When verifying one-gram samples against 2 mm steel sheet, the Liptex plastic explosive was verified at density of 1.75g/cc.
The Liptex plastic explosive is based on TACP and its exact composition is not public. The detonation velocity is variable and ranges from 5000 to
6800 m/s depending on the density, diameter of the charge, etc. The floating detonation velocity and therefore the fragmentation effect is variable
for all plastic explosives. The charge had a diameter of 8 mm. Hole has diameter cca 10,5 mm. The cuted steel plate off corresponds to a VoD of around
6500 m/s. The support lines from the steel support are visible on the underside.

Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper
60 (2025)
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
During the research of friction and impact sensitive mixtures, a reliable mixture was developed, which has high sensitivity like EPH 20,
but low energy like H48. And his toxicity is reduced to a minimum.
Was examinated:
Mixture EPH 20 is too power. Poisonity od EPH 20 is high. Plus can can cause hole in cup on side of firing pin. Nitrocellulose decrease brisantion
of EPH 20, same as bigger ammount of glass. But poisonity of entire mixture is main problem further.
Was examinated:
Mixture H48 is corrosive, his oxicity is low but his sensitivity is also low and unreliable in some applications.
Therefore was developed and examinated in long time of weeks a new mixture, which takes the best from both substances.
In Laboratory of Liptakov was developed mixture H48 + 5% LH. Called as work name Hypo 48.
Ratios in part by weight: Sb2S3 30 + S 11 + KClO3 59 + Pb(H2PO2)2 5 . Compounds mix under water + IPA 1:1. Create wet grain 1x1 mm. Final drying on
surface 40C. On bottom cup pour carborundum black grain from abrasive paper, which is harder than glass. 0.5 - 1 mm. Second layer is 2 - 3 mm of Hyppo
48, press 1 Kg, and 1 drop nitrocellulose 5%. Cup dry at 40 C by 30 minute. Only my reccomend for reliable cup filling. Sure exist some better
mixtures and procedures.
  
Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper
60 (2025)
|
|
|
EF2000
Hazard to Others
 
Posts: 155
Registered: 10-5-2023
Location: The Steppes
Member Is Offline
Mood: Taste testing the Tonka fuel
|
|
Are you sure it's not public? You posted it yourself: https://www.sciencemadness.org/whisper/viewthread.php?tid=26...
Wroom wroom
"The practice of pouring yourself alcohol from a rocket fuel tank is to be strongly condemned encouraged"
-R-1 User's Guide
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
I know it of course. On picture is simple 9 years old mixture. A new composition is different and more powerful.....
Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper
60 (2025)
|
|
|
ExcerptSix
Harmless
Posts: 10
Registered: 13-4-2025
Member Is Offline
|
|
Wouldn't Hypo 48 be still poisonous because of the lead hypophosphite?
Wouldn't the KClO3 make it corrosive as well?
The big pro in my eyes of EPH formulas is that they are not corrosive.
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
The only advantage is high sensitivity with low explosion energy. The disadvantage remains partial toxicity and corrosiveness. Therefore, the article
ended with the sentence:
Sure exist some better mixtures and procedures.....
Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper
60 (2025)
|
|
|