How hot does charcoal actually burn ?


When burning wood in my woodstove I did some tests with an infrared pyrometer. When all wood was decomposed and there was a layer of hot embers in the well ventilated stove, I measure 800-900 C. But when I blow air on it via a makeshift tuyere (a metal pipe connected to my mouth which blows), temperatures reach 1100 C.
The largest online chemistry textbook also mentions such values.

But how did ancient users make steel using charcoal without electric fans and tuyeres ?
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 23-11-2024 at 11:45


Who needs electric fans when you have water and animals and slaves (yep) to power the bellows?

From somewhere in the same textbook:
Quote:
In the Old World, humans learned to smelt metals in prehistoric times, more than 8000 years ago.

and
Quote:
Most early processes in Europe and Africa involved smelting iron ore in a bloomery, where the temperature is kept low enough so that the iron does not melt. This produces a spongy mass of iron called a bloom, which then must be consolidated with a hammer to produce wrought iron. Some of the earliest evidence to date for the bloomery smelting of iron is found at Tell Hammeh, Jordan, radiocarbon-dated to c. 930 BC.


Here is an article: E. A. Ginzel, Steel in Ancient Greece and Rome.

Conversion of wrought iron to steel was manageable.

Edit: I forgot this one:
Quote:
Archeologists have discovered tuyeres dating from the Iron Age; one example dates from between 770 BCE and 515 BCE.


[Edited on 23-11-2024 by bnull]




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 23-11-2024 at 11:47


the ren stove where somtimes over 3meter high it was the chimney effect that sucks air in.

[Edited on 23-11-2024 by Alkoholvergiftung]
View user's profile View All Posts By User
4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 23-11-2024 at 13:33


Although steel was possible to make in small quantities, it wasn't really mass produced up until about the start of the Industrial Revolution. As bnull said, at first, iron wasn't even molten, it was just a red hot bloom that was forged to turn it into something useful, but the bloom was made out of wrought iron, so it was (relatively) soft. Then, they started making cats iron. It has a low melting point (~1200°C), so it was possible to make out of charcoal. Steel is technically possible to make using charcoal, but very hard, so mostly coke was used for making steel (although charcoal still has used, especially at the beginning). The maximum temperature achievable with charcoal is a little over ~1500°C.