Author: Subject: Unconventional Shaped Charges
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 18-9-2015 at 01:34


Nice test Nux, but damn plate, we still don't know where your charge stands on the graph because one of the welds broke which would have affected the jets performance I'm guessing. Even though it broke you still got more depth so it can go deeper.
Just goes to show how much energy these jets carry if they can break the welds that they don't even contact:D

For a charge 3x standoff and 4 CD penetration, it stands around non-precision line at the moment but I think you could get over it if the plates didn't break apart at the weld.


[Edited on 18-9-2015 by greenlight]





View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 18-9-2015 at 02:39


The 5 plates were scattered over a half meter it just blew it to shit.
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 18-9-2015 at 02:52


:D
Where all the plates welded together?
If so, did it break all the welds between the plates?





View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 18-9-2015 at 02:56


All 5 plates were tacked welded on 4 corners so it broke 18 tacks in total,where the carrot pokes through it only broke 2 tacks so 4x4= 16+2=18 a lot of tacks anyway. :(

[Edited on 18-9-2015 by nux vomica]
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 18-9-2015 at 04:50


Very interesting, do you have a density measurement for the plastic explosive mix you are using at the moment for that charge?




View user's profile View All Posts By User
gnitseretni
Hazard to Others
***




Posts: 290
Registered: 5-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 18-9-2015 at 10:12


Very nice!

I would increase standoff even more. That first hole is pretty big. It takes a lot of energy to punch a hole that size. If you increase standoff, you'll reduce the size of that initial hole and you'll have more energy available for penetration.
View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 18-9-2015 at 20:14


Quote: Originally posted by gnitseretni  
Very nice!

I would increase standoff even more. That first hole is pretty big. It takes a lot of energy to punch a hole that size. If you increase standoff, you'll reduce the size of that initial hole and you'll have more energy available for penetration.


Hmm ive got another piece of pvc pipe and 10 grms of etn plastic left so I think the next ones standoff will be 5.5cd or 110mm thoughts?

[Edited on 19-9-2015 by nux vomica]
View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 18-9-2015 at 21:36


Quote: Originally posted by greenlight  
Very interesting, do you have a density measurement for the plastic explosive mix you are using at the moment for that charge?


Its 1.26 grams per cubic centermeter greenlight
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 994
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 21-9-2015 at 07:28



Quote:

Its 1.26 grams per cubic centermeter greenlight


Really? That is surprisingly good performance for such a low density.
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2822
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 21-9-2015 at 10:26


How did you determine density? Did you further process the plastique after that measurement, possibly changing the density?



Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
markx
National Hazard
****




Posts: 657
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline

Mood: Very Jolly

[*] posted on 21-9-2015 at 15:00


Quote: Originally posted by nux vomica  


Its 1.26 grams per cubic centermeter greenlight


That seems a tad bit low actually, at least for such excellent results....perhaps a characteristic peculiarity in the measurement technique is responsible for that. I've never overworked my plastiques too much with the rolling and homogenisation, but still the density (by water displacement method) seems to land in the vincinity of 1.4g/cm3




Exact science is a figment of imagination.......
View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 21-9-2015 at 15:13


Unfortunately after checking my etn plastic my earlier post was the wrong density measurement :( I mismeasured the aluminium tube dia and being a small dia and etn weight it made a large difference to the result.

I remade my density measuring tool to measure 10 grams, I reamed a 20mm hole in some delrin and made a base and plunger to suit it and found it actually measured 1.417 grms cm3 density .

The etn plastic pellet measures 20 mm dia by 22.46 long so 3.141 x sqr10 x 22.46 = 7.056 cm3
10 grams / 7.056 cm3 = 1.417grms cm3

So it seems my etn plastic is a reasonable density for shaped charges after all, nux



20150922_164200.jpg - 1.4MB 20150922_162656.jpg - 1.1MB 20150922_162801.jpg - 1.1MB

[Edited on 22-9-2015 by nux vomica]
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 24-9-2015 at 19:22
Russian RPG 7 vs 16 inches bullet proof glass


www.youtube.com/watch?v=_J-uKNb6TaI

Trivia
RPG stands for " ruchnoy protivotankovyy granatomyot " ( Romanised ) which translates as " hand-held anti-tank grenade launcher "




Techniques to Disrupt, Deviate and Seize Control of an Internet Forum In case you wonder W T F ! is going on here ?
www.zerohedge.com/contributed/2012-10-28/cointelpro-techniques-dilution-misdirection-and-control-internet-forum https://web.archive.org/web/20120814124000/www.washingtonsblog.com/2012/08/the-15-rules-of-internet-disinformation.html
___________________________________________________________________________________________________________________
___________________________________________________________________________________________________________________
___________________________________________________________________________________________________________________
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 24-9-2015 at 23:49


Thats a really nice video, you can see the jet penetrating and the rocket motor portion of the RPG igniting after the booster portion in the high speed footage.




