Maybe ZnO can be turned into Zn By converting it to ZnCl2 with hydrochloric acid and then adding Al foil to the solution.. The zinc should precipitate
as the Al goes into the solution. A good stir should keep it from forming sheets and give you a nice fine powder. I recently saw a website somewhere
that showed this exact reaction. I seemed to work quite nicely. As soon as I get my hands on some Zn or ZnO I'll try this
#261501 +(11351)- [X]
the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally
courtesy of bash
|
|
|
aldol
Harmless
Posts: 30
Registered: 7-3-2005
Member Is Offline
Mood: No Mood
|
|
dust
why not use zncl ; bakers soldering fluid is 10% in water you can get it anywhere.
and then percipertate out the zn with a more electropositive metal
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Did you read the thread? Organikum seemed successful at making Zn from ZnCl2 and Al !
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
jimmyboy
Hazard to Others
 
Posts: 235
Registered: 1-3-2004
Location: Texas
Member Is Offline
Mood: No Mood
|
|
are the pics gone? - the pic of the zinc metal from the reaction was nice
|
|
|
Ashendale
Harmless
Posts: 47
Registered: 3-4-2005
Location: Estonia
Member Is Offline
Mood: Hydrated
|
|
Theoretical production of zinc?
I was wondering today, how to make zinc, and I came up with this...
2NaOH + ZnSO<sub>4</sub> = Na<sub>2</sub>SO<sub>4</sub> + Zn(OH)<sub>2</sub>
Na<sub>2</sub>SO<sub>4</sub> + Zn(OH)<sub>2</sub> (temp)---->
Na<sub>2</sub>SO<sub>4</sub> + ZnO + H<sub>2</sub>O
ZnO + 2HCl = ZnCl<sub>2</sub> + H<sub>2</sub>O
2Al + 3ZnCl<sub>2</sub> = 2AlCl<sub>3</sub> +3Zn
EDIT: Balanced o.o
I wanted to ask you, is this possible for the contents to react differently?
[Edited on 20-4-2005 by Ashendale]
[Edited on 20-4-2005 by Ashendale]
|
|
|
Esplosivo
Hazard to Others
 
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
This was already discussed on the zincdust thread, except for the first couple of steps in the procedure. Instead of NaOH I would prefer using sodium carbonate (to produce the
carbonate and some hydroxide), since being less basic than the hydroxide it reduces the conversion of Zn(OH)2 to the zincate ion [Zn(OH)4]2-, and
therefore prevents to a certain extent the 'wastage' of zinc and/or annoying drop-by-drop addition of the sodium hydroxide. The second step
is useless. You can react either the hydroxide or the carbonate (if you decided to use Na2CO3) with HCl directly. No need for that reaction, which
frankly I don't think occurs or else you would need extremely high temperatures. Hope this helps.
[Edited on 20-4-2005 by Esplosivo]
Theory guides, experiment decides.
|
|
|
cyclonite4
Hazard to Others
 
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
Not to mention you didn't even bother to balance the equations.
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
|
Ashendale
Harmless
Posts: 47
Registered: 3-4-2005
Location: Estonia
Member Is Offline
Mood: Hydrated
|
|
I know it was discussed, yet I tried to think another way of doing it. No need to bash me..
| Quote: | The second step is useless. You can react either the hydroxide or the carbonate (if you decided to use Na2CO3) with HCl directly.
|
Second step: Na<sub>2</sub>SO<sub>4</sub> + Zn(OH)<sub>2</sub> (temp)---->
Na<sub>2</sub>SO<sub>4</sub> + ZnO + H<sub>2</sub>O
HCl? Where's HCl?
As for the balancing, I usually never balance anything I write, unless needed. Stupid habbit? Maybe.
[Edited on 20-4-2005 by Ashendale]
|
|
|
Esplosivo
Hazard to Others
 
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
First of, I didn't bash you. Take it easy 
Secondly, I meant that your second step is not necessary. You could instead react the Zn(OH)2 from the first reaction with HCl. Is it clear now?
Theory guides, experiment decides.
|
|
|
Ashendale
Harmless
Posts: 47
Registered: 3-4-2005
Location: Estonia
Member Is Offline
Mood: Hydrated
|
|
Ahh, guess I was thinking the longer the fancier.
|
|
|
UhhKaipShaltaBlet
Harmless
Posts: 11
Registered: 23-1-2005
Member Is Offline
Mood: Shalta Blet ...
|
|
About CaC2 + ZnO reaction.... It doesn't work at all... Maybe at Super-Mega High temperatures. Powdered CaC2(VERY HARDLY) mixed with ZnO. Added
to steel "baker" and tried firstly to ignite by match(hahahah) - no success. Then tried with Black Powder with +10% Al powder. No success.
Another try was Fe2O3 + Al. And Guess what ? Made little hole in center and putted 100g(!!!!!!!!!) thermite. On top thermite was 20g Al/S. Thermite
ignited ,but no success igniting CaC2/ZnO. This mix is tottal bullshit. Maybe in some furnace or there is tricky thing that I don't know ....
Don't even try to ignite that CaC2/ZnO mixture ....
|
|
|