hodges
National Hazard
  
Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline
|
|
Getting rid of mineral oil in calcium samples
I purchased some calcium metal (many small nuggets) from an online auction site. I didn't realize that it would be packed in mineral oil. In the
past when I have purchased calcium nuggets, they were just packed in an airtight bottle.
I use calcium as a reagent for various purposes, and the mineral oil is definitely not good news. It affects the mass when I am weighing out the
calcium, and contaminates reactions.
Is there an economical way, that does not involve trying to vaporize it, to get rid of the mineral oil? My first thought would be to decant off as
much of the mineral oil as possible, then wash with an easily evaporated non-polar solvent to wash away the mineral oil. Acetone comes to mind. But
my concern would be that store-bought acetone probably contains a non-negligible amount of water, which would likely react with the calcium. Any
thoughts? I did not pay too much for the calcium, so perhaps it would be better to just order more from another supplier. But if there is an
inexpensive way to clean it up I would rather do that.
|
|
|
Rainwater
National Hazard
  
Posts: 993
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
I was going to say, melt some in a test tube, then insert a wire and let it harden. But after reading the melting point of 842c, i see that isnt going
to work.
Maybe a reflux with dioxane? I know it works with sodium, and i believe other group 1 metals.
Its easy enough to make inside of a few hours with the right equipment. Maybe try a very small sample to start with.
"You can't do that" - challenge accepted
|
|
|
Admagistr
Hazard to Others
 
Posts: 395
Registered: 4-11-2021
Location: Central Europe
Member Is Offline
Mood: The dreaming alchemist
|
|
I recently offered high purity calcium here on the Forum that has never been stored under any oil....The offer still stands
|
|
|
Admagistr
Hazard to Others
 
Posts: 395
Registered: 4-11-2021
Location: Central Europe
Member Is Offline
Mood: The dreaming alchemist
|
|
Otherwise, I was approached years ago by a friend who is a professional seller of high purity chemical elements asking for advice on how to degrease
reactive metals stored under paraffin oil before fusing it in a glass ampoule under argon... Gasoline came to my mind... A few days later he wrote me
enthusiastically that it was a great idea and he had managed to degrease this metals perfectly, using a cleaner of gasoline...
|
|
|
dawt
Hazard to Self

Posts: 74
Registered: 9-5-2016
Location: EU
Member Is Offline
Mood: fluorescent
|
|
Yep, that works great for degreasing reactive metals. Whenenver I use sodium I dump the freshly cut pieces into a small beaker with petrol ether
before transferring them to the reaction flask.
|
|
|
Tsjerk
International Hazard
   
Posts: 3040
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Petroleum ether works without leaving behind residual crap, as part of the production process is distilling.
Acetone from the store is usually dry. I don't know how it is produced, but the process ensures a dry product.
Just wash the calcium with some solvent. Adding mineral oil is common practice to many air/water sensitive chemicals, as washing away the oil is easy
and leaves few traces as long as the solvent used to do so is clean.
I never worked with gasoline, but I wouldn't use it without distilling it as I don't know what high boiling stuff is in there.
Also, maybe not calcium, but e.g. with sodium, more complex aromatics might react with the metal, making complex mixtures like gasoline unsuitable.
[Edited on 5-2-2022 by Tsjerk]
|
|
|
Dr.Bob
International Hazard
   
Posts: 2900
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
Hexane is a great solvent for washing alkali metals (and sodium hydride) of oil. But then be careful to put the used solvent in a place that is safe
in case it catches fire. It sometimes gets a little material in it and that will spark in humidity. Two washes or rinses in hexanes, and your
metal will be clean enough for most purposes.
|
|
|
hodges
National Hazard
  
Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline
|
|
Thanks for the replies.
I bought some "100% acetone" (nail polish removed) and tried it with a small sample of the calcium. There was no reaction, so I decanted as much of
the mineral oil as possible and then used the acetone to wash the calcium.
I found that the mineral oil and acetone are not miscible. However, the mineral oil is washed off by the acetone and can also be poured off. After
several washes, I left the calcium to dry in open air for a bit, then put it back in its bottle. There is still a slight acetone smell, but the
calcium is now clean and dry and shakes easily in the bottle. I am leaving the cap on loosely so the remaining acetone vapor can dissipate.
|
|
|