View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 25-9-2015 at 03:07


Franklyn you got me looking on the tube this one was impressive as well. nux

https://youtu.be/q6j9wEF1sf8

[Edited on 25-9-2015 by nux vomica]
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 25-9-2015 at 08:40
More kinematics


www.youtube.com/watch?v=7VSfUt1ggxk



Techniques to Disrupt, Deviate and Seize Control of an Internet Forum In case you wonder W T F ! is going on here ?
www.zerohedge.com/contributed/2012-10-28/cointelpro-techniques-dilution-misdirection-and-control-internet-forum https://web.archive.org/web/20120814124000/www.washingtonsblog.com/2012/08/the-15-rules-of-internet-disinformation.html
___________________________________________________________________________________________________________________
___________________________________________________________________________________________________________________
___________________________________________________________________________________________________________________
View user's profile View All Posts By User
VladimirLem
Hazard to Others
***




Posts: 204
Registered: 24-5-2010
Member Is Offline

Mood: Have no fear <Vlad> is here.

[*] posted on 25-9-2015 at 11:21


Quote: Originally posted by nux vomica  
Franklyn you got me looking on the tube this one was impressive as well. nux

https://youtu.be/q6j9wEF1sf8

i love that video, but its not a normal tandem shaped charge as the title says (afaik) , its an anti structure warhead - first one is a shapedcharge and the other detonation is a electronic delayed HE-Frag...

just sayin :D
View user's profile View All Posts By User
nitro-genes
International Hazard
*****




Posts: 1048
Registered: 5-4-2005
Member Is Offline


[*] posted on 1-10-2015 at 02:52


@ Nux: Did you spin those liners on a lathe? Brings back good memories. :)


[Edited on 1-10-2015 by nitro-genes]

Spun formed Copper Liners Nitro-genes.jpg - 170kB
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 1-10-2015 at 04:26


Attempted penetration of a 19mm steel plate with a new batch of plastic explosive but no good effect.
EFP was 30mm diameter 60 cm standoff and 17 g charge weight.
Only 12 mm penetration. I even placed some ballistics gel behind the plate to see effects on the other side:mad:

I think it is bad plastic because I added the PETN/acetone mix too fast to ice water whereas I usually add slowly. The fast addition resulted in still a fluffy non-granular product which didn't roll easily. This meant I used more binder/plasticizer which has affected VOD quite badly. There is a visible flame for a second during detonation that is not usually there.
I rolled 150 grams too which is a shame, maybe I can use it to attempt to catch the EFP slug in the next test as it looks like it is still forming the slug okay.


[Edited on 1-10-2015 by greenlight]

20150929_152604.jpg - 9.7MB 20150929_152622.jpg - 7.5MB

[Edited on 1-10-2015 by greenlight]

20151001_200015.jpg - 3.6MB

[Edited on 1-10-2015 by greenlight]





View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 1-10-2015 at 05:06


Quote: Originally posted by nitro-genes  
@ Nux: Did you spin those liners on a lathe? Brings back good memories. :)


Nitro-genes I use a set of forming tools in a hydraulic press, I have tried spinning cones on a lathe but my success rate was low, its easier to press them out and have a 100% success rate.
cheers nux
View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 1-10-2015 at 05:14


Too bad greenlight, looks a nicely formed efp though, it would have made a mess of that gel if it had made it through I'm sure, are you going to bump the charge weight up by much for the next try?.
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 1-10-2015 at 05:22


I think I will use 20 to 24 grams next time but I think it should have penetrated more than 12mm. The last EFP with the same specs went straight through the 10mm steel with hardly any sign of loss of velocity.
I am convinced it is the plastic explosive having too much inerts and fluffy PETN as you should be able to see the flame on camera at normal speed.





View user's profile View All Posts By User
NeonPulse
Hazard to Others
***




Posts: 417
Registered: 29-6-2013
Location: The other end of the internet.
Member Is Offline

Mood: Isolated from Reality! For Real this time....

[*] posted on 1-10-2015 at 15:44


Have you considered making the projectile like a spear? This is achieved by placing a metal cross across the back of the copper platter. There are patents which detAil his the elongated spear is made and this would probably help the penetration greatly. This is a tantalum liner and they have worked out how to catch them intact somehow

image.png - 221kB




Where there is a will
there is a way.

AllCheMystery!
https://www.youtube.com/channel/UCWbbidIY4v57uczsl0Fgv7w?vie...
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 1-10-2015 at 18:51


I know that curvature of the liner and the head height of the explosive affect the elongation of the liner. I think I am getting quite wide slugs instead of more elongated shaped because the explosive height in the charge above the liner is only .75 the diameter of the liner. This is because of the density of the PE though its rollled for several hours to about 1.45-1.49.

This metal cross idea sounds interesting. I will look for patents documenting it if it too affects the elongation of the liner it could be useful. I always thought altering the back of the liner having it thicker in parts would make it break up when subjected to a detonation wave.
The projectile in the picture you just uploaded is the perfect shape for penetration and is the most well-formed I have ever seen. I wonder how they caught it in that state:o


[Edited on 2-10-2015 by greenlight]

[Edited on 2-10-2015 by greenlight]





View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 268
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 1-10-2015 at 20:14


Try a little more curvature greenlight it will push the efp more towards a jetting formation and will make a smaller projectile and more penetration .