ZRFARMS
Harmless
Posts: 5
Registered: 5-6-2025
Member Is Offline
Mood: No Mood
|
|
Turning DCM ---> Paint Stripper
I'll preface this quickly,
I'm a farmer in the USA, not a chemist lol. I have some new(to me) equipment that I purchased. Previous owners lathered everything in paint every
year. No matter what...
Needless to say, all this paint has to come off, and I'd prefer not to spend long doing it.
Commercially available strippers are garbage. Found out DCM is the active ingredient in older paint strippers. Bought DCM... Dries too fast. Not
penetrating and lifting.
I have approximately 2 liters of 99.99% DCM to play around with to prove its efficacy before I buy more.
I have tried mixing with approx
30:70 Methanol CM
50:50 Methanol CM
10:30:60 Laquer Thinner:Methanol: DCM
I found a paper detailing DCM and its use as a paint stripper.
Journal
I am a little bit out of my depth here and am looking for the easiest way to make this stuff work. I don't mind investing in different chemicals if I
can continue to make and use this stuff on demand.
**As for safety, I have the correct gloves, filters in my masks and a wind tunnel to handle DCM and other solvents. I just need some direction and am
open to ideas. Thanks.
|
|
|
bnull
National Hazard
  
Posts: 993
Registered: 15-1-2024
Location: East Woods
Member Is Offline
Mood: Fecking annoyed
|
|
I'd try first to remove the most part with one of those wire brushes that go in a power tool and then remove the rest with the stripper. The first
part is as boring as boredom goes but saves a lot of patience for the second part.
What size is the equipment? Tractor and above?
|
|
|
CouchHatter
Hazard to Others
 
Posts: 154
Registered: 28-10-2017
Location: Oklahoma
Member Is Offline
Mood: 76 elements taken!
|
|
Yeah, other "commercial strippers" are a joke, comparatively. Pure DCM is hard to beat. You could soak rags and temporarily fasten them in place, if
vertical, to decrease evaporation rate. This might be easier than messing with solvent ratios.
Alternatively, xylene is a slow-dry solvent that is easy to find. A 1:10 xylene-to-DCM combo ought to substantially slow the evaporation rate enough
to work with the stuff.
|
|
|
ZRFARMS
Harmless
Posts: 5
Registered: 5-6-2025
Member Is Offline
Mood: No Mood
|
|
3x 36' Disc Harrows.
The hydraulics and steel are fine. It's been in regular use for years.
Wire wheel is a great option for the loose and peeling but unfortunately, some of the paint layers are just stuck on too hard for it to be a
cost-effective option. I'd much prefer to slop on some stripper in the fall and give it a fresh epoxy coat after prep.
The nooks and crannies also make a wire wheel a much less attractive option.
|
|
|
MrDoctor
Hazard to Others
 
Posts: 249
Registered: 5-7-2022
Member Is Offline
|
|
DCM paint thinner here has some ammonia in it, im told the DCM lets the ammonia migrate through the paint causing it to unstick from the surface since
a strong base will impact the charge on a given surface (apparently thats part of why bases are slippery on your skin), combined with the DCM also
soaking the paint causing it to bow or wrinkle, making it flake off. DCM alone will do the trick but ammonia should cause a little to go a long way,
and probably blister up a bit as well, especially with an additional solvent like methanol, ethylene glycol, or perhaps xylene as was mentioned
before, to stop the DCM being able to evaporate away quite so fast.
|
|
|
yobbo II
National Hazard
  
