Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
 Pages:  1  ..  58    60    62  ..  78
Author: Subject: Pretty Pictures (2)
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 10-3-2018 at 09:17


Looks like it would fit in very well with a model train set or diorama! Who would’ve known that something so inorganic could seem as if you’ve collected it straight from the outdoors, like some weird moss or fungus.



In chemistry, sometimes the solution is the problem.

It’s been a while, but I’m not dead! Updated 7/1/2020. Shout out to Aga, we got along well.
View user's profile View All Posts By User
Pumukli
National Hazard
****




Posts: 725
Registered: 2-3-2014
Location: EU
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2018 at 12:58


Have you ever tried sublimating benzoic acid in a pickle's jar?
After two days 8 g benzoic acid filled up the jar like this:

benzoic.JPG - 286kB
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 10-3-2018 at 13:06


Pyrolyse it, exactly as it is.

Either it will be simply destroyed, or you'll have an amazing substance.

The Jar will be a gonner.

[Edited on 10-3-2018 by aga]




View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 16-3-2018 at 15:18


Beautiful yellow crystals of p-benzoquinone.



p-benzoquinone.jpg - 1MB
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4509
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 20-3-2018 at 15:54


1) Crystals of silver grown by reacting copper with silver nitrate solution on a microscope slide.

2) Vanadium(III) solutions with a) excess oxalate and b) excess glycinate.

Ag2.jpg - 318kBVandy.jpg - 311kB




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Pumukli
National Hazard
****




Posts: 725
Registered: 2-3-2014
Location: EU
Member Is Offline

Mood: No Mood

[*] posted on 30-3-2018 at 10:39


Failed recrystallization attempt of MCPA.
The liquid separated into two layers upon cooling and after a few days in the cold crystals started to grow.
Then a few days later they grew through the layer seperating barrier into the other layer. It seemingly did not bothered them much. :-)

mcpacryst.jpg - 58kB
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 4-4-2018 at 14:58


Accidental big crystals of potassium iron (iii) oxalate.

UNADJUSTEDNONRAW_thumb_1527.jpg - 119kB
View user's profile View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 5-4-2018 at 07:05


First crystal of my CoSO4 solution prepared from CoCl2 + Na2CO3, then CoCO3 + H2SO4.
I'll try to make prettier crystals when the solution is all evaporated.

IMG_20180405_170144_489.jpg - 75kB




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 5-4-2018 at 07:48


Beautiful color!
View user's profile Visit user's homepage View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 5-4-2018 at 08:11


Quote: Originally posted by MrHomeScientist  
Beautiful color!

Thanks, I like it too, reminds me of Garnet.
CoCO3 (I know It's not the actual formula) is also quite interesting :) even though it's just a bubbling mess inside of a beaker.


IMG_20180331_113334.jpg - 2.3MB




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
greenlight
National Hazard
****




Posts: 796
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 17-4-2018 at 01:38


Cleaning some sodium metal made using Nurdrages procedure.
This is on the third wash.
Looks so nice before it gets oxidized by atmospheric O2

[Edited on 17-4-2018 by greenlight]

20180417_160557.jpg - 2.2MB





View user's profile View All Posts By User
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 17-4-2018 at 04:05
Beauty of carbamide crystals




IMAG1759.jpg - 4MB




View user's profile Visit user's homepage View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4509
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 17-4-2018 at 08:39


I just made some salen. One of the simplest, quickest organic reactions I've ever done. Too bad the reaction of the ligand with copper acetate wasn't as nice.

salen.jpg - 66kB




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 17-4-2018 at 08:58


Quote: Originally posted by TheMrbunGee  

Wow, they kind of reminds me of asbestos.




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 17-4-2018 at 08:58


Quote: Originally posted by DraconicAcid  
I just made some salen. One of the simplest, quickest organic reactions I've ever done. Too bad the reaction of the ligand with copper acetate wasn't as nice.

Beautiful :).




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
mayko
International Hazard
*****




Posts: 1230
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline

Mood: anomalous (Euclid class)

[*] posted on 17-4-2018 at 20:40


The boiling flask at the end of a nitric acid distillation:

IMG_20180415_nitricDist.jpg - 194kB

Something that stood out was the remarkably stable vapor front that formed in the
condenser:

IMG_20180415_vaporFront.jpg - 231kB




al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
View user's profile Visit user's homepage View All Posts By User
Hegi
Hazard to Others
***




Posts: 199
Registered: 27-9-2013
Member Is Offline

Mood: No idea.

[*] posted on 19-4-2018 at 05:30


Quote: Originally posted by DraconicAcid  
I just made some salen. One of the simplest, quickest organic reactions I've ever done. Too bad the reaction of the ligand with copper acetate wasn't as nice.


Hey man! Where did you get reactants? ... I would like to make salen too and make complexes with several metals. Then write down some article about it. Thanks for any help .)




Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4509
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 19-4-2018 at 10:12


I work at a college, so I cheat- I can basically order anything I like as long as it's not too expensive and I intend to use it for educational purposes (not just my own).



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3040
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 19-4-2018 at 10:37


Not exactly salen, but close enough and with very OTC chemicals!

http://www.asianjournalofchemistry.co.in/User/ViewFreeArticl...
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4509
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 19-4-2018 at 11:04


Quote: Originally posted by Tsjerk  
Not exactly salen, but close enough and with very OTC chemicals!

http://www.asianjournalofchemistry.co.in/User/ViewFreeArticl...

Cool- but I wonder if a 2:1 ratio would give a more salen-like chelate....




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Hegi
Hazard to Others
***




Posts: 199
Registered: 27-9-2013
Member Is Offline

Mood: No idea.

[*] posted on 20-4-2018 at 12:17


Quote: Originally posted by DraconicAcid  
I work at a college, so I cheat- I can basically order anything I like as long as it's not too expensive and I intend to use it for educational purposes (not just my own).


My bad I left academic environment.. ;)




Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
View user's profile View All Posts By User
Hegi
Hazard to Others
***




Posts: 199
Registered: 27-9-2013
Member Is Offline

Mood: No idea.

[*] posted on 20-4-2018 at 12:19


Quote: Originally posted by Tsjerk  
Not exactly salen, but close enough and with very OTC chemicals!

http://www.asianjournalofchemistry.co.in/User/ViewFreeArticl...


I see yes, thiourea is cheap but what about salicylaldehyde, where can I get it? Any idea?




Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3948
Registered: 8-2-2015
Member Is Offline


[*] posted on 20-4-2018 at 13:54
not so pretty picture


As a part of my ongoing investigation into the corrosive effects of aqua regia fumes on common objects,
I submit the following annotated photograph.

AR.jpg - 2.6MB

The aqua regia is the green solution in the background,
the colour is due to gold and silver dissolved in the aqua regia.





CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4509
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 20-4-2018 at 13:58


I suspect that the green colour is due more to copper impurities in the silver and gold, since silver(I) ions are colourless and AuCl4- is orange-yellow.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3948
Registered: 8-2-2015
Member Is Offline


[*] posted on 20-4-2018 at 14:06


Quote: Originally posted by DraconicAcid  
I suspect that the green colour is due more to copper impurities in the silver and gold, since silver(I) ions are colourless and AuCl4- is orange-yellow.


D'oh !

Of course the colour is due to copper not silver - brain fart :(
-------------------------------------------------------------------------------
I've recovered gold from scrap many times
(but my total gold collected is only just over one gram)
and I love the colour of chloroauric acid in solution - like urine but with with a sheen.

[Edited on 20-4-2018 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
 Pages:  1  ..  58    60    62  ..  78

  Go To Top