Bugs Eat Plastic.....yeah
I found a short blurb in our local newspaper reporting on molecular biologist Federica Bertocchi who led a study reported in the journal Nature
Communications (no other reference). "Two substances in the saliva of wax worms - moth larvae that eat wax made by bees to build honeycombs - readily
break down a common type of plastic." The plastic was polyethylene.
I understand that these types of studies have been s topic of research for quite a while.
I'm sure waxworms will not starve even if all the bees disappear from earth!
|
|
|
mayko
International Hazard
   
Posts: 1230
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
I tried this with some meal worms... eventually they died but I think it was from too little water.
There's some background in these papers; it's basically a symbiosis between the bug (which physically shreds the plastic into manageable pieces) and a
gut microbe (which biochemically degrades it)
https://www.sciencemadness.org/whisper/viewthread.php?tid=10...
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
|
j_sum1
Administrator
      
Posts: 6488
Registered: 4-10-2014
Location: Limbo
Member Is Offline
Mood: Just got through yet another "take this job and shove it" moment.
|
|
This is a good start. But, as with anything in the biosphere, it opens up other critical questions:
How much plastic will be eaten?
At what rate?
What else is needed for the bugs to survive? What abiotic conditions do they need?
What are the other environmental impacts of a population increase in these bugs?
It is possible to begin with a promising concept and still create something non-sustainable, or worse, having a negative environmental impact.
When it comes to polymer waste, I personally am in favour of high-temperature incineration, gas scrubbing and energy harvesting as a disposal
mechanism. Preferably at a small scale so as to minimise total transportation of the waste material.
|
|
|
Bedlasky
International Hazard
   
Posts: 1253
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Few years ago I read about some bacteria eating PET. It decompose PET using some enzymes and ethylene glycol was actual food source for bacteria.
|
|
|
CharlieA
National Hazard
  
Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline
Mood: No Mood
|
|
@Mayko: thanks for the reference. I downloaded them and now I just have to read (and understand, hopefully) them.
@j_sum1: I imagine like most things, the ultimate(?) answer will be a bunch of things. Probably they will be the ones underwritten (supported) by
governments. Ideally there would be a solution that would be very highly efficient, very easy, and very cheap! ...I'm not asking for much, am I (well maybe some stock in such a wonderful enterprise. 
@Bedlasky: The bacteria that will eat PET will certainly never go hungry!
|
|
|
j_sum1
Administrator
      
Posts: 6488
Registered: 4-10-2014
Location: Limbo
Member Is Offline
Mood: Just got through yet another "take this job and shove it" moment.
|
|
I guess my point is that we tend to underestimate the interconnectedness in ecosystems and there is often a large uncalculated ripple effect when we
introduce changes. Introduction of plastic-eating bugs sounds great but it is not guaranteed to have an overall net benefit. And even if it is an
improvement, there is always the chance that other problems may be introduced.
|
|
|
CharlieA
National Hazard
  
Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by j_sum1  | I guess my point is that we tend to underestimate the interconnectedness in ecosystems and there is often a large uncalculated ripple effect when we
introduce changes. Introduction of plastic-eating bugs sounds great but it is not guaranteed to have an overall net benefit. And even if it is an
improvement, there is always the chance that other problems may be introduced.
|
j_sum1: I agree with you completely. When you choose any process to do something, I think you hope that, at best, you are choosing the lesser of two
evils. I guess the ideal process would be one that used abundant starting materials that were consumed 100% in making product...oh and also, no energy
would be required by the process, and no energy would be produced by the process!
|
|
|
Dr.Bob
International Hazard
   
Posts: 2922
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
There are also many bacteria that eat crude oil, as it has been seeping into the ocean and rivers for many years in places like Oil City, PA, Le Brea,
most of the Gulf Coast, and Jed Clampit's backyard. I think they have found a few more bacteria that eat other plastics, although most are too slow
to make a difference. If they made plastics out of biosave monomers, they would degrade faster, such as polyamides made from amino acids (like silk
and wool), and poly esters made from naturally occuring acids and alcohols. I would be happy with a plastic that degraded in 10 years even, as long
as it held together long enough to use.
I see biodegradable straws now, which are certainly better than the paper ones they keep trying here to save the ocean (which is funny in that we are
nowhere near the ocean). But I would hate for some germs to eat my shorts or T-shirt. I read that there is a growing shortage of cotton, so that
is one reason synthetics are becoming more popular, as apparel makers cannot get enough cotton now. Especially this year after Pakastan's crop was
mostly wiped out from flooding.
|
|
|
mayko
International Hazard
   
Posts: 1230
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
One cool thing I forgot to mention is that if you put your ear to the container you can hear the bugs as they wiggle and chew on the styrofoam ...
ASMR on demand!
I have a worm bucket in my kitchen ... long story short I had to downsize last year from a house with a compost pile to an apartment (kinda salty
about the situation still). I've tried experimenting with in-house composting, but I usually ran into problems with 1) waterlogging and putrefecation
at the bottom and 2) the sheer volume of kitchen waste produced relative to the decomposition rate.
I've been able to deal with 1 with two buckets, one with holes drilled in the bottom inside of a second to catch "compost tea" (I've had problems with
it being too salty to use on plants though).
2 was harder, until I got easy access to liquid nitrogen. Now about once a week I take the scraps out of the freezer and dunk them in the nitrogen
until they're brittle, then throw them in the blender. At the end I have a few cups of a multicolor powder. This helps to reduce bulk and to speed
decomposition... imagine you're a worm and you encounter a whole banana peel, where would you even start? Mix the powder with some sand, coffee
grounds, and paper shreds, and it's halfway to dirt before the worms get to it.
Anyway, you can hear the same sort of quiet seething in the worm bucket, squishier-sounding though 
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
|
pneumatician
Hazard to Others
 
Posts: 416
Registered: 27-5-2013
Location: Magonia
Member Is Offline
Mood: ■■■■■■■■■■ INRI ■■■■■■■■■■ ** Igne Natura Renovatur Integra **
|
|
https://www.plasticstoday.com/packaging/the-incredible-edibl...
|
|
|
EF2000
Hazard to Others
 
Posts: 155
Registered: 10-5-2023
Location: The Steppes
Member Is Offline
Mood: Taste testing the Tonka fuel
|
|
Pardon for resurrecting the thread, but:
Unfortunately, no. Waxworms just make holes in PE film. Paper by Faunhofer Institute says:
| Quote: |
No biodegradation of polyethylene
The results so far have surprised the project team: caterpillars eat holes in the polyethylene, absorb small amounts of it and at the same time lose a
significant amount of body mass. If holes are present, the caterpillars stop taking up further material. The analytical measurement data shows that
the caterpillars excrete the polyethylene unchanged. |