pyrolytic carbon electrodes
I have heard of glassy carbon making amazing electrodes, but what about pyrolytic carbon?
I haven't found any information on wikipedia or Google about it's conductivity or use in electrodes.
\"For every action there is an equal and opposite government program.\"
|
|
Waffles
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 1-10-2006
Member Is Offline
Mood: No Mood
|
|
Pyrolytic graphite has essentially the same properties as graphite, except it can be cleaved into sheets since the molecular arrangement is oriented
that way. I would guess it would behave similarly to graphite except probably flake off more often and is a shit-ton more expensive.
Wikipedia and Hochtemperatur-Werkstoffe GMBH say that glassy carbon is the most chemically resistant form of carbon, and that makes sense.