Author: Subject: Best way to get green nickel oxide into solution ?
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 29-1-2025 at 04:36
Best way to get green nickel oxide into solution ?


Hi!
I got some very cheap green nickel oxide (fine powder, like dust, great surface) and want to prepare different nickel salts.

Unfortunately, this batch of nickel oxide refuses to go into solution. According to different web sources, the solubility of nickel oxide can differ greatly between easy soluble and almost insoluble. Generally, light green nickel oxide should be better soluble as dark brown or even black nickel oxide.

I´ve refluxed a sample with an excess 80% acetic acid overnight and the acid is still almost colorless. Same happens even with perchloric acid (about 40-50%, I do not dare to reflux azeotropic 70 % for a prolonged time).

Ideas/suggestions?

View user's profile View All Posts By User
Precipitates
Hazard to Others
***




Posts: 186
Registered: 4-12-2023
Location: SE Asia
Member Is Offline

Mood: Acid hungry

[*] posted on 29-1-2025 at 05:43


Can you try a stronger acid e.g., sulphuric, nitric or hydrochloric, and then perform a double displacement to get the desired salt?

Probably what I'd try if the nickel oxide is just refusing to dissolve in weak acids.
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 29-1-2025 at 05:49


I thought perchloric is one of the strongest acids and nickel perchlorate is also very well soluble? I also found a statement that nickel oxide is soluble im ammonia water, maybe i should try this even if i´m not convinced.
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 29-1-2025 at 06:17


This is the source of information about nickel oxide green and black:

https://www.todini.com/chemicals/nickel/nickel-oxide-green

https://www.todini.com/chemicals/nickel/nickel-oxide-black

The German Wikipedia states that nickel oxide is soluble in ammonia water and refers to "Georg Bauer, handbook of preparative inorganic chemistry" whereas the English Wikipedia states that it is soluble in KCN (what I really don´t want to try).

https://de.wikipedia.org/wiki/Nickel(II)-oxid

https://en.wikipedia.org/wiki/Nickel(II)_oxide
View user's profile View All Posts By User
Precipitates
Hazard to Others
***




Posts: 186
Registered: 4-12-2023
Location: SE Asia
Member Is Offline

Mood: Acid hungry

[*] posted on 29-1-2025 at 06:25


Quote: Originally posted by Nemo_Tenetur  
I thought perchloric is one of the strongest acids and nickel perchlorate is also very well soluble? I also found a statement that nickel oxide is soluble im ammonia water, maybe i should try this even if i´m not convinced.


It is*, but it appears nickel oxide doesn't dissolve in perchloric acid as well as other strong acids such as sulphuric (1).

I believe senior forum members have previously produced nickel perchlorate from nickel oxide (2), so they may chip in on how they did this/how this went etc.,

1. Effect of Solid State Impurities on the Dissolution of Nickel Oxide
2. Uses for nickel (II) perchlorate hexahydrate

*Sorry previous post was misleading, perchloric acid is a very strong acid, stronger than those I mentioned.

View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 29-1-2025 at 06:38


Thank you for this information. The first link doesn´t work, but the second work well. Maybe @woelen can give more details about the preparation from nickel oxide and perchloric acid.
View user's profile View All Posts By User
Precipitates
Hazard to Others
***




Posts: 186
Registered: 4-12-2023
Location: SE Asia
Member Is Offline

Mood: Acid hungry

[*] posted on 29-1-2025 at 06:42


Quote: Originally posted by Nemo_Tenetur  
Thank you for this information. The first link doesn´t work


Attachment: Effect of Solid State Impurities on the Dissolution of Nickel Oxide.pdf (625kB)
This file has been downloaded 171 times
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2926
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 29-1-2025 at 07:08


I would definitely prefer hydrochloric acid, since chloride is a weak ligand for nickel. Perchlorate on the other hand is a highly non-coordinating anion.



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 29-1-2025 at 07:10


Quote: Originally posted by Nemo_Tenetur  
The German Wikipedia states that nickel oxide is soluble in ammonia water and refers to "Georg Bauer, handbook of preparative inorganic chemistry"

We have an old English edition of Brauer's in the Library. Nickel (ii) oxide is in page 1548.

[Edited on 29-1-2025 by bnull]




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1927
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2025 at 08:44


Have you tried adding a little hydrogen peroxide? This certainly assists in the dissolution of Co and Mn oxides though it doesn't seem to make much difference to Fe3+ oxides.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4505
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 29-1-2025 at 10:05


Quote: Originally posted by clearly_not_atara  
I would definitely prefer hydrochloric acid, since chloride is a weak ligand for nickel. Perchlorate on the other hand is a highly non-coordinating anion.


Agreed. You probably need a ligand to help get the nickel into solution- hydrochloric acid, or concentrated ammonia/ammonium chloride.




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 29-1-2025 at 10:46


You don't need the nickel salts right away, do you? Put a little oxide into a vial, add some acid and leave the vial alone for a couple of days or a week. Do that with the acids you have (and ammonia too) and see later what dissolved the oxide the most. Give them time and go do something else.

