RLyon
Harmless
Posts: 9
Registered: 7-5-2025
Member Is Offline
Mood: No Mood
|
|
Silicone masking material- with alkaline lift?
Here's a hard one. Looking for a resist liquid that I can use on *cured* two part platinum silicone three dimensional shape (Think skull, not circuit
board) that will flow (like an ink)- and presumably dry with some decent adhesion.
AND that can also resist a highly acidic underwater environment as this is essentially for masking out areas in an electroplating bath.
Id like to be able to also easily remove the resist as needed with a minimum of volatile chemicals.
Right now my only working option is more two part silicone, which needs to be peeled off- but id like some thing that can be removed with a solvent-
or ideally Im guessing an alkaline wash...
any ideas?
|
|
|
Cathoderay
Hazard to Self

Posts: 97
Registered: 29-1-2023
Location: US-Texas
Member Is Offline
|
|
Have you considered a type of wax?
|
|
|
RLyon
Harmless
Posts: 9
Registered: 7-5-2025
Member Is Offline
Mood: No Mood
|
|
getting anything to stick to the silicone other than silicone has been hard. The wax would need to be sort of sticky- maybe like a museum wax? And it
would be hard to draw with unless it was hot...
|
|
|
bariumbromate
Hazard to Others
 
Posts: 105
Registered: 4-2-2025
Location: australia
Member Is Offline
Mood: nitrating
|
|
nurdrage has a video on making silver ink https://www.youtube.com/watch?v=EBlqPS8boLI
paint on and heat to 100 degrees in a oven once electroplating is done use ammonia to wash silver off if your electroplating metal does not interact
with ammonia
|
|
|
bnull
National Hazard
  
Posts: 995
Registered: 15-1-2024
Location: East Woods
Member Is Offline
Mood: Fecking annoyed
|
|
| Quote: | | (...) silver ink (...) |
Won't work. Silver ink is conductive and what @RLyon needs is an insulating substance. If they are using an electroless deposition followed by
electroplating, it will mess things up. They could use it to draw the patterns on the surface, of course, but it may be much more work than needed.
@RLyon: Have you tried nail polish? Soluble in acetone, easy to peel off. I considered that for my PCB etching but bought cheap CD markers instead.
|
|
|
Twospoons
International Hazard
   
Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Would a grease like lanolin work for you? Its very water repellant, and sticky. Whether it would survive an acid bath is something you would have to
try.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
|
RLyon
Harmless
Posts: 9
Registered: 7-5-2025
Member Is Offline
Mood: No Mood
|
|
I think nail polish is probably going to be the best bet. If it falls off the silicone it will at least stay together and not fall apart into tiny
bits in the bath which can cause its own problems. Ill give it a try!
Thanks
|
|
|
RLyon
Harmless
Posts: 9
Registered: 7-5-2025
Member Is Offline
Mood: No Mood
|
|
@Twospoons how would one remove the lanolin after the fact?
|
|
|
Twospoons
International Hazard
   
Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Probably any organic solvent would remove the lanolin. You'd have to test, of course. I'd try isopropanol first.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
|