[*] posted on 9-11-2015 at 04:51
Barium chloride or nitrate more usefull ?


To test for sulfates I can buy barium chloride or barium nitrate,
Which has the more general use as an indictator and as a general reagent ?
View user's profile View All Posts By User
Detonationology
Hazard to Others
***




Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline

Mood: Electrophillic

[*] posted on 9-11-2015 at 05:20


Barium nitrate can be used to make some really beautiful green compositions in pyrotechnics.



“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6462
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 9-11-2015 at 05:28


Why not get barium hydroxide and make the chloride or nitrate as needed?


Calcium chloride is an acceptable substitute for testing sulfates.

[Edited on 9-11-2015 by j_sum1]
View user's profile View All Posts By User
Upsilon
Hazard to Others
***




Posts: 392
Registered: 6-10-2013
Member Is Offline

Mood: No Mood

[*] posted on 9-11-2015 at 06:06


Quote: Originally posted by j_sum1  
Why not get barium hydroxide


Barium carbonate is cheaper, just as an FYI.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 9-11-2015 at 06:50


The commercially available barium carbonate (from potteries) is very impure. It contains a lot of BaSO4 and BaS as well. Making pure and clear solutions from this is hard. I once used this to make clean and pure BaCl2.2H2O, but this was not really easy. It was much more involved than simply dissolving some of the material in dilute HCl.

I would go for the Ba(NO3)2. It is sufficiently soluble for aqueous chemistry tests and experiments, and it also is quite interesting for colorful pyrotechnics experiments.

[Edited on 9-11-15 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Upsilon
Hazard to Others
***




Posts: 392
Registered: 6-10-2013
Member Is Offline

Mood: No Mood

[*] posted on 9-11-2015 at 08:51


What makes it hard to deal with those impurities? In theory, on addition of HCl the BaSO4 would not be attacked and the BaS would form H2S and BaCl2. Then you would just have to filter off the BaSO4.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 9-11-2015 at 09:44


Theory and practice differ a lot in many cases. The sulfide is partially oxidized by oxygen from the air, leading to formation of colloidal sulphur, which remains suspended in the liquid and which is VERY hard to filter. Evaporating the liquid to dryness hence yields a very impure product, which is yellow and has a dirty smell of sulphurous compounds.

http://woelen.homescience.net/science/chem/exps/BaCl2_2H2O/i...

The procedure is not really difficult, but it also is not as easy as dissolving some BaCO3 in dilute HCl. It is a long and tedious process.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
MolecularWorld
Hazard to Others
***




Posts: 110
Registered: 30-10-2015
Member Is Offline

Mood: No Mood

[*] posted on 9-11-2015 at 09:48


Quote: Originally posted by Upsilon  
What makes it hard to deal with those impurities? In theory, on addition of HCl the BaSO4 would not be attacked and the BaS would form H2S and BaCl2. Then you would just have to filter off the BaSO4.


Suppose you wanted to react 100g of barium carbonate with an 8% barium sulfide impurity (not atypical for pottery grade), you would generate 1.6g, or 1.05 liters, of hydrogen sulfide. That is enough to stink up about two million cubic meters of air (@0.47ppb), and enough to render 105 cubic meters of air (a 7x5x3 meter room) unsafe (@10ppm).

Edit: Slight correction to calculations (probably still wrong). The point is, even a little hydrogen sulfide can be a big problem if you're not expecting it or don't know how to deal with it.

[Edited on 9-11-2015 by MolecularWorld]




View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 9-11-2015 at 10:39


Quote: Originally posted by MolecularWorld  
Quote: Originally posted by Upsilon  
What makes it hard to deal with those impurities? In theory, on addition of HCl the BaSO4 would not be attacked and the BaS would form H2S and BaCl2. Then you would just have to filter off the BaSO4.


Suppose you wanted to react 100g of barium carbonate with an 8% barium sulfide impurity (not atypical for pottery grade), you would generate 1.6g, or 1.05 liters, of hydrogen sulfide. That is enough to stink up about two million cubic meters of air (@0.47ppb), and enough to render 105 cubic meters of air (a 7x5x3 meter room) unsafe (@10ppm).

Edit: Slight correction to calculations (probably still wrong). The point is, even a little hydrogen sulfide can be a big problem if your not expecting it or don't know how to deal with it.