I remember some iron oxide sold as pigment that refused to dissolve in cold, hot, and boiling hydrochloric acid. I gave up and forgot the matter. Some time later, while digging through my stuff, I saw that a good part of the oxide had dissolved.




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 29-1-2025 at 11:04


Quote: Originally posted by bnull  
You don't need the nickel salts right away, do you? Put a little oxide into a vial, add some acid and leave the vial alone for a couple of days or a week. Do that with the acids you have (and ammonia too) and see later what dissolved the oxide the most. Give them time and go do something else.

I remember some iron oxide sold as pigment that refused to dissolve in cold, hot, and boiling hydrochloric acid. I gave up and forgot the matter. Some time later, while digging through my stuff, I saw that a good part of the oxide had dissolved.


That´s a good idea! I´ll give the ammonia solution a try, put it in a closed bottle and make a review in a month or two. In contrast to acetic and perchloric acid, I can´t reflux it as I have no pressure-resistant equipment (otherwise most of the ammonia goes off).
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 30-1-2025 at 02:14


I have different excperiences with different oxides, even of the same metal.

I have black nickel oxide (I think it is a higher oxidation state or mixed oxidation state oxide), and it dissolves with great difficulty in acids. I also have NiO, and my oxide dissolves easily in strong acids (I made solutions of nickel perchlorate from this, used for doing experiments with nickel complexes of amines).

The solubility of a metal oxide strongly depends on how it is prepared. If it is strongly heated during preparation, then it becomes very very inert. I have two samples of Nd2O3, both looking very similarly (grey powder with a purplish hue). One of these samples dissolves in a strong acid quickly, and even hisses a little bit on addition to the acid, and leads to noticeable heating up of the liquid. The other sample does not dissolve at all. Not even an hour of refluxing with any of the common strong acids gives more than trace amounts of Nd in solution. I have a similar experience with my dark red Fe2O3, green Cr2O3, and white SnO2.

You indeed could put the nickel oxide aside in concentrated HCl (30% by weight) and leave it that way for days or weeks. I think that HCl is the best option, because it forms complexes, which may help dissolving the oxide. In my experience, HNO3, H2SO4 and HClO4 all are less suitable for dissolving hard to dissolve oxides, because their anions are not coordinating to the metal ions.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3943
Registered: 8-2-2015
Member Is Offline


[*] posted on 30-1-2025 at 03:01


as aqua regia dissolves both nickel and nickel oxide, I'd give it a go.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 30-1-2025 at 03:07


Thank you very much for this detailed writeup. The oxide preparation temperature is critical, without question, but impurities are also important if I understand the pdf-document from the user "Precipitates" correct.

The source of my cheap nickel oxide is pottery, therefore contaminants are very likely.

Chromium impurities act as inhibitor, whereas lithium promotes dissolution. Maybe I should add a trace amount lithium salt?
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 30-1-2025 at 06:54


If you hadn't seen my post from before.

"1.5g (0.02mol) nickel oxide and 11.5g (0.08mol) 70% perchloric acid in 20ml water.

Heat with stirring on 150 degree hotplate (solution temp 75 rising to 90) until a slurry with no black oxide left. Dilute and redissolve with 50ml water for a clear emerald green."

Unfortunately you do need to heat it but there's no problems with aqueous perchloric acid at these temperatures. I used "pottery" black NiO. I had to use the 2x excess HClO4 otherwise it just wouldn't fully react. I've used 32% HCl and 68% HNO3 too and let it heat to dry without issue.
View user's profile Visit user's homepage View All Posts By User
RU_KLO
Hazard to Others
***




Posts: 319
Registered: 12-10-2022
Location: Argentina
Member Is Offline


[*] posted on 31-1-2025 at 04:49


maybe if you want to try another route (not tried by myself) but why not...:

use oxalic acid, at 70-90°C for at least 5 hs. (refluxing)
Read somewhere that "complexation power" of oxalic acid helps with the solution of some difficult metal oxides.

"Dissolution of Nickel Oxide in Oxalic Acid Aqueous Solutions"
https://www.sciencedirect.com/science/article/abs/pii/S00219...

Then you will have insoluble nickel oxalate (or maybe some "Oxalatonickelate" https://en.wikipedia.org/wiki/Oxalatonickelate).

Treat this with a calcium chloride strong solution to get insoluble calcium oxalate + soluble nickel chloride




Go SAFE, because stupidity and bad Luck exist.
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 4-3-2025 at 15:46
Update


Just for your information, a prolonged refluxing with about 35 % perchloric acid for 48 - 72 hours dissolved most of the nickel oxide.

After cooling to room temperature, a vacuum filtration with a buchner funnel yielded a heavy somewhat viscous clear dark green solution.

I´ve done two batches. First batch with about 48 hours refluxing yielded a dark green solution with a measured density of 1.49 gram per milliliter at seven degree centigrade. It didnt´t crystallize after three days at 7 degree centigrade. So the whole batch was evaporated to dryness at about 40 - 50 degree centigrade in a very large open pan. Yield about 60% of the weight from the heavy solution.

The second batch was refluxed for about 72 hours, the nickel oxide went almost completely into solution, only a few percent residue. I´ve used an almost stoichometric quantity of perchloric acid (no excess, it´s much more expensive and valuable than nickel oxide) and I guess it was almost completely used.

