Barium chlorate cell
I've produced around 2 litres of saturated barium chloride solution by neutralising barium carbonate with HCL.
I have now set it up in a cell with an MMO anode and titanium cathode and so far i'm pushing 10amps through it.
I seem to be getting an insoluble layer at the bottom which i'm guessing might be residual barium carbonate which is sparingly soluble in water.
I'm planning to keep it running a few weeks and just keep topping it up with water then eventually allow it to evaporate and hopefully get some long
barium chlorate crystals.
|
|
|
mysteriusbhoice
Hazard to Others
 
Posts: 477
Registered: 27-1-2016
Member Is Offline
Mood: Became chemistry catboy Vtuber Nyaa
|
|
careful of any sulfate contamination as barium sulfate is known to fuck up MMO temporarily and soon long term if it builds up on the anode.
blinding deposits are removed by running the anode in acidic medium with high chloride.
|
|
|
Jome
Hazard to Others
 
Posts: 154
Registered: 10-6-2004
Location: Soutwest sweden
Member Is Offline
Mood: desiccated
|
|
If you get an insoluble layer, might that not be Ba(OH)2 from the bath going alkaline, since some Cl2 will inevitably be evolved?
|
|
|
Chemgineer
Hazard to Others
 
Posts: 240
Registered: 25-5-2021
Member Is Offline
|
|
This is progressing well, after 8 days of electrolysis i've poured it into a wide dish to evaporate and j'm getting good barium chlorate which
oxidises sugar in a bright green flame.
A really interesting thing is i'm seeing Triboluminescence and blue electrical flashes in the solution as crystals drop out of solution and then when
I break them apart later I see blue flashes again!
|
|
|
woelen
Super Administrator
       
Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Very interesting effect. I have some Ba(ClO3)2 and will try whether I can reproduce the triboluminiscence by dissolving some in hot watert and then
letting it crystallize on cooling down.
Be careful with Ba(ClO3)2 in pyrotechnics experiments. Mixes with it are really sensitive. I understood that these mixes are even more sensitive than