Author: Subject: Possibility of electrolytic lithium metal production in organic solvents (do it like a battery)
experimenter_
Harmless
*




Posts: 38
Registered: 18-2-2016
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2022 at 10:07
Possibility of electrolytic lithium metal production in organic solvents (do it like a battery)


It is known that lithium can be isolated electrolyticaly from its molten salts. But there could be an easier and safer method to produce lithium metal by electrolysis of its salts dissolved in an organic solvent.

The process is performed routinely inside Li-ion batteries or LiFePO4.

Lithium is intercalated inside the graphitic electrode of the anode during charging. Intercalated lithium may be difficult to use but under some special conditions it can be electroplated as a metal outside:

https://www.upsbatterycenter.com/blog/lithium-plating/

In older Li-ion batteries lithium metal was used as the anode and it seems that direct electroplation of lithium onto that anode was the norm

https://en.wikipedia.org/wiki/Lithium-ion_battery#History

Why isn't anyone making lithium with this method? Are the required organic solvents so difficult to get hold of?

https://www.sciencemadness.org/whisper/viewthread.php?tid=10...


View user's profile View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 14-2-2022 at 13:53


1 Dissolve LiCl in Pyridine.
2 Run current through it
3 ????
4 Profit!




View user's profile View All Posts By User
experimenter_
Harmless
*




Posts: 38
Registered: 18-2-2016
Member Is Offline

Mood: No Mood

[*] posted on 15-2-2022 at 09:44


People have filled up 66 pages about making "unconventional" sodium or potassium with crazy methods. I think this method for lithium worths being investigated. I'm sure there are various attempts around the forum that were unsuccessful. I just haven't stumbled accross them yet to be discouraged enough.

[Edited on 15-2-2022 by experimenter_]
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 993
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 15-2-2022 at 14:14


And the man with google connections Slowly slipps a folder under the table while not at all looking suspicious. Then abruptly wishes you good luck and leaves.
Could be born. Or plans for morld bomination.

Attachment: bf00610946.pdf (769kB)
This file has been downloaded 353 times




"You can't do that" - challenge accepted