Will Na-ion batteries eventually replace Li-ion ?
This online chemistry textbook page tells about the viability of sodium ion batteries. I have watched some Youtube videos about this (look for 'sodium
ion battery') most of which are recent (< 2 years old).
It looks promising, they even tell that Cobalt is not needed but Iron and Manganese.
What are your ideas ?
|
|
|
Herr Haber
International Hazard
   
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
You asked for it...
"Oh, manganese from my poop, the rest are readily available!".
More seriously I think I'll research some of these videos after dinner. Too many questions but it seems pretty interesting cost-wise.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
|
JGHFunRun
Harmless
Posts: 5
Registered: 11-7-2022
Location: [REDACTED]
Member Is Offline
Mood: V and Y are the best letters
|
|
Quote: Originally posted by Herr Haber  |
You asked for it...
"Oh, manganese from my poop, the rest are readily available!".
More seriously I think I'll research some of these videos after dinner. Too many questions but it seems pretty interesting cost-wise.
|
Yea... I'm gonna need context
HeH⁺ HeH⁺ HeH⁺ HeH⁺
|
|
|
j_sum1
Administrator
      
Posts: 6463
Registered: 4-10-2014
Location: At home
Member Is Online
Mood: Most of the ducks are in a row
|
|
Na will never achieve the charge to mass ratio possible with lithium. But if the tech develops, it should be a lot cheaper. So, applications in
stationary batteries with lithium for vehicles.
|
|
|
hexahydrate
Harmless
Posts: 15
Registered: 17-3-2018
Member Is Offline
Mood: No Mood
|
|
Apparently Sodium Ion batteries are already commercially available. Last year CATL announced their introduction to the market https://www.catl.com/en/news/665.html and advertised 160Wh/kg energy density. However they probably sell them to large customers only, so far. I
have yet to see Na-Ion battery available to individual customers.
|
|
|
brubei
Hazard to Others
 
Posts: 188
Registered: 8-3-2015
Location: France
Member Is Offline
Mood: No Mood
|
|
Sodium is less perfomant than lithium if used for mobility. It is still very competitive for domestic usage.
I'm French so excuse my language
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2913
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
I'm not exactly bullish. Sodium anodes are obviously more reactive than lithium anodes. This is something many of us have direct familiarity with.
The name of the game in grid batteries is manufacturing. Making the damn thing tends to be way more expensive than the materials going in. Therefore,
low energy density can impact the cost per kWh because you need more components per kWh. But more importantly, it's hard for amateurs to spitball what
technology is going to be easy to make.
There are a couple of technologies that might compete with lithium on scale: sodium-ion, potassium-ion, zinc-bromine, tetrachloroaluminate-ion, iron
sulfate, and the crazy-sounding "organic radical battery". I'm generally skeptical of any "flow" technology; moving parts are terrible.
|
|
|
Herr Haber
International Hazard
   
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Well, it's a bit childish... Back when I discovered KMnO4 and it's stains I thought "Oh, this looks just like sh**"
You asked for it 
That said, the research was interesting. As I may have said in other pages my second hobby is "everything underground".
Some people talk about their cars, me and my buddies talk about... who has the biggest. Flashlight of course !
So everything that has to do with batteries is interesting to me.
Na batteries dont seem as mature as Li but some companies seem to have built hybrids.
For me personnally the biggest issue seems to be the number of cycles they can go through even before the density.
It's interesting to check on developping technologies from time to time.
Greatest example are solar panels from the 90's and current panels: better lifespan, better output, etc.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
|
khlor
Hazard to Others
 
Posts: 112
Registered: 4-1-2014
Location: Who knows, really...
Member Is Offline
Mood: No Mood
|
|
I guess, that for mobile/vehicle applications sodium batteries might not fly. but stationary batteries might be right for it. I mean, power density is
low, but when wright is not a problem, you can stand the lower performance for a significant lower cost. there might be a niche for this market.
"NOOOOOO!!! The mixture is all WROOOOOOONG!"
|
|
|