Posts: 820
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
Great read on paint strippers.
Quoting from the journal
Thickeners allow the paint stripper to remain in place on vertical surfaces. Thickeners also increase contact time by reducing the rate of
evaporation, thus holding the solvent on the substrate's surface for a longer period.
Many companies offer products in a range of viscosities, from liquid to dense pastes. Paintbusters' Brand Architectural Paint Stripper, distributed by
On-Site Wood Restoration, claims to be the thickest. Its product literature states, “We start with Methanol-softened Parafin [sic] and a finned
blender; we stir in Methylene Chloride, until we reach a saturated solution. We add wetting agents. That is all. No thinners, no buffers, no stringy
thickeners, no volatile solvents.”
It is recommended that paint strippers thickened with wax be applied in a heavy .........
You need to add a thickening or gelling agentnto the DCM.
Try looking for 'professional' stripper.
The DCM stripper is available in UK as 'professional' stripper.
https://www.stripperspaintremovers.com/dcm-in-paint-removal/
Yob
|
|
|
Twospoons
International Hazard
   
Posts: 1392
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Have you considered sand blasting? That would also yield a good clean paintable surface.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
|
MrDoctor
Hazard to Others
 
Posts: 249
Registered: 5-7-2022
Member Is Offline
|
|
you can get home sandblasting kits rather cheap too, i saw consumables for it at the auto shop, until a few months ago i always assumed you had to
take it to a professional with dedicated hardware, but nope, i guess all you need is a compressor and some small scale feeder to dispense the sand
(and either a chamber or respirator)
|
|
|
BromicAcid
International Hazard
   
Posts: 3322
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
You need more contact time, you could try to wrap or cover in cotton rags and soak in DCM. Not as efficient as the gelling agents but should help.
|
|
|
ZRFARMS
Harmless
Posts: 5
Registered: 5-6-2025
Member Is Offline
Mood: No Mood
|
|
I agree. I thought about calling the author who wrote it, but he died in 2010 or so. I understood the words in the paper, but I don't know all the
specifics of the processes or steps. My girlfriend at the time did all of my chemistry in high school and college. I may need to get in touch with her
lol.
My attempt at this project has been on the side and not exactly at the forefront of my attention.
In my prior research, I found lots of posts about distilling DCM from paint stripper, but nothing at all about reverse engineering paint stripper. I
think it's kinda interesting.
I assume that paraffin wax is the correct form of paraffin to use. I will play around with that and update the thread accordingly.
|
|
|
ZRFARMS
Harmless
Posts: 5
Registered: 5-6-2025
Member Is Offline
Mood: No Mood
|
|
I have considered it, and it would be ideal. This may end up being cheaper, though, so we'll see. If it's more trouble than it's worth, I'll bite the
bullet and call a dustless blaster.
During the winter(30-60f), we have a lot of downtime once equipment is repaired/winterized.
|
|
|
ZRFARMS
Harmless
Posts: 5
Registered: 5-6-2025
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by MrDoctor  | | DCM paint thinner here has some ammonia in it, im told the DCM lets the ammonia migrate through the paint causing it to unstick from the surface since
a strong base will impact the charge on a given surface (apparently thats part of why bases are slippery on your skin), combined with the DCM also
soaking the paint causing it to bow or wrinkle, making it flake off. DCM alone will do the trick but ammonia should cause a little to go a long way,
and probably blister up a bit as well, especially with an additional solvent like methanol, ethylene glycol, or perhaps xylene as was mentioned
before, to stop the DCM being able to evaporate away quite so fast. |
Would an aqueous ammonia solution that is available off the shelf work?
Quick search showed that most of the stuff is around 29.5%.
|
|
|
yobbo II
National Hazard
  
Posts: 820
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
There is a device for a power washer called a wet sandblaster.
You need dry free flowing sand which is protected from the water that will be flying around. I have seen an upturned road cone as a sand reservior
into a container used.
It is a messy business as all sand blasting is, unlass you have a chamber or dedicated area and protective gear.
https://www.amazon.co.uk/Sandblasting-Sandblaster-Attachment...
Yob
|
|
|
AdamAlden
Dismissed
 
Posts: 113
Registered: 18-3-2016
Location: California
Member Is Offline
Mood: stressed
|
|
ur better off sand blasting
do ur self a favor and skip the head ache... get a sand blaster and a heck good dust mask
do not take notes
|
|
|
AdamAlden
Dismissed
 
