ETN-erythirthol tetranitrate good and bag yields


Just got a 91% yield of ETN after recrystallisation with 99% isoproypl alochol and I ve used 20g of erythrithol and dissolved it in 60ml of 98% conc sulfuric, while keeping everything cool in an normal water bath, than when everything was dissolved I put the etn-sulfuric acid soulution in a dropping funnel and dripped everything dropwise without cooling to the red fuming nitric acid, the temperture rised up to I guess close 40 after everything was added, than everything was heated to 45C with a hot water bath (it was the same cooling water from the beginning) and was stirred for 30 min. No runaway happend and it was stirred the whole time. Than after the time was over I just cooled everything down with and salt-ice bath to 10C and during this time ETN crystals started to percipitate. And at 10C I started to crash everything in an ice bath and filter it. I didnt meassure the crude yield but after recrystallisation in 55C hot Isopropyl alcohol I let the solution cool down to 10C and crashed everything again in a 10% urea solution and filter the recrystallised ETN. In the end I got 45,65g of ETN. Is this yield good? I am a beginner in engergetics I just synthesize the ETN by a literature I found online here:
https://yadda.icm.edu.pl/baztech/element/bwmeta1.element.baz...
So I was just wondering if this what I got was a average yield or not
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 993
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2025 at 12:59


91% is a decent yield for nitric esters. However, be aware that ETN is a very sensitive energetic, and 45 grams will easily kill you if it goes off at the wrong time.
View user's profile View All Posts By User
Sir_Gawain
National Hazard
****




Posts: 528
Registered: 12-10-2022
Location: southeast
Member Is Offline


[*] posted on 26-5-2025 at 14:01


That’s interesting, I tried the dissolve-in-sulfuric-acid-first method and got an abysmal yield. Perhaps because I used 68% nitric acid and kept it around 10°C. How much RFNA did you use?



View user's profile Visit user's homepage View All Posts By User
dettoo456
Hazard to Others
***




Posts: 291
Registered: 12-9-2021
Member Is Offline


[*] posted on 26-5-2025 at 16:39


@Sir_Gawain If he followed the prep method he linked, the molar ratio of HNO3 to Erythritol was very large; 3.4 moles HNO3 per OH-. That volume was probably what kept the exotherm in check. Even then though, it is odd that such high yields were achieved at 40C instead of the normal chilled temps. The excess of water in your synth is probably just what killed the yields.

Maybe if a molar excess of 2 or less HNO3:OH dissolved in DCM was used, the reverse addition scheme (H2SO4 & Erythritol to HNO3) could work. Or simpler, as ETN isnt soluble in DCM afaik, DCM could be added to the mixture after nitration, and the excess HNO3 could be extracted and recycled, granting enough H2SO4 was present to sequester water generated in the nitration.
View user's profile View All Posts By User
Sir_Gawain
National Hazard
****




Posts: 528
Registered: 12-10-2022
Location: southeast
Member Is Offline


[*] posted on 26-5-2025 at 21:00


Since nitric acid is nearly always the most expensive and difficult to obtain, shouldn’t the yield be based on it instead of erythritol?



View user's profile Visit user's homepage View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 27-5-2025 at 11:26


The article that started this thread looks like it was created using artificial intelligence. The error in the title and the other information looks like it was put together from several sources. Including an unrealistically high yield. Especially for a beginner.....:cool:



Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
nitropyrotech
Harmless
*




Posts: 33
Registered: 6-5-2025
Member Is Offline


[*] posted on 27-5-2025 at 11:44


@Laboratory of Liptakov Hmm idk I just searched for some random ETN synthesis in the internet and found this article at my first attempt I got pretty low yield I dont really remember it but it was like in the 70% range or so but that was because I didnt kept the temp, soon I ll just improved my yield quickly by just letting everything stir at constantly at 45C, but I really got this big 91% yield, Idk how but it wasnt the weight of the remain water I checked the weight after drying for a week or so flat on paper, I also tested it in some of my blasting caps and the ETN works just fine
View user's profile View All Posts By User
nitropyrotech
Harmless
*




Posts: 33
Registered: 6-5-2025
Member Is Offline


[*] posted on 27-5-2025 at 11:48


Quote: Originally posted by Sir_Gawain  
That’s interesting, I tried the dissolve-in-sulfuric-acid-first method and got an abysmal yield. Perhaps because I used 68% nitric acid and kept it around 10°C. How much RFNA did you use?

I used regular RFNA I distilled my own from cheap Ammonium nitrate and melt sufluric acid drain cleaner, for my batch I used 96ml of RFNA
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 27-5-2025 at 12:31


nitropyrotech...Thanks for explain. Interesting.....:cool:

[Edited on 27-5-2025 by Laboratory of Liptakov]