"That Reaction is incorrect
That last reaction does not happen."
What, 2K+2KOH=>2K2O+H2 doesn't happen? What the hell? It happens with
NaOH when it's electrolysed (that's why the reaction's yield is 15%) , why the hell not with KOH?
|
|
|
PrimoPyro
on fire
 
Posts: 122
Registered: 7-8-2002
Member Is Offline
Mood: No Mood
|
|
It does
All alkalai metals react with their hydroxides to liberate hydrogen.
|
|
|
Marvin
National Hazard
  
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
Anyone who gets a yeild of 15% sodium by electrolysis of molten NaOH is doing something very wrong.
At 5C over the melting point yeilds are over 80% sodium produced based on current. A small amount (I think about 7%) of carbonate also helps.
The reaction between the metal and the hydroxide does happen and can be made to work preperativly at higher temperatures. Observation of this is
complicated however, becuase the alkali metals are also soluable in their molten hydroxides to a certain extent.
Electrolysis of NaNO3 also works, but there are a few problems, firstly its an oxidising agent, and sodium is a reducing agent so reactions happen
during its formation, secondly the cell generates the highly toxic NO2 gas. I'm not sure how long the electrolysis has to progress before sodium
can be collected from it, maybe until a large portion of the nitrate around the cathode has been reduced. Casutic soda is spectacular enough, I think
this is best left alone.
[Edited on 1-11-2003 by Marvin]
|
|
|
PrimoPyro
on fire
 
Posts: 122
Registered: 7-8-2002
Member Is Offline
Mood: No Mood
|
|
O2 Liberated
Na2O might not conpletely solvate in Molten Na, but I would bet that it's ionic structure is exposed enough so that in a molten NaOH solution,
Na2(+2) and O(-2) can be seperated, liberating O2 at the anode.
|
|
|
PrimoPyro
on fire
 
Posts: 122
Registered: 7-8-2002
Member Is Offline
Mood: No Mood
|
|
Another Process
http://l2.espacenet.com/espacenet/viewer?PN=US6221310&CY...
Found from http://www.ewire.com/display.cfm/Wire_ID/1490
PrimoPyro
|
|
|
Marvin
National Hazard
  
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
Ross, electrolysis of molten NaCl is not feasable outside an industrial setting. For a start the cells have to be big, or its not possible to lag
them well enough to keep the salt molten electrically. Also Sodium at the melting point of salt has a large vapour pressure (about a third of an
atmosphere IIRC) so a mistake can be spectacular in a very bad way.
|
|
|
navarone
Horny Bunny
Posts: 19
Registered: 29-1-2004
Location: fuck no!
Member Is Offline
Mood: chillin'
|
|
vacum electrolysis
i just read of it on a chem site but it should work.
take an elenmeyer vacum container.
tap the top with a double holed cork.
tight fit two electic poles going all the way till the bottom without touching.
turn on the vacum.
heat the elenmeyr until the sodium chloride that is putted in the bottom melts.
molten sodium chloride conducts electricity.
when the salt is molten turn on the electrycity.
voila. the chlorine gas comes out of the sodium and gets sucked but the vacum.
since there is no oxygen to...the sodium wont oxydise.
once u have the sodium just pot it in a pure hydrocarbon liqid such as pure white gasoline.
so it wont oxidise.
|
|
|