Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
 Pages:  1  2    4
Author: Subject: Electroforming is useful...
Nixie
Hazard to Others
***




Posts: 490
Registered: 12-12-2006
Member Is Offline

Mood: ?

[*] posted on 18-12-2006 at 12:39


Is there any other way from Ag to the chloride (since I'm starting with Ag, not the nitrate).
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 18-12-2006 at 13:08


You should be able to by use of a silver cathode in a salt(or perhaps HCl) solution. Assuming of course that the precipitated AgCl does not cling to the electrode too much.

EDIT: HCl is preferable I think, especially in an undivided cell, otherwise Ag2O may contaminate.

[Edited on 18-12-2006 by The_Davster]




View user's profile View All Posts By User
Nixie
Hazard to Others
***




Posts: 490
Registered: 12-12-2006
Member Is Offline

Mood: ?

[*] posted on 18-12-2006 at 13:16


Great! Any substitutes for the binder? I shall try this procedure as soon as I can.
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 18-12-2006 at 21:37


Yeah, AgCl builds up very fast on the silver, but the silver chloride sticks to the electrode stopping further reaction. If the silver electrode was flat and placed on the bottom of the beaker under a stirbar it would work. The AgCl comes off the electrode with mild scraping.



View user's profile View All Posts By User
Tacho
National Hazard
****




Posts: 582
Registered: 5-12-2003
Member Is Offline

Mood: No Mood

[*] posted on 19-12-2006 at 03:29


Binder is not really necessary, just salt and AgCl on some toilet paper, it probably works anyway.



View user's profile View All Posts By User
hashashan
Hazard to Others
***




Posts: 255
Registered: 10-10-2006
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2007 at 01:00


Guys i found this :
http://www.google.com/patents?id=dFpyAAAAEBAJ&printsec=a...

it does look promising, however do you have an idea what sodium phosphate did they mean there?

btw. sorry for the bump, but i do believe there is some interest in it

[Edited on 19-6-2007 by hashashan]
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 4-7-2012 at 13:42


Electroplaters view of Physical Vapor Deposition Processing
http://infohouse.p2ric.org/ref/25/24745.pdf
A very thorough comparison with electroplating and other methods of metal coating.

Another useful thread here _
http://www.sciencemadness.org/talk/viewthread.php?tid=1990#p...

.
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 10-8-2012 at 08:12
Saturday Night Special


www.businessinsider.com/it-is-now-possible-to-download-and-3...

It's entirely possible to use ceramic powder which is sintered much as clay pots are
fired in a kiln to make firearm parts which cannot be seen by a metal detector.

resources
www.websiteslike.org/site/makepartsfast.com

Paste this into Google => desktop manufacturing
click on the "Images for desktop manufacturing" link below

_____________________________________

somewhat related
www.sciencemadness.org/talk/viewthread.php?tid=20889

.
View user's profile View All Posts By User
argyrium
Hazard to Others
***




Posts: 123
Registered: 3-2-2008
Location: Pacific
Member Is Offline

Mood: No Mood

[*] posted on 2-8-2016 at 15:47


I happened upon this very interesting clip showing a recent development of a nano-Ag based "ink".

Silver based "ink" for electrical conductivity - in a pen.

a clip: https://www.youtube.com/watch?v=zRbQvEefhXc#t=39

and the site:

https://agic.cc/en

and a paper:

Attachment: p363-kawahara.pdf (7.7MB)
This file has been downloaded 778 times

Hope it will be useful for someone here.
View user's profile View All Posts By User
 Pages:  1  2    4