SbO2 anode


I see on Aliexpress someone is selling an SbO2 Ti substrate anode. Just out of interest, does anyone know what this is good for?
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 993
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 14-6-2022 at 10:23


In lithium battery is the only place ive heard of it being used as an electrode. Its also a fire retardant
Sb2O3 charges up to Sb2Ox then as the battery discharges the oxygen moves through a membrane to the lithium. Trying to remember were i read about it.




"You can't do that" - challenge accepted
View user's profile View All Posts By User
mysteriusbhoice
Hazard to Others
***




Posts: 477
Registered: 27-1-2016
Member Is Offline

Mood: Became chemistry catboy Vtuber Nyaa

[*] posted on 14-6-2022 at 19:02


this electrode is used as an inert substrate or used for O2 evolution but dont even try it for making chlorates cuz the efficiency is trash!!
its usually a mix of SnO2 and SbO2 thermally baked on Ti sheets at 450C similar to MMO which uses a blend of TiCl4 with ruthenium and iridium salts.
instead they have SnCl4 and SbCl3 in ethanol painted and baked on the activated Ti substrate.
These are usually also used if you wanna plate PbO2 on it but other than that or something like electroplating or electrowinning its shit.