Ylang-Ylang
Harmless
Posts: 8
Registered: 7-10-2003
Member Is Offline
Mood: No Mood
|
|
Nickel from nickels, again
I also tried the HCl dissolve of nickel with same (slow) results, and am now looking for electrolytic methods to accellerate the process.
Unfortunately, I don't know electrochem well. If I put some nickels in a copper basket, since the nickel is more noble, could I just plate it on
the other electrode? Or is there some way of increasing the rate of acid dissolving the nickel?
|
|
|
blip
Hazard to Others
 
Posts: 133
Registered: 16-3-2003
Member Is Offline
Mood: absorbed
|
|
I've been messing around with HCL, H<sub>2</sub>O<sub>2</sub>, and Cu pennies recently and it seems that the copper is
oxidized. I use pool HCl (heavily contaminated with FeCl<sub>x</sub>
and store-bought H<sub>2</sub>O<sub>2</sub>. I was being very careful at first because I did not want
Cl<sub>2</sub> to spew in my face. Maybe that'll do the trick, but beware: nickel compounds are very poisonous IIRC!
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Did you try to heat up Ni and HCl? I am sure the rate of reaction would go up...
Otherwise, try electrolysing Ni, where Ni would be the anode, in a weak HCl solution, with a graphite kathode... beware of Cl2 fumes though!
Else, you could always obtain NiO from pottery supplies, i.e. briarwheels, and simply dissolve NiO in HCl to get NiCl2.
good luck
|
|
|