[Edited on 9-11-2015 by MolecularWorld]


<p>On the strength of this argument, I can say that the barium carbonate currently being sold by Seattle Pottery is pretty pure.</p>

<p>Treating 1000 grams of it with pool grade HCl (patio) produced a distinct hydrogen sulfide smell but hardly anything I would describe as a "stench" and not noticeable beyond several feet away. I would not want to do that indoors, the smell would linger, but I was expecting (from reports) a far greater H2S release.
View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 9-11-2015 at 10:45


Quote: Originally posted by Upsilon  
Quote: Originally posted by j_sum1  
Why not get barium hydroxide


Barium carbonate is cheaper, just as an FYI.


Indeed, it is much, much cheaper. The cheapest barium hydroxide I can find is more than 100 times more expensive that the cheapest barium carbonate.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3920
Registered: 8-2-2015
Member Is Offline


[*] posted on 9-11-2015 at 13:57


I am as far as possible trying to not generate toxic waste
so I like j_sum1's suggestion of calcium chloride substitution (thanks)
but
I just ordered 100g of BaCl2.2H2O claimed >99.8% purity
as solubility of earth alkaline sulphates decreases with increasing atomic number,
so more sensitive than Calcium salts,
and barium chloride is relatively cheap.

I almost bought barium and strontium nitrates as they would be nice for pyrotechnics, maybe another time.

[Edited on 10-11-2015 by Sulaiman]
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 9-11-2015 at 14:49


Be aware that calcium salts are not as sensitive as barium salts. ~2g CaSO<sub>4</sub> will dissolve in one liter of water as compared with ~2mg for BaSO<sub>4</sub>. Strontium salts may be a good compromise, as they are non toxic and the solubility of SrSO<sub>4</sub> is ~100mg per liter.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6462
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 9-11-2015 at 15:26


Quote: Originally posted by gdflp  
Be aware that calcium salts are not as sensitive as barium salts. ~2g CaSO<sub>4</sub> will dissolve in one liter of water as compared with ~2mg for BaSO<sub>4</sub>. Strontium salts may be a good compromise, as they are non toxic and the solubility of SrSO<sub>4</sub> is ~100mg per liter.

Agreed. It really depends on how sensitive a test you need for your application.
If you test with CaCl2 first, you might have a need for only a very small amount of Ba(NO3)2. That answers some of your toxicity concerns as well as some of your acquisition concerns. Synthesising barium nitrate from pottery grade carbonate might be a PITA but if all you need is a few grams, it should be reasonably do-able.
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 9-11-2015 at 18:10


Synthesizing barium nitrate from pottery grade barium carbonate is actually much easier than synthesizing barium chloride because nitric acid is an oxidizing acid. The nitric acid oxidizes barium sulfide either to barium sulfate or sulfur dioxide which removes the issue of colloidal sulfur contamination. I have found that it is necessary to boil the solution for a few minutes with a decent excess of nitric acid to fully oxidize the sulfur in some instances.
View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 9-11-2015 at 19:02


Hot toluene dissolves sulfur, according to this:
http://media.rsc.org/Classic%20Chem%20Demos/CCD-73.pdf
it is about 10 g per 100 mL at 50 C.
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1238
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 31-12-2024 at 19:02


Quote: Originally posted by Sulaiman  
I am as far as possible trying to not generate toxic waste
so I like j_sum1's suggestion of calcium chloride substitution (thanks)
but
I just ordered 100g of BaCl2.2H2O claimed >99.8% purity
as solubility of earth alkaline sulphates decreases with increasing atomic number,
so more sensitive than Calcium salts,
and barium chloride is relatively cheap.

I almost bought barium and strontium nitrates as they would be nice for pyrotechnics, maybe another time.

[Edited on 10-11-2015 by Sulaiman]


Barium is not as tedious to handle like lead. I’m working with barium now and I have a beaker full of concentrated magnesium sulfate ready to decontaminate. My insoluble residues are a mix of excess barium carbonate, unreacted barium sulfate and I suspect barium thiosulfate from oxidation of sulfides with 2 ml of 35% hydrogen peroxide. Once my barium bromide solution is fully filtered and ready for crystallization, I’ll take insoluble residues and filter paper and put them in one beaker, add dilute HCl until just acid to pH paper and add magnesium sulfate to everything and let it all digest overnight. Liquid can be neutralized with baking soda and decanted off and the solid residues safely disposed of in the trash. Or I could attempt to save crude barium’s sulfate to reduce it later for reuse





Fellow molecular manipulator