
***




Posts: 368
Registered: 30-4-2004
Member Is Offline

Mood: ok

[*] posted on 8-5-2006 at 16:39


Yes, 95% is very good purity for me....however, maybe you don't caught the problem....the bag is without writings, except a big "Calcium Nitrate" on the front, but that's all...no tables, purity etc.

[Edited on 9-5-2006 by kazaa81]
View user's profile View All Posts By User
guy
National Hazard
****




Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline

Mood: Catalytic!

[*] posted on 8-5-2006 at 17:00


Dissolve a sample and try precipitating it. Mass the precipitate and see how it compares with the stoichiometry.



View user's profile View All Posts By User
kazaa81
Hazard to Others
***




Posts: 368
Registered: 30-4-2004
Member Is Offline

Mood: ok

[*] posted on 8-5-2006 at 17:18


Precipitate? maybe dissolve in water and then crystallize
View user's profile View All Posts By User
guy
National Hazard
****




Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline

Mood: Catalytic!

[*] posted on 8-5-2006 at 17:20


I mean dissolve, then treat with carbonate or something. Make sure to wash the precipitate to make it as pure as possible.



View user's profile View All Posts By User
skippy
Harmless
*




Posts: 35
Registered: 10-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 9-5-2006 at 04:25


I'm not so sure now if it is made from limestone. It can be made (evidently) from phosphate rock. They suck out the calcium (along with any impurities, I'm sure) from the phosphate rock. This also facilitates making phosphate fertilizers

Is there no manufacturer or packager contact on the bag? If so maybe you could phone? Lord knows that would be easier than trying to analyze it yourself.

I think that Sweden makes a lot of nitrate fertilizers and maybe you could learn something from this angle. http://www.idswater.com/water/europe/Yara_international_asc/...
View user's profile View All Posts By User
kazaa81
Hazard to Others
***




Posts: 368
Registered: 30-4-2004
Member Is Offline

Mood: ok

[*] posted on 9-5-2006 at 05:53


Quote:
Originally posted by skippy
It was made by reacting nitric acid with calcium carbonate, and whatever soluble impurities are present are probably those that were in the neutralized limestone (calcium carbonate). Maybe some magnesium? How pure do you actually need it to be? 95% is probably fine for many uses.


Impurities? I don't think that a fertilizer supplier would make a ton of 99% Ca(NO3)2 and sell you 99% in 5kg bags at pottery...I think that it would dilute the ton and make at least 2 tons of 50% Ca(NO3)2 and sell it. So impurities are not only by the process, but also added.
View user's profile View All Posts By User
DrP
National Hazard
****




Posts: 625
Registered: 28-9-2005
Member Is Offline

Mood: exothermic

[*] posted on 9-5-2006 at 06:10


What would they add - CaCO3? Dolomite? If for pottery then something more heat resistant for firing like a cheap mullite or something?

I rekon the same as skippy anyway - ring the manufacturer (or supplier) - they should know the purity.
View user's profile View All Posts By User
Ramiel
Vicious like a ferret
***




Posts: 484
Registered: 19-8-2002
Location: Room at the Back, Australia
Member Is Offline

Mood: Semi-demented

[*] posted on 9-5-2006 at 19:01


You could precipitate the Calcium as an insoluble salt… I’d be worried about error here, how much of the salt is still in solution? Gravimetric analysis is very finicky in the first place (requiring accurate scales and expensive filtering – sintered glass filters and vacuum filtration is ideal). At large scale, sulphuric gravimetric would work okay – since I guess magnesium would be the largest contaminant.
I could recommend a titration, and I know it sounds tedious at first for the home experimenter, but if you really want to find out the purity [and IMHO, titrations are <i>always</i> quicker and easier than gravimetric!].

As for nitrate… total kjeldahl nitrogen if you are sure it’s all nitrate, or a metal oxidation titration to determine nitrate?




Caveat Orator
View user's profile View All Posts By User This user has MSN Messenger
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 16-5-2006 at 11:13


"You could precipitate the Calcium as an insoluble salt… I’d be worried about error here, how much of the salt is still in solution?"
Er, pretty much none, otherwise it doesn't really count as an insoluble salt.

While it's interesting to speculate on the purity and on the nature of the possible contaminants, who cares?
If it's cheap, buy some and try to use it. If it works then it's pure enough. If not, then I guess you might need to recrystalise it or some such. If the use involves heating it with nitric acid you might want to do it on a very small scale first.
View user's profile View All Posts By User