Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Preparation of biodiesel from waste cooking oil
palico
Hazard to Self
**




Posts: 70
Registered: 1-10-2013
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2024 at 01:00
Preparation of biodiesel from waste cooking oil


Hello people,

today we an experiment which I am very proud of, and it is also the best video on my YT channel at this moment: the preparation of biodiesel from waste cooking oil.

The reaction involved is the transesterification of oil with ethanol using sulfuric acid as catalyst.

reaction_cutted.jpg - 79kB

This experiment present different point of novelty compared to common biodiesel production method. First, it use waste cooking oil as substrate, and so has the advantage to convert a waste into a resource. Second, ethanol is used rather than methanol, which the purchase in some countries can be restricted for individual or hardly to find. Ethanol instead, is free to buy everywhere, readily available, cheap, and also can be renewable, because obtained from wine and spirit industry. Third, I am using an acid recipe, not basic, which is not sensitive to residual water, moisture, free fatty acids.

No complicated oil pre-titration is needed, the reaction is then more versatile and can accept various pil charge.

Procedure

The oil is pre-treated as follows: oil is collected, filtered roughly through a steel strainer, and the again through a tighter one. The oil is then heated to 100 Celsius on hotplate under stirring and kept for hours, until all water and volatiles are boiled off.

Once cool, 100 g of waste cooking oil is introduced in a 250 ml round bottomed flask, then 40 ml of 90 degree denaturated ethanol are added. The reaction mixture is biphasic. 1 ml of concentrated sulfuric acid is pipetted in, the reaction mixture brought to 90 Celsius in oil bath, and gently refluxed at this temperature for 8 hours. Initially, reaction mixture becomes soapy and single phase. Bubbles also decrease to disappears in few hours, evidence of ethanol getting consumed and transesterification going on. The reaction mixture becomes also more limpid.

Once finished the flask is removed from bath, let cool down to room temperature: two phase are seen, which the bottom is glycerol. Glycerol is removed in separatory funnel, the biodiesel washed with 3 x 50 ml water. A strong emulsion forms, indicating still presence of mono and di-glycerides.
A last washing with 5% bicarbonate solution is done.

The product is opalescent, is filtered through cotton plug, then heated under stirring at 80 Celsius to remove all volatiles: product become limpid and clear.

An yield 68 g, 76 ml of yellow oily liquid is obtained.

1684896504945_1.jpg - 775kB

Discussion

Product is characterized by density, refractometry, flame test and compared to initial waste oil. Results are the following.

table.jpg - 122kB

It is shown, product has lower density and refractive index, and this is as expected for a shorter chain molecule. The flame test is done as follow. A paper towel is impregnated with the sample, placed in a steel can and ignited. The oil is diffcult to catch on fire. Its combustion is awful. It generates acrid, toxic terribles fumes. The biodiesel instead, catch easily on fire, the combustion is smooth and stable and does not generates terrible fumes.

The behaviour of both on freezing is identical.

I am planning to repeat this reaction with more ethanol, and then with 96 degrees denaturated ethanol.

As usual I thank you for attention and link to YT video for a more detailed procedure.

See you,

palico




Transform waste into resources.
Animus tuus dominus.
YT Channel ZodaChem: https://www.youtube.com/@zodd0001/featured
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2920
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 2-3-2024 at 20:44


That is a great experimental. I have made methanol based biodiesel before, and know that ethanol is harder to make it with, so that is a good job. And not only is biodiesel less toxic, it is actually drinkable, used as a treatment for heart disease.

Good luck with work, I am happy that it is working. Even better if someone could find a biochemical method for producing ethyl biodiesel, or something as safe as that, and lower the energy needed to make it. That could make a safe fuel even more practical. It would also be great to bioengineer plants to make the oils better in the US climate, since we cannot get the high yields of palms in the tropics with soybeans or rapeseed crops. Thus people are clearing millions of acres in tropical rain forests.


View user's profile View All Posts By User
palico
Hazard to Self
**




Posts: 70
Registered: 1-10-2013
Member Is Offline

Mood: No Mood

[*] posted on 6-3-2024 at 02:42


Hello Dr. Bob. To know if that biodiesel is good for trasportation it requires more accurate analysis and fit law-based requirements as cetane number, metal impurities level, but I think instead it is good enough as heating fuel or for power generator, since waste cooking oil cannot be used directly for any combustion. In EU doing so it is envoironmental crime. The emulsion is evidence of mono and di-glycerides presence, but it can be mixed with fossil diesel in case.

Thanks for comment.




Transform waste into resources.
Animus tuus dominus.