Firebrick and Inert Gas
I'm planning to make an electrical resistance furnace using firebrick and resistance wire hooked up to a Variac, and I was wondering; do firebricks
provide enough resistance to leaks to make it viable to install an inert gas port so I could pump argon or nitrogen in, and maintain a reasonable
positive pressure without wasting a ton of gas?
|
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Not at all, no. Gas-tight chambers are generally not constructed with loosely-placed components. Now, if you had an inner chamber that was made of
welded steel, that would be a lot better.
Alternatively, you can use steel plumbing pipes and nickel-graphite anti-seize compound to get a vacuum seal at very high temperatures.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
|
yobbo II
National Hazard
  
Posts: 820
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
You could put the welded steel box on the outside either.
|
|
|
Texium
|
Thread Moved 27-11-2023 at 11:08 |
Sulaiman
International Hazard
   
Posts: 3947
Registered: 8-2-2015
Member Is Offline
|
|
I GUESS that making a gas-tight oven is expensive
but if there are only small leaks then accepting a little gas loss
may be significantly cheaper,
unless you plan to go into significant repeated production.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
|