Hello everyone. I was wondering how one could make a system that constantly inputs a powder into a reaction flask. Let's assume that one already has a
system (an auger/conveyor) that can move a powder at a defined rate. But, how can the powder be put inside the flask? Can something like this (https://www.directindustry.com/prod/lambda-laboratory-instru...) be improvised?
Because if there is just simply a funnel connected in one of the flask inputs, the fumes of whatever is being distilled will escape out that exit
instead of going in the condenser. The powder could also clump up and get stuck and just overflow out of the funnel.

The funnel could be put on tup of a separate condenser to remove the fumes that escape, but this would create a reflux (which can decompose some
compounds) and the condenser can still clog up and the powder would still overflow and spill.
Something like this would be perfect, IF it could be made automatic (electric) instead of having to be spun manually.

Any ideas?
|
|
|
Rainwater
National Hazard
  
Posts: 993
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
Short answer - A bigger hole, which the powder will not contact anything but the solution/solvent.
If vapor/gases are an issue, purging them before opening the reactor.
Usually an automated system will be on a much larger scale.
My perfered method is to create a solution of known concentration and deliver that. Its much easier to measure and transport.
If it must be a powder, the exact specifications need to be properly defined in order to design a low maintenance system. For example, baking bread.
We have to mix an explosive powder, with a corrosive powder, then into a parashable solvent.
It is undesirable to simply dump the correct amounts into a mixer and start stirring. The results will not be the well mixed recipe required.
But instead measure out and shift together, in roughly the correct proportions, then add to the solution.
"You can't do that" - challenge accepted
|
|
|
Sulaiman
International Hazard
   
Posts: 3942
Registered: 8-2-2015
Member Is Offline
|
|
There are a few threads here on SM with similar questions and some discussions,
at least one member made a working prototype,
but the consensus seems to be that it is not a trivial task.
Adding a liquid/solution is the preferred approach.
For most of us a batch method starting with solids in the rbf and adding liquid slowly is the norm.
What sort of scale / addition rate are you considering?
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
|
Lambda-Eyde
National Hazard
  
Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline
Mood: Cleaved
|
|
What's stopping you from getting one of these: https://us.vwr.com/store/product/11717091/24-40-powder-dispe...
...and slapping a motor with an axle and a suitable controller on it? Apart from these things being terribly expensive and rare to find used.
This just in: 95,5 % of the world population lives outside the USA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
|
|
|
BromicAcid
International Hazard
   
Posts: 3323
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Powder funnels can be useful. I hardly use them though in practice, so often the solids are somewhat soluble in the case of adding a reactant and
become dewy and clumpy - or just the refluxing solvent works its way up there and makes them clumpy even when they don't dissolve at all. They can be
pretty slick though when they do work.
|
|
|
4-Stroke
Hazard to Self

Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
Air isn't an issue, I meant the vapors that escape out the hole if a distillation is taking place simultaneously.
Quote: Originally posted by Rainwater  | Usually an automated system will be on a much larger scale.
My perfered method is to create a solution of known concentration and deliver that. Its much easier to measure and transport. |
Yes, but the problem is that some powders are insoluble (or very poorly soluble) in any solvents, or the solvents can react with whatever the powder
is being added to.
Quote: Originally posted by Sulaiman  | There are a few threads here on SM with similar questions and some discussions,
at least one member made a working prototype |
I searched for everything related I could find, but I didn't see anyone making a working prototype. Do you mind sharing it?
Yes, but that is not always possible.
Yeah, that's why I usually do as well. But I am just trying to make a fully automatic continuous reactor, so that's why this is the problem for me
now. Adding liquids is easy (e.g. pump), but solids are much harder.
No idea yet, but let's say approximately 10kg/h.
It's that they're terribly expensive and rare to find used 
And also, as Bromic Acid said, they don't actually always work like they are supposed to. Also I don't think that they can be used with granulated
powders.
Ukrainium
|
|
|
VincenzoTheGreat
Harmless
Posts: 6
Registered: 4-3-2019
Member Is Offline
|
|
did you try Alibaba?
https://www.alibaba.com/product-detail/Tiandi-Lab-250ml-Boro...
min. order of 5 @ $80USD a piece though
edit: I just bought a single unit (as a sample) for $110 USD. I'll let you know if they're any good or not.
As for handling the mass quantities you describe the unit has a ground glass inlet at the top which could accomodate a larger vessel containing the
bulk powder you wish to add. Maybe one of those column chromatography reservoirs would be ideal.
Regarding automation, I think the main challenge is fitting a DC motor to the PTFE auger and making sure it's flush. Controlling the motor is a
trivial exercise and documented ad nauseum elsewhere. I'm similarly motivated to you so the DC motor/automation angle is something I'd like to
investigate.
A much cheaper proof-of-concept could be rigged up with an overhead stirrer, 24/40 glass addition funnel, and a plastic screw that sits flush with the
walls of the funnel bottom. The design would mimic a regular industrial auger filler. I think that would be much more economical for us amateurs to
rig up something like that because all the parts are readily available.
And one more thing regarding addition. I saw wetting mentioned in a flow chemistry article about powder addition. The powder in question was wetted
10%, making a slurry, allowing for more even and controlled addition. Depending on the wetting solvent in question this might also act as a protective
barrier against solvent vapour which may react with the powder being added e.g. NaBH4 wetted by toluene entering a vigorously stirred solution of
MeOH.
[Edited on 13-11-2024 by VincenzoTheGreat]
|
|
|
4-Stroke
Hazard to Self

Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
Yeah, I saw that before. Sometimes you might even be able to get free samples (or even if not free, you at least don't have to order 5 pieces). The
shipping is expensive though. I am trying to order a 1kg sample of something, and the shipping for it is over $100! . And they apparently cannot ship it by sea because it is a "white powder"! Like is
it so hard to tell apart from cocaine? I think that they ship the bulk orders by sea, so why can't my sample also be shipped by sea?
Ukrainium
|
|
|
VincenzoTheGreat
Harmless
Posts: 6
Registered: 4-3-2019
Member Is Offline
|
|
without derailing the original topic, is it viable to make a slurry and continuously feed that into the system via a peristaltic pump?
|
|
|
4-Stroke
Hazard to Self

Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
Ah, that's nice. Yeah when it arrives, let me know how well it works. How much did the shipping cost?
Quote: Originally posted by VincenzoTheGreat  | | As for handling the mass quantities you describe the unit has a ground glass inlet at the top which could accomodate a larger vessel containing the
bulk powder you wish to add. Maybe one of those column chromatography reservoirs would be ideal. |
Yeah, most likely. If the powder is dry and granulated (not finely ground) make just a very big funnel could be used and filled with the powder which
would ensure that the addition funnel is constantly full. The funnel would probably have to be supported, however, as it's probably going to be very
heavy.
Quote: Originally posted by VincenzoTheGreat  | | Regarding automation, I think the main challenge is fitting a DC motor to the PTFE auger and making sure it's flush. Controlling the motor is a
trivial exercise and documented ad nauseum elsewhere. I'm similarly motivated to you so the DC motor/automation angle is something I'd like to
investigate. |
I've got a 3D printed, so maybe it could be somehow attached to a 3D printed bracket that would be glued or clamped (with screws) around the funnel.
But connecting it to the PTFE is probably going to be harder, as it's virtually impossible to glue anything to it. But that might not even be
necessary if the shape is correct so that it could just be "inserted" into another 3D printed part.
An ESP32 is ~$6 on AliExpress, and that's pretty much the only thing needed to automate the motor. It could probably all be done for under $10. But
automation might not even be necessary if the powder is just added at the correct predefined constant rate.
Quote: Originally posted by VincenzoTheGreat  | | A much cheaper proof-of-concept could be rigged up with an overhead stirrer, 24/40 glass addition funnel, and a plastic screw that sits flush with the
walls of the funnel bottom. The design would mimic a regular industrial auger filler. I think that would be much more economical for us amateurs to
rig up something like that because all the parts are readily available. |
That's a very good idea actually. But the screw would have to be pretty small (and also spin pretty slow but also have good torque). Usually overhead
stirrers are rated for higher speed, but here, I think ~100rmp is best. The overhead stirrers also cost a lot
Quote: Originally posted by VincenzoTheGreat  | | And one more thing regarding addition. I saw wetting mentioned in a flow chemistry article about powder addition. The powder in question was wetted
10%, making a slurry, allowing for more even and controlled addition. Depending on the wetting solvent in question this might also act as a protective
barrier against solvent vapour which may react with the powder being added e.g. NaBH4 wetted by toluene entering a vigorously stirred solution of
MeOH. |
Yes, for example sulfur could be wetted with some S2Cl2. But I don't think that a slurry would be easier to add than a
granulated powder. Maybe even the opposite. The powder could clump, stick, and now move properly to and with the PTFE screw.
Ukrainium
|
|
|
4-Stroke
Hazard to Self

Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
Wow that's a lot better then putting the slurry in a powder addition funnel. Those pumps don't cost that much, are unreactive (if PTFE tubing is
used), can move a relatively large volume, are easy to improvise, and are just overall perfect for this task. The slurry would have to be stirred
constantly to avoid the powder settling down to the bottom and clogging the pump, but that's nothing a 5 gallon bucket with a cement mixer cannot fix
Ukrainium
|
|
|
VincenzoTheGreat
Harmless
Posts: 6
Registered: 4-3-2019
Member Is Offline
|
|
check out these powder dosers from https://www.lambda-instruments.com/powder-doser/ for inspiration:

pretty neat idea! much more elegant design than the auger-style addition funnels.
|
|
|
4-Stroke
Hazard to Self

Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
It sure is a neat idea, but the price isn't 
But really, it seems very similar to the idea you suggested, just 100x more expensive. It's pretty much just a container (funnel) with a rotating
screw at the bottom.
[Edited on 13-11-2024 by 4-Stroke]
[Edited on 13-11-2024 by 4-Stroke]
Ukrainium
|
|
|
Dr.Bob
International Hazard
   
Posts: 2918
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
I still have a few 24/40 solid addition funnels that are decent quality for a good price. The VWR one shown above is one of the worst designs ever,
so don't ever get that one, I have one and won't sell it, as it sucks. But most others are good. You could likely hook one of them into motor if
geared low enough. I have never used a doser like shown just above.
|
|
|
MrDoctor
Hazard to Others
 
Posts: 249
Registered: 5-7-2022
Member Is Offline
|
|
Look up teardowns of CD/DVD polishers, i cracked one open once, they use peri pumps to move a slurry of cutting compound (common alumina grit), it
would clog up or kind of "set" if not for one simple trick, which is this great big solenoid squishing a section of tubing between a pair of check
valves, forcing water to get injected in one direction, but i forget exactly where that water went, with quite a bit of pressure, this kept everything
moving, i had to fix that mechanism to get the polisher to stop clogging constantly, as well as undo the repair done by the previous person that
connected everything wrong.
A slurry will work especially well if the particle size is consistent, things settle much quicker when everything has somewhere other than forwards,
that it can go.
if feasible consider adding a detergent or gelling agent to suspend the solid, provided it wont interfere with the reaction. if i was pumping
something like cinnamon powder into some sort of spirit distillation as part of a recipe that demands the solid be continuously added, i would use
gelatin to thicken it so it wont settle, as i know gelatin wont screw anything up.
Sometimes neutral oils like high viscosity silicone oil are used in situations like this, i know i read it a couple times be added purely for
mechanical benefits.
|
|
|
Mister Double U
Hazard to Self

Posts: 66
Registered: 21-2-2025
Member Is Offline
|
|
Vacuum
Hello 4-Stroke,
Have you thought about using a vacuum pump at the end of your condenser.
That way you can feed your powder into the flask without the need of a seal.
Best Greets!
|
|
|