Author: Subject: Silicone masking material- with alkaline lift?
RLyon
Harmless
*




Posts: 9
Registered: 7-5-2025
Member Is Offline

Mood: No Mood

[*] posted on 22-5-2025 at 06:20
Silicone masking material- with alkaline lift?


Here's a hard one. Looking for a resist liquid that I can use on *cured* two part platinum silicone three dimensional shape (Think skull, not circuit board) that will flow (like an ink)- and presumably dry with some decent adhesion.

AND that can also resist a highly acidic underwater environment as this is essentially for masking out areas in an electroplating bath.

Id like to be able to also easily remove the resist as needed with a minimum of volatile chemicals.

Right now my only working option is more two part silicone, which needs to be peeled off- but id like some thing that can be removed with a solvent- or ideally Im guessing an alkaline wash...

any ideas?
View user's profile Visit user's homepage View All Posts By User
Cathoderay
Hazard to Self
**




Posts: 97
Registered: 29-1-2023
Location: US-Texas
Member Is Offline


[*] posted on 22-5-2025 at 09:13


Have you considered a type of wax?
View user's profile View All Posts By User
RLyon
Harmless
*




Posts: 9
Registered: 7-5-2025
Member Is Offline

Mood: No Mood

[*] posted on 23-5-2025 at 23:29


getting anything to stick to the silicone other than silicone has been hard. The wax would need to be sort of sticky- maybe like a museum wax? And it would be hard to draw with unless it was hot...
View user's profile Visit user's homepage View All Posts By User
bariumbromate
Hazard to Others
***




Posts: 105
Registered: 4-2-2025
Location: australia
Member Is Offline

Mood: nitrating

[*] posted on 24-5-2025 at 23:17




nurdrage has a video on making silver ink https://www.youtube.com/watch?v=EBlqPS8boLI

paint on and heat to 100 degrees in a oven once electroplating is done use ammonia to wash silver off if your electroplating metal does not interact with ammonia





View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 995
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 26-5-2025 at 09:35


Quote:
(...) silver ink (...)

Won't work. Silver ink is conductive and what @RLyon needs is an insulating substance. If they are using an electroless deposition followed by electroplating, it will mess things up. They could use it to draw the patterns on the surface, of course, but it may be much more work than needed.

@RLyon: Have you tried nail polish? Soluble in acetone, easy to peel off. I considered that for my PCB etching but bought cheap CD markers instead.




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 26-5-2025 at 15:40


Would a grease like lanolin work for you? Its very water repellant, and sticky. Whether it would survive an acid bath is something you would have to try.



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
RLyon
Harmless
*




Posts: 9
Registered: 7-5-2025
Member Is Offline

Mood: No Mood

[*] posted on 31-5-2025 at 02:03


I think nail polish is probably going to be the best bet. If it falls off the silicone it will at least stay together and not fall apart into tiny bits in the bath which can cause its own problems. Ill give it a try!
Thanks
View user's profile Visit user's homepage View All Posts By User
RLyon
Harmless
*




Posts: 9
Registered: 7-5-2025
Member Is Offline

Mood: No Mood

[*] posted on 31-5-2025 at 02:04


@Twospoons how would one remove the lanolin after the fact?
View user's profile Visit user's homepage View All Posts By User
Twospoons
International Hazard
*****




Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 31-5-2025 at 14:44


Probably any organic solvent would remove the lanolin. You'd have to test, of course. I'd try isopropanol first.



Helicopter: "helico" -> spiral, "pter" -> with wings