I am going to leave my input. You could use sodium chloride, manganese dioxide and add concentrated sulfuric acid(drain cleaner kind) with a little heat. You could try a higher temperature method replacing sulfuric acid with anhydrous sodium bisulfate. Another method I read about which may or may not work is heating sodium chloride with sand and anhydrous magnesium sulfate to red heat. The later starts with dirt cheap reactants but requires considerable heat input. I may try it on a 5 gram scale just for the science aspect.



Fellow molecular manipulator
View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 22-11-2024 at 05:39


clearly_not_atara They pressed it because they used samothing like an very big Kip Gas generator and the powder could get into the bellow tank and releases to much chlorine. oh they soaked the MnO2 briks with little bit MnCl2 bevore the baking because they where more stable. Better procedur is Weldon mud.

The MnO2 NaCl sulfruic acid need heating and you need lots of sulfuric acid
MnO2 +2NaCl + 3H2SO4 = MnSO4 + 2NaHSO4 +2 H2O+2Cl

[Edited on 22-11-2024 by Alkoholvergiftung]
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3938
Registered: 8-2-2015
Member Is Offline


[*] posted on 23-11-2024 at 04:37


Quote: Originally posted by bnull  
... Where would you store all that?...
this is a factor that I did not realise the significance of for many years,
Scale matters!
When I first wanted jointed glassware I checked the options and costs of different glassware based on joint size.
At that time, and even now I think, neck size 24 (24/29 or 24/40) was the best buy.
Now most of my glassware is NS24.
So I typically use 100ml to 1000ml RBFs,
which means that I use 50ml to 500ml quantities per batch,
which means that I buy in 500ml or 500g quantities or more
(usually more to benefit from lower cost per ml/g and postage)
So I need a LOT of storage space for equipment, supplies and products,
and all hazardous chemical storage problems scale up as well.
So
I'm giving the same advice that I ignored when I started.....
work at small scale, unless it's for something spectacular.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 23-11-2024 at 04:54


I have the same problem. Same too with joints of glassware 29/32 arent cheap where i live .but chinese from vevor 24/40 you can buy 130 parts destilling setup with 3 colums for 130 Euro.Bevor i could only by an bridge and 2 roundflasks for that money.
For chemicals sometimes you make big batches or precursors because every time to synthesis this to make that is an hasle.

[Edited on 23-11-2024 by Alkoholvergiftung]

[Edited on 23-11-2024 by Alkoholvergiftung]
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1240
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 7-12-2024 at 08:31


Quote: Originally posted by Alkoholvergiftung  
I have the same problem. Same too with joints of glassware 29/32 arent cheap where i live .but chinese from vevor 24/40 you can buy 130 parts destilling setup with 3 colums for 130 Euro.Bevor i could only by an bridge and 2 roundflasks for that money.
For chemicals sometimes you make big batches or precursors because every time to synthesis this to make that is an hasle.

[Edited on 23-11-2024 by Alkoholvergiftung]

[Edited on 23-11-2024 by Alkoholvergiftung]
Some things are worth buying in multiple pound quantities. Sodium hydroxide, copper sulfate, sodium metabisulfite, sodium bisulfate, nitrate salts to name a few. For instance copper sulfate is my gateway to copper chemistry. That reminds me I need to brew up some calcium acetate so I can make copper calcium acetate crystals.



Fellow molecular manipulator
View user's profile View All Posts By User
 Pages:  1  2

  Go To Top