| Pages:
1
2 |
Tsjerk
International Hazard
   
Posts: 3040
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
And that was not in a second package? You have to label it somehow.
|
|
|
DocX
Hazard to Others
 
Posts: 179
Registered: 22-10-2015
Member Is Offline
Mood: No Mood
|
|
Yeah, but preferably not with the reagent name slapped on the outside of the package.
Yes, that is Nitrochemis.
It's not my picture though. But the user who shared it with me gave the product and the seller official praise, he was just a little put off by the
packaging . I was just about to order from there, but this was an absolute
dealbreaker.
I have no interest in P2NP, I just wanted some nitromethane and nitroethane. But with labels like that ... I mean, it doesn't really matter if you're
Up To No Good or not, that kind of packaging warrants unwanted attention anyhow.
Luckily, there's solid alternatives. Not with the great prizes nitrochemis offers, but I'd rather pay a little more than have these things sent to me.
[Edited on 20222222/10/3 by DocX]
|
|
|
SuperOxide
National Hazard
  
Posts: 542
Registered: 24-7-2019
Location: Devils Anus
Member Is Offline
|
|
Me too.. well, and the fact that
they won't ship to anyone outside the EU. That made it an even easier decision, lol.
Quote: Originally posted by DocX  | I have no interest in P2NP, I just wanted some nitromethane and nitroethane. But with labels like that ... I mean, it doesn't really matter if you're
Up To No Good or not, that kind of packaging warrants unwanted attention anyhow.
Luckily, there's solid alternatives. Not with the great prizes nitrochemis offers, but I'd rather pay a little more than have these things sent to me.
|
I'm in the same boat. What solid alternatives are you talking about for nitroEthane?
The only two routes I know of to synthesize nitroethane are pretty low in terms of atomic efficiency. But I don't really need that much of it anyways
(honestly, I don't even have a specific use planned for it). But I'm curious what alternatives you're referring to.
|
|
|
Organikum
resurrected
   
Posts: 2344
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
The picture is from the nitrochemis webpage directly where they state that they take care to label and declare everything correctly. The picture is to
show how professionally it is packed. I asked a little bit around and this in the picture comes of course packed in another envelope or cardboard
box, this is not in plain sight for everybody handling the parcel, what would be not only unusual but most probably it would be against postal
regulations about everywhere.
I attach the original picture from Nitrochemis.com, which tells that it just proof for good packaging, something what is not always guaranteed at
other places.
In my opinion this is much better then to have unlabeled mystery crystals in a package as those would go to closer inspection for sure if the package
got opened. This now looks exactly like it should look like - professional, official and with all the right in the world to be there.
|
|
|
DocX
Hazard to Others
 
Posts: 179
Registered: 22-10-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Organikum  | | I asked a little bit around and this in the picture comes of course packed in another envelope or cardboard box, this is not in plain sight for
everybody handling the parcel, what would be not only unusual but most probably it would be against postal regulations about everywhere.
|
Funny. Because I asked around and got the exact opposite answer.
In fact, in the right part of the label the persons contact information (including telephone number) was printed. What would be against postal
regulations do you mean?
It's good if things are well packaged, declared and everything. But maybe not if it's a content that can be deemed suspicious. Those are the kind of
shipments you want packaged in an anonymous cardboard box labelled "Toys". Whatever your intent is.
[Edited on 20222222/10/4 by DocX]
|
|
|
Mateo_swe
National Hazard
  
Posts: 590
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
Long time ago i ordered a liter of nitroethane from a company in Italy, i think it was Eurochem or something very similar.
It was quite expensive, but its expensive everywhere.
I remembered i got mail from them a year later offering it at half price, but its also several years ago now.
If anyone need some it might be worth checking out if they still sell it in small volumes, they usually sell by the barrel.
|
|
|
DocX
Hazard to Others
 
Posts: 179
Registered: 22-10-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by SuperOxide  | Me too.. well, and the fact that
they won't ship to anyone outside the EU. That made it an even easier decision, lol.
Quote: Originally posted by DocX  | I have no interest in P2NP, I just wanted some nitromethane and nitroethane. But with labels like that ... I mean, it doesn't really matter if you're
Up To No Good or not, that kind of packaging warrants unwanted attention anyhow.
Luckily, there's solid alternatives. Not with the great prizes nitrochemis offers, but I'd rather pay a little more than have these things sent to me.
|
I'm in the same boat. What solid alternatives are you talking about for nitroEthane?
The only two routes I know of to synthesize nitroethane are pretty low in terms of atomic efficiency. But I don't really need that much of it anyways
(honestly, I don't even have a specific use planned for it). But I'm curious what alternatives you're referring to. |
Well, right here for example . Just a few posts above or below this one you’ll
find Chemship’s listing. He comes highly recommended, by me and any number of people.
|
|
|
SuperOxide
National Hazard
  
Posts: 542
Registered: 24-7-2019
Location: Devils Anus
Member Is Offline
|
|
Quote: Originally posted by DocX  | Well, right here for example . Just a few posts above or below this one you’ll
find Chemship’s listing. He comes highly recommended, by me and any number of people. |
Great! I just ordered some from him based off of your referral. Thanks
|
|
|
crow6283
Hazard to Self

Posts: 60
Registered: 14-1-2018
Member Is Offline
Mood: No Mood
|
|
Look a little closer at Acrifix’s products one of them is mostly nitroethane.
|
|
|
SuperOxide
National Hazard
  
Posts: 542
Registered: 24-7-2019
Location: Devils Anus
Member Is Offline
|
|
Quote: Originally posted by DocX  | Well, right here for example . Just a few posts above or below this one you’ll
find Chemship’s listing. He comes highly recommended, by me and any number of people. |
Thanks to your referral to chemship1978, I was able to add 500g of nitroethane to my inventory :-D

Will definitely do business with chemship again.
|
|
|
Fantasma4500
International Hazard
   
Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
ill let you guys in on a little sneaky trick- and in this context it seemed to pay off.
type this into google
acrylic glue "nitroethane" msds
lets see if "nitroethane" msds will do too? ok no that didnt go well, just popped a bunch of sales of pure stuff up
glue "nitroethane" msds gave me this
https://signgeer.com/media/productattach/e/x/extru-fix_msds.... - issued in 2019 so probably still a thing, based in UK
it says 5-20% by weight, 500mL, 25-100g? 20 pounds for one unit, rest is DCM.
bonus, 30-60%!!
https://www.theplasticshop.co.uk/plastic_safety_data_sheets/... says 2009 though
https://www.edplastics.co.uk/Tensol%20-%20bostik/Extrufix%20...
https://www.trentplastics.co.uk/adhesives-tapes-cleaners/ext... 25 pounds 500mL possibly 30-60%, further digging in MSDS's just makes it more
unclear- however impossible to order outside of the UK seemingly.
https://unionesadhesivas.com/es/index.php?controller=attachm...
cyanoacrylate remover, nitroethane blend, 2009- acetone wasnt good enough? HernonCyanoacrylate Remover 14 €542.50 for 10x55mL bottles, idk about
that.
ACRIFIX® 1S 0116 Pure-V contains ethyl formate and nitroethane- also pretty neat combo - on link they explain it has no DCM but doesnt mention
nitroethane any longer, safety datasheet doesnt reveal much, this might be decent concentration of NE, based on the secrecy. 1kg is 85 dollars
https://plastic-craft.com/acrifix-1s-0116-pure-v/
[Edited on 11-12-2022 by Antiswat]
|
|
|