Phosphor the easy way


I ve found this patent from 1892 about the easy way to manufacture Phosphor. The patent says that Metaphosphoric acid or its sodium salt can simply at low red glowing heat be readuced with aluminium in every form or zinc dust. It can be done in an reaganz tube with an alcohol lamp or an bunsen burner. If this works thats an Phosphor cheat.
P.s i think you need an good fume hood because he writes when the aluminium touches the (molten) Metaphosphoric acid the metall desolves imidataly and phosphoric vapors are released.
Patent in german.

Attachment: Phosphor_all_pages.pdf (49kB)
This file has been downloaded 79 times

View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1143
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 25-10-2025 at 23:15


The problem is, what kind of vessel will you use to heat up the acid? Glass is attacked by metaphosophoric acid, and so is metal of course, unless you use, as the patent suggests, salts instead of acid?

View user's profile View All Posts By User
Alkoholvergiftung
Hazard to Others
***




Posts: 238
Registered: 12-7-2018
Member Is Offline


[*] posted on 25-10-2025 at 23:32


i see the problem when mixing. If it release imidataly the phosphor and how to seal it fast enough. but in theorie its an good methode because of low heat. i think an copper vesel would work.
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1143
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 25-10-2025 at 23:45


Maybe? You could probably use a copper vessel with a single hole and fit a Claysen adapter into it, much like what NileRed shows in his benzene video (q.v.). You connect one of the branches to a 'powder' dropping funnel for zinc or aluminium powder (if you use dust, I’m sure you can use a standard funnel), and the other one to a condenser. Flush the apparatus under argon/nitrogen before beginning to heat seems to me a good precaution to avoid the phosphorus vapours igniting right away.

These old patents are a source of unquenchable knowledge (es scheint mir schwer, dieser Satz auf Deutsch zu übersetzen).