explosive polymers
Does anyone have any information on explosive polymers for example:
Polyvinyl Peroxymonoslufate
Polyvinyl Peracetate
Polyvinyl Nitrate
Polyvinyl Perchlorate
Polyvinyl chlorate
Nitropolystyrine
I suspect all the former could be prepared by the reaction of the respective acid with polyvinyl alcohol and the latter could be prepared by the
nitration of the phenyl groups of polystyrene.
|
|
|
hinz
Hazard to Others
 
Posts: 201
Registered: 29-10-2004
Member Is Offline
Mood: No Mood
|
|
You forgot the most common one: cellulose hexanitrate (nitrocellulose).
Most of those polymers you mentioned aren't stable / don't exist, like Polyvinyl chlorate.
The explosive properties of the existing ones aren't superior, so if you want to do some pyro, use the classical ones. Some nitrated polymers like
nitrated polystyrene are used as binder in compositions.
|
|
|
The_Davster
A pnictogen
     
Posts: 2861
Registered: 18-11-2003
Member Is Offline
Mood: .
|
|
http://www.roguesci.org/chemlab/energetics/PVN.html
http://www.roguesci.org/chemlab/energetics/DNPA_polymer.html
http://www.roguesci.org/chemlab/energetics/dinitropolystyren...
Most of what you proposed would not exist, and other than PVN, could not be prepared by simple reactions with acids.
Note the det velocities, especially the polystyrene nitration product...1500m/s...not exactly interesting stuff.
|
|
|