fuckin plastic piece of shit hoses


i almost lost my life right now. was working with a reactor with a heating jacket 210C, heated by mineral oil from the termostat, pumped by 0.5 -1m/s.
and the little fuckin retarded techincian idiot supplied me with a hose that can stand up to 75C.
i dont need to explain what happened next, the hose melted, the oil started bursting all over the lab, i got burns over my chest, the reactor cracked, the mixture caught fire, my lab coat started to burn, my gloves melted....FUUUUUCK.
im standing in the middle of some 5 m2 of oil around me..

luckily i was fast enough to put out the fire and strip. i hope the burns are not too dangerous, there are only a few blisters, and some part of the melted glove in my fuckin hand. and not to mention the embarresment when the firemen ran in and found me in my boxershorts and undershirt trying to put out the fire...

goddamnit, I HATE FUCKIN TECHINICIANS.

sorry for the bitching but i had to let off some steam, since officaly im responcible for this shit....im off to the doc

peace, oil, sand and soap.

[Edited on 13-6-2006 by daeron]




Humans with their brains are like a caveman with a supercomputer. Yes there is a chance that the caveman will use it to calculate the trajectories and the momentums of the celestial bodies, but the chances are that he will just crack open a coconut with it.
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 13-6-2006 at 03:44


Wow. That sucks. Glad you're ok.

Btw, fire the bastard.




"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to... satisfy any applicable law, regulation or legal process"
View user's profile View All Posts By User
chochu3
Hazard to Others
***




Posts: 185
Registered: 21-10-2003
Location: South Side Tejas [Cloverland]
Member Is Offline

Mood: Inside looking out

[*] posted on 13-6-2006 at 04:52


That's why an authority always over checks the work of a techinician.



\"Abiding in the midst of ignorance, thinking themselves wise and learned, fools go aimlessly hither and thither, like blind led by the blind.\" - Katha Upanishad
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1371
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 13-6-2006 at 10:16
Technician


Agreed. Fire the incompetent fuck. Also, with the next technician you get, carefully
review the setup. Glad your OK.




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 13-6-2006 at 12:43


Fire the guy who didn't train the tech.
View user's profile View All Posts By User
Nerro
National Hazard
****




Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline

Mood: Whatever...

[*] posted on 13-6-2006 at 13:38


If you do such work it can't hurt to check the items supplied to you, you may want to do that from now on.

Jope you'll be ok though, burns really suck. I once melted a bit of plastic into the skin of my hand, took ages to come off.




#261501 +(11351)- [X]

the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally

courtesy of bash
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2006 at 11:30


I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.

BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire.
View user's profile View All Posts By User
Nerro
National Hazard
****




Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline

Mood: Whatever...

[*] posted on 14-6-2006 at 13:12


Quote:
Originally posted by unionised
I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.


BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire.
LOL!



#261501 +(11351)- [X]

the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally

courtesy of bash
View user's profile View All Posts By User
daeron
Hazard to Self
**




Posts: 74
Registered: 26-3-2005
Member Is Offline

Mood: cancerogenic

[*] posted on 22-6-2006 at 03:39


thx to all who replied, the person altho she was HOT was fired, so no fucking of technicians there. got burns over my chest and some plastic in my right arm but otherwise im okay. this was a good lesson.



Humans with their brains are like a caveman with a supercomputer. Yes there is a chance that the caveman will use it to calculate the trajectories and the momentums of the celestial bodies, but the chances are that he will just crack open a coconut with it.
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1371
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 22-6-2006 at 08:01
Technician


Ashame she's real HOT ! I'd say she owes you a fuck for the misery she put you through
as a contrite apology to the agrieved. :D:D:D




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
DeAdFX
Hazard to Others
***




Posts: 339
Registered: 1-7-2005
Location: Brothel
Member Is Offline

Mood: @%&$ing hardcore baby

[*] posted on 22-6-2006 at 10:29


If your going to fuck people at your work place at least make sure that they can give you a promotion otherwise its not worth the time to take out the knee pads...;)

[Edited on 22-6-2006 by DeAdFX]
View user's profile View All Posts By User
andersderis
Harmless
*




Posts: 4
Registered: 24-6-2006
Member Is Offline

Mood: No Mood

[*] posted on 3-7-2006 at 13:00


fire tha bitch!!!
View user's profile View All Posts By User
Adar
Harmless
*




Posts: 7
Registered: 8-7-2006
Location: Sweden
Member Is Offline

Mood: Having fun with vaseline

[*] posted on 8-7-2006 at 05:50


Could you show a picture of the cracked reactor and point out the hose? It could be useful to avoid future mishaps for other people (and be quite intresting).
View user's profile View All Posts By User This user has MSN Messenger

  Go To Top