What is soldering iron tip refresher?


I bought a tin of 'tip refresher' for a cheap soldering iron,
It works very well so I'd like to know what it is.
As new it is a greyish crystaline powder,
Dipping a hot (>360oC according to instructions) soldering iron tip into it causes the powder to melt into a dark brown viscous liquid,
and the tip gets a plating of tin.
Some minutes after cooling most of the brown liquid returns to a greyish solid.
Any ideas what it is?

IMG_20230111_225944.jpg - 94kB




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
highpower48
Hazard to Self
**




Posts: 96
Registered: 30-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2023 at 10:07


Not sure since I've never used it. But it sounds like a mixture of tin and borax.
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 11-1-2023 at 11:27


It is mostly diammonium hydrogen phosphate, tin, a small amount of surfactant and a couple percent of secrete herbs and spices.

Edit - according to the MSDS

[Edited on 11-1-2023 by B(a)P]
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3920
Registered: 8-2-2015
Member Is Offline


[*] posted on 11-1-2023 at 16:28


My google skills failed me!
I did not find an msds :(
Thank you

Looks like it is not worth diy,
I'll just buy more of the commercial product when needed.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 11-1-2023 at 17:03


I only knew of it because I had seen it is a shop and was curious about it, so looked up the MSDS on the suppliers web site (it is a mandatory requirement to have online access to the MSDS in Australia).
Attached for your reference.


Attachment: TS1512-msdsMain.pdf (104kB)
This file has been downloaded 287 times

View user's profile View All Posts By User
Junk_Enginerd
Hazard to Others
***




Posts: 251
Registered: 26-5-2019
Location: Sweden
Member Is Offline


[*] posted on 15-1-2023 at 01:40


Quote: Originally posted by Sulaiman  
My google skills failed me!
I did not find an msds :(
Thank you

Looks like it is not worth diy,
I'll just buy more of the commercial product when needed.


I mean there are a lot of formulations that would give you the same results. Essentially, it's a strong fluxing agent and metal tin particles. Ammonium chloride and tin particles would be the most straightforward recipe I can think of. Then there are a zillion ways you could tweak it for optimal performance, like surfactants etc.
View user's profile View All Posts By User

  Go To Top