Gammatron
Hazard to Others
 
Posts: 125
Registered: 30-8-2022
Location:
Member Is Offline
|
|
Green iron cyanide complex
Hello everyone, haven't posted in a while but I got a weird one, or at least to me.
As usual I am working on another uranium extraction. The ore was leached with H2SO4 + H2O2. I neutralized the solution with NaOH to precipitate the
uranium and most other metals. Further increase of pH precipitates a thick blue/green sludge which I assume is Fe(OH)2 as it turns brown upon addition
of H2O2. I would've thought everything would be completely oxidized from the leach but maybe the U4+ reduced all the iron? Anyways, dissolving the
brown precipitate in HCl and addition of potassium ferricyanide (I don't have ferrocyanide) creates this intense green solution, I had to use a
flashlight for it to show up in the pic. Adding a reducer turns it blue which I assume is Prussian blue. H2O2 + KI will turn it green again but
neither one will do it on its own and reducing again returns the blue color. A quick google search didn't give any results for green iron cyanide
compounds so I wonder if anyone here might know??
Here is a pic of the green solution and the blue after reducing it.
https://imgur.com/a/0eqmCKZ
|
|
|
Stokes
Harmless
Posts: 7
Registered: 6-11-2023
Member Is Offline
|
|
It sounds like ferric ferricyanide, also known as Prussian green or Berlin green. Berlin green is insoluble in water, but forms dispersions easily, so
if it is Berlin green, it should eventually settle to the bottom of the container.
|
|
|
Gammatron
Hazard to Others
 
Posts: 125
Registered: 30-8-2022
Location:
Member Is Offline
|
|
I actually wondered if that was a real thing and if it's what I made. There doesn't seem to be much info on it other than paint pigments, It did
settle to the bottom.
|
|
|
Stokes
Harmless
Posts: 7
Registered: 6-11-2023
Member Is Offline
|
|
I just did a quick search for "Berlin green" on google scholar, and it looks like most of the information is about using it for battery materials and
electrochemical sensors. I've also encountered it myself when I was trying to make ferri/ferrocyanides by the old protein pyrolysis processes.
[Edited on 20-11-2023 by Stokes]
|
|
|
Gammatron
Hazard to Others
 
Posts: 125
Registered: 30-8-2022
Location:
Member Is Offline
|
|
Oh yeah I saw those studies too but I didn't look into any of them. Thanks for the info. This confirms that I was able to precipitate the uranium and
vanadium without getting much iron contamination which only complicates things
|
|
|