The measured density of the dark green solution of this batch was 1.53 gram per milliliter. It´s still evaporating and I expect a slightly better yield, maybe somewhat above 60% (calculated by the weight of the solution by evaporation to dryness). The total conversion rate (nickel oxide to nickel perchlorate) is probably about 95% .

Thank you @Axt for the perchloric acid refluxing suggestion!

@woelen I think there´re some typos in the corresponding sciencemadness wiki article, see attached screenshot.

"Nickel(II) nitrate is the chemical compound with the formula Ni(ClO4)2."

I doubt that the solubility data is correct. From my experience, a nickel perchlorate solution with a concentration of more than 60% by weight is possible even at 7 degree centigrade. So even if the solubility is calculated as the anhydrous salt , it´s too low.






Wiki entry.jpg - 201kB
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 5-3-2025 at 04:45


Nickel perchlorate is extremely soluble in water. I have a wet slurry of nickel perchlorate 6-hydrate. It is a wet mass of green crystals under a layer of dark green solution. Never tried to dry it further, I only use this stuff in aqueous solution, so no need to first dry it.

It is good that you used excess nickel oxide. You don't want excess acid in the solution. But even with the excess nickel oxide, I can imagine that the solution still is quite acidic. You could try testing it with pH-paper, or with a little solid NaHCO3.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 5-3-2025 at 13:55


Yes, I don´t want acid residue. I´ve dried it in a large open pan and finally (required almost two days) got, after grinding with a stainless steel spon, apple-green crystals, free flowing. Therefore I think the acid residue is negligible, but I should confirm this with pH-paper.

Does perchloric acid have a detectable smell at moderate elevated temperatures (about 50 degree centigrade)? I´ve always avoided to test it because it´s said to be very corrosive to organic tissue.

Anhydrous perchloric acid is said to be a volatile fuming liquid, very dangerous, whereas somewhat diluted solutions (the commercial 60 % and azeotropic 70 %) aren´t fuming and more viscous.

View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 5-3-2025 at 23:44


Perchloric acid at 70% or less is completely odorless, even if somewhat heated. It does not give off any fumes (other than water vapor) at all, not even at somewhat elevated temperatures. The hydrated acid has a high boiling point (well over 200 C), that's why it is not fuming at all.

I aslso noticed that perchloric acid is not extremely corrosive to skin, not more so than e.g. HCl. of course, you should not allow it to remain on your skin for minutes, but if you spill something on you, it has no immediate effect like sulfuric acid. It is more like getting some HCl on your skin. Just rinse it off with some water and no further effect is noticed.

Anhydrous acid is another thing. It is very dangerous and fumes a lot in contact with air.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 6-3-2025 at 04:39


Thank you for explanation. That means, even a considerable residue of perchloric acid is not detectable by smell.

By the way, do you know if the hexammine complex of nickel perchlorate is labile? I´ve dissolved the residue of my nickel perchlorate in the bowl and glassware with several milliliter distilled water and added excess 25 % ammonia water. Immediately a deep blue complex precipitated out and was filtered yesterday in the evening, followed by washing with distilled water (no more ammonia smell was detectable) and I let it stand outside in the cold.

Today the precipitate wasn´t dry (that´s no surprise as the temperature outside was somewhat below zero degree centigrade), but it was partially discolored back to greenish.

See attached jpeg.



I also noticed some weak ammonia smell.

Is it possible that it loses some ammonia? I have no other explanation for this oberservation. I guess (pure speculation!) that the ammonia loss was only partially, not completely, because otherwise the extremely soluble nickel perchlorate probably wouldn´t precipitate in such a wet environment.




P1140571.JPG - 2.6MB

P1140569.JPG - 2.6MB
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1240
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 12-4-2025 at 13:53


A lot of discussion of difficult to dissolve metal oxides here. I am tempted to try molten potassium and sodium bisulfates since they are my chemical waste products



Fellow molecular manipulator
View user's profile View All Posts By User
teodor
International Hazard
*****




Posts: 1169
Registered: 28-6-2019
Location: Netherlands
Member Is Offline


[*] posted on 14-4-2025 at 23:49


You can try any salts with melting point below 450C. This is the average top limit of an average "tinbad" which (as I can imagine) is very convenient to use for working with molten salts.
The main purpose of the molten salt is to give mobility to oxide ions. Then you can add a compound to react with. In some cases the solvent (the molten salt) can perform the role of the reactant also.
Bisulfate will be converted to pirosulfate. You can try to add persulfate as an oxidiser to get a higher valency.
I have very succesfull experiment in dissolving "ijzerchromat" (Fe2Cr2O3) in Graham's salt ( Na(PO3)n ) which converts it to green Cr compound (phosphate?).
Other examples of salts with m.p. below 450C are nitrates, acetates, obviously - alkali hydroxides. Fluorides (of course) but some of them can react with water vapours to release HF, you have to check information about a particular compound.
High melting point solvents are not studied (or popularised) as good as water so many discoveries/rediscoveries are still possible.



[Edited on 15-4-2025 by teodor]