Posts: 113
Registered: 18-3-2016
Location: California
Member Is Offline
Mood: stressed
|
|
i speak from an insanity freakazoid experiment where i striped all the paint on my entire car... i regret this after only having money to liquor it up
when i needed that good shit the car manufacturer has tubs of
do not take notes
|
|
|
jackchem2001
Hazard to Others
 
Posts: 110
Registered: 2-6-2024
Member Is Offline
|
|
When you are stripping paint, remember that DCM's odor threshold is quite high. If you are smelling it then you definitely need to step back, improve
ventilation, etc. It's not like other solvents like turpentine or toluene/gasoline where you will smell it even if you have very good ventilation.
DCM is not dangerous but it's still unhealthy. Also DCM and alcohol will make each other's toxicity stronger
|
|
|
zed
International Hazard
   
Posts: 2316
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Umm. Paint stripper used to be available as a DCM "Paste"; a thick molasses-like product that clings to vertical surfaces nicely, and evaporates
slowly, which gives the DCM an opportunity to penetrate through paint.
With enough personal protective gear, it is possible to spray this product via an airless sprayer, thereby making it possible to strip the paint
quickly from a whole house (or barn).
Just spray the goo on, let it sit for a while, and then pressure wash the peeling paint right off.
In simpler times, Sodium or Potassium Hydroxide solutions were used to strip off old paint.
Do not get these products on your penis! Likewise, don't let this corrosive crap get into your eyes.
If'n you do, you will become a modern day Virgil Moats, and such blindness interferes greatly with your dating
possibilities.
Don't know who Virgil Moats is? Virgil is the protagonist of the great John Huston Film, "Wise Blood".
Great stuff!
|
|
|
zed
International Hazard
   
Posts: 2316
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Whoops! I was wrong! Hazel Moats, not Virgil.
|
|
|
AdamAlden
Dismissed
 
Posts: 113
Registered: 18-3-2016
Location: California
Member Is Offline
Mood: stressed
|
|
Quote: Originally posted by ZRFARMS  | I'll preface this quickly,
I'm a farmer in the USA, not a chemist lol. I have some new(to me) equipment that I purchased. Previous owners lathered everything in paint every
year. No matter what...
Needless to say, all this paint has to come off, and I'd prefer not to spend long doing it.
Commercially available strippers are garbage. Found out DCM is the active ingredient in older paint strippers. Bought DCM... Dries too fast. Not
penetrating and lifting.
I have approximately 2 liters of 99.99% DCM to play around with to prove its efficacy before I buy more.
I have tried mixing with approx
30:70 Methanol CM
50:50 Methanol CM
10:30:60 Laquer Thinner:Methanol: DCM
I found a paper detailing DCM and its use as a paint stripper.
Journal
I am a little bit out of my depth here and am looking for the easiest way to make this stuff work. I don't mind investing in different chemicals if I
can continue to make and use this stuff on demand.
**As for safety, I have the correct gloves, filters in my masks and a wind tunnel to handle DCM and other solvents. I just need some direction and am
open to ideas. Thanks.
|
<3 you a god man get that paint bro hit it with that cancerous shiznitz.. bro u need to use a sand blaster and a shop vac and a bunch 3m dust masks
change often. Seel off the area so u can reduce contamination of your areas around the equipment my friend. cheapest way
you could even run boxfans with air filters attached twith tape the whole time to keep dust down bro if u want more ideas just let me know
do not take notes
|
|
|
AdamAlden
Dismissed
 
Posts: 113
Registered: 18-3-2016
Location: California
Member Is Offline
Mood: stressed
|
|
save the dcm for when u wanna paint the shiz u sand blast. at that point u need a activated carbon 3m mask i think its the purplish pinkish filter
[Edited on 29-6-2025 by AdamAlden]
do not take notes
|
|
|