Author: Subject: Making Magnesium Turnings
Lancer85
Harmless
*




Posts: 13
Registered: 13-6-2024
Member Is Offline


[*] posted on 14-11-2024 at 06:19
Making Magnesium Turnings


I need some magnesium turnings of Grignard quality but have no way of buying them. What are some possible ways I could make them? Drilling holes through a magnesium ingot is the last resort as that would be tedious and would probably produce magnesium pieces too large.

Another idea was maybe putting through magnesium ribbon through a micro-cut paper shredder. I'm not sure if that will work or if the paper shredder blades would be strong enough.

Let's hear your ideas!
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 590
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 14-11-2024 at 07:06



Isnt magnesium soft enough so you could shave of thin flakes with a woodworking tool?
Something like in the picture?
Or use a dremel type rotary tool.

[Edited on 2024-11-14 by Mateo_swe]
View user's profile View All Posts By User
Sir_Gawain
National Hazard
****




Posts: 525
Registered: 12-10-2022
Location: southeast
Member Is Offline


[*] posted on 14-11-2024 at 09:21


A lathe is probably your best option. Magnesium should be soft enough to cut without using oil.



View user's profile Visit user's homepage View All Posts By User
Fulmen
International Hazard
*****




Posts: 1794
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 14-11-2024 at 11:35


Nah, Mg is too hard for woodworking tools. It's comparable to pure aluminum. You could hand file it if you only need a small amount.
Drilling, milling or turning would be more efficient.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 14-11-2024 at 15:56


You can work aluminium and magnesium with woodworking tools.
3:05
https://www.youtube.com/watch?v=4-3l1yau5aU

If you want magnesium turnings the way to do it is to turn it on a lathe. There's a hint in the name.
Be careful not to set it on fire.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3322
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 14-11-2024 at 16:02


The scrap yard by my old house had some magnesium scrap in the form of sheets. I took a drill to it going it a it sequentially with 1/4 - 1/2" bits and made a ton of shavings, goes quick because the MW of Mg is so low, it does make nice turnings.



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 14-11-2024 at 16:31


I used a stepper drill bit and got some great turnings.
View user's profile View All Posts By User
Lancer85
Harmless
*




Posts: 13
Registered: 13-6-2024
Member Is Offline


[*] posted on 15-11-2024 at 00:00


Quote: Originally posted by j_sum1  
I used a stepper drill bit and got some great turnings.


A stepper seems like a smart idea. Would you say it would be enough to get 50-100g worth without having to spend all day?

[Edited on 15-11-2024 by Lancer85]
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1794
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 15-11-2024 at 00:35


Quote: Originally posted by unionised  
You can work aluminium and magnesium with woodworking tools

True enough. I would say pure Mg is comparable to pure Al, so fairly soft. But I responded to a picture of a planer, and that's probably not going to work.
At least I cannot imagine it's possible to make any significant amount of turnings that way, and I have machined magnesium in the past.

The step drill sounds like a better choice. The fire hazard should be minimal as long as you keep the speeds down and don't allow chips to accumulate.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 15-11-2024 at 02:24


Since the stepper has gained some interest, let me provide some details - from memory.

I have some half inch Mg plate. Hitting it with the drill bit and a battery drill caused filings to spin off really quickly. It took only a couple of minutes to fill a jam jar.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2024 at 03:16


Quote: Originally posted by Fulmen  
Quote: Originally posted by unionised  
You can work aluminium and magnesium with woodworking tools

...But I responded to a picture of a planer, and that's probably not going to work.
...
The step drill sounds like a better choice....


I assure you that it's possible and practical to plane aluminium.
The step drill does seem like a step forward (sorry, couldn't resist a pun)
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2918
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 15-11-2024 at 07:45


If you are in the US, I could likely get you some Mg turnings. I can ship small amounts of those I believe.
View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 15-11-2024 at 08:14


Try ebay. I bought 2,5kg magnesium turnings from there.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2315
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 16-11-2024 at 17:11


On the other hand, as I recall, older air-cooled VW engine blocks were made of Magnesium. Throw a rod, and the whole block is shot. If you can salvage such an item; it might fulfill your Magnesium needs for a good long while.

https://www.thesamba.com/vw/forum/viewtopic.php?t=598238

[Edited on 17-11-2024 by zed]
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 590
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 18-11-2024 at 05:09


Well many high preformance car and bike wheel rims are made out of magnesium but they cost a fortune.
A damaged one on the other hand is probably just the magnesium per kilo price if you can find one.
Or maybe just buy some of those fire making rods in the outdoors sport shops.
Its magnesium and they are meant to be flaked off with a knife and used as a firestarter.
Probably not that expensive if you want a smaller amount.
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 993
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 18-11-2024 at 05:40


There is a woodworking too called a rasp. Magnesium should be soft enough to use it. What size of turnings are you interested in?



Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Myc
Harmless
*




Posts: 8
Registered: 30-5-2022
Member Is Offline


[*] posted on 21-11-2024 at 03:11


I made my own turnings by drilling some magnesium rod using a drill press. It's pretty simple and fast. Initially I drilled using a ~10 mm drill bit or larger and actually ended up with turnings that were too thin - and I guess had too much surface area or oxide or similar. I reduced the bit size to ~5 mm and had much better results for what I needed it for.
View user's profile View All Posts By User