cool.gif posted on 23-12-2025 at 08:31
metal wax


Oh hi its me again!
has anyone had any luck reverse engineering a solid metal wax for sealing? Renaissance and Sculpt Nouveau make sort of the same top of the line archival stuff-its a nice smelling wax- which is as far as I can tell Microcryrstaline wax maybe a petroleum jelly and some kind of relatively harmless solvent which keeps the whole thing close to a meting temperature. It is however ferociously expensive and I have plenty of microcrystalline paste around- its just not sort of able to be applied as smoothly with the other adjuncts.

I feel like theres a reasonably good solution here, but I lack the vocabulary to ask the right questions of google.

PS if you want to see what Im brewing up see attached.

DSC01277wide sconce- 3200 composite.png - 7.1MB
View user's profile Visit user's homepage View All Posts By User
bnull
National Hazard
****




Posts: 995
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 23-12-2025 at 10:14


See the SDS for Sculpt Nouveau metal wax below. You're going to have to experiment with the proportions (compare melting point homemade vs commercial, for example) to get a similar wax.

Attachment: SDS Sculpt Nouveau metal wax.pdf (68kB)
This file has been downloaded 76 times




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
RLyon
Harmless
*




Posts: 9
Registered: 7-5-2025
Member Is Offline

Mood: No Mood

[*] posted on 26-12-2025 at 10:58


Thanks !! Looks alot like the secret is mineral oil and turpentine, lol I should have guessed. :)
View user's profile Visit user's homepage View All Posts By User
bnull
National Hazard
****




Posts: 995
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 26-12-2025 at 14:12


And carnauba wax, which won't be hard to find